摘要
Polymer materials used in railway field are degraded by environmental factors such as thermal, oxidative, photolytic, hydrolytic, and mechanical. The expected service life of the polymer materials used in railway field is approximately 20 years that is relatively long period for the polymer material; therefore, respective degradation factors should be well considered. Some of the degradation conditions indicate similar mechanism. The oxidative reaction was seen in every degradation conditions under air atmosphere. The hydrolytic reaction was mainly observed in chemical and biological degradations. The degradation behavior of the polymer material was analyzed by various methods. FTIR, thermal analysis (TG, DSC), and molecular weight determination were mainly applied for its purpose. However, the degradation mechanism of practical products made of polymer material was insufficiently studied and the exchange criteria of the products depended on the visual inspection without the suitable degradation analysis not only in the railway field but also in other commercial and industrial fields. In addition, most of the methods to analyze degradation of polymer material are performed on the standard specimen forms. For the installed product, some kinds of damage are generated through the sample collection process: therefore, the damaged products have to be exchanged for brand new ones OF repaired totally to be used for more period. Moreover, it is hard to suspend the railway service for the degradation analysis of polymer products. From these backgrounds, the prospect of degradation analysis related to polymer materials used in railway field was proposed. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1723 / 1735
页数:13
相关论文
共 191 条
[81]   MECHANISM OF COBALT DRIER ACTION [J].
GIRARD, TA ;
BEISPIEL, M ;
BRICKER, CE .
JOURNAL OF THE AMERICAN OIL CHEMISTS SOCIETY, 1965, 42 (10) :828-&
[82]   Polymer bulk erosion [J].
Gopferich, A .
MACROMOLECULES, 1997, 30 (09) :2598-2604
[83]   The influence of biodegradation on the loss of a plasticiser from poly(vinyl chloride) [J].
Gumargalieva, KZ ;
Zaikov, GE ;
Semenov, SA ;
Zhdanova, OA .
POLYMER DEGRADATION AND STABILITY, 1999, 63 (01) :111-112
[84]   Problems of ageing and stabilization of poly(vinyl chloride) [J].
Gumargalieva, KZ ;
Ivanov, VB ;
Zaikov, GE ;
Moiseev, JV ;
Pokholok, TV .
POLYMER DEGRADATION AND STABILITY, 1996, 52 (01) :73-79
[85]  
Gunatillake P, 2006, BIOTECHNOL ANN REV, V12, P301, DOI 10.1016/S1387-2656(06)12009-8
[87]   POLY(ARYL ETHERS) BY NUCLEOPHILIC AROMATIC SUBSTITUTION .2. THERMAL STABILITY [J].
HALE, WF ;
FARNHAM, AG ;
JOHNSON, RN ;
CLENDINN.RA .
JOURNAL OF POLYMER SCIENCE PART A-1-POLYMER CHEMISTRY, 1967, 5 (9PA1) :2399-&
[88]   Morphology and degradation of biodegradable poly(L-lactide-co-β-malic acid) [J].
He, B ;
Bei, JZ ;
Wang, SG .
POLYMERS FOR ADVANCED TECHNOLOGIES, 2003, 14 (09) :645-652
[89]  
Helbig M., 1978, J POLYM SCI PS, V63, P329
[90]   THERMOSTABLE ORGANIC POLYMERS DEVOID OF HYDROGEN AND OTHER PENDENT GROUPS [J].
HIRSCH, SS .
JOURNAL OF POLYMER SCIENCE PART A-1-POLYMER CHEMISTRY, 1969, 7 (1PA1) :15-&