Degradation issues of polymer materials used in railway field

被引:47
作者
Ito, Mikiya [1 ]
Nagai, Kazukiyo [2 ]
机构
[1] Railway Tech Res Inst, Mat Technol Div, Kokubunji, Tokyo 1858540, Japan
[2] Meiji Univ, Dept Appl Chem, Tama Ku, Kawasaki, Kanagawa 2148571, Japan
关键词
Polymer degradation; Degradation condition; Mass production polymer; Railway; Test method;
D O I
10.1016/j.polymdegradstab.2008.07.011
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polymer materials used in railway field are degraded by environmental factors such as thermal, oxidative, photolytic, hydrolytic, and mechanical. The expected service life of the polymer materials used in railway field is approximately 20 years that is relatively long period for the polymer material; therefore, respective degradation factors should be well considered. Some of the degradation conditions indicate similar mechanism. The oxidative reaction was seen in every degradation conditions under air atmosphere. The hydrolytic reaction was mainly observed in chemical and biological degradations. The degradation behavior of the polymer material was analyzed by various methods. FTIR, thermal analysis (TG, DSC), and molecular weight determination were mainly applied for its purpose. However, the degradation mechanism of practical products made of polymer material was insufficiently studied and the exchange criteria of the products depended on the visual inspection without the suitable degradation analysis not only in the railway field but also in other commercial and industrial fields. In addition, most of the methods to analyze degradation of polymer material are performed on the standard specimen forms. For the installed product, some kinds of damage are generated through the sample collection process: therefore, the damaged products have to be exchanged for brand new ones OF repaired totally to be used for more period. Moreover, it is hard to suspend the railway service for the degradation analysis of polymer products. From these backgrounds, the prospect of degradation analysis related to polymer materials used in railway field was proposed. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1723 / 1735
页数:13
相关论文
共 191 条
[1]   Study on permeation behavior and chemical degradation of PA66 in acid solution [J].
Abastari ;
Sakai, Tetsuya ;
Sembokuya, Hideki ;
Kubouchi, Masatoshi ;
Tsuda, Ken .
POLYMER DEGRADATION AND STABILITY, 2007, 92 (03) :379-388
[2]   SHEAR DEGRADATION OF POLYISOBUTENE [J].
ABBAS, KB ;
PORTER, RS .
JOURNAL OF APPLIED POLYMER SCIENCE, 1976, 20 (05) :1289-1300
[3]  
ABE N, 1995, RTRI REPORT, V9, P13
[4]   DEGRADATION OF CROSSLINKED RESINS IN WATER AND ELECTROLYTE-SOLUTIONS [J].
ABEYSINGHE, HP ;
EDWARDS, W ;
PRITCHARD, G ;
SWAMPILLAI, GJ .
POLYMER, 1982, 23 (12) :1785-1790
[5]   Nonisothermal crystallization kinetics and morphology of poly(ethylene terephthalate) modified with poly(lactic acid) [J].
Acar, Isil ;
Durmus, Ali ;
Oezguemues, Saadet .
JOURNAL OF APPLIED POLYMER SCIENCE, 2007, 106 (06) :4180-4191
[6]   Characterization of the degradation of polylactic acid polymer in a solid substrate environment [J].
Agarwal, M ;
Koelling, KW ;
Chalmers, JJ .
BIOTECHNOLOGY PROGRESS, 1998, 14 (03) :517-526
[7]   Investigation of oxidative degradation in polymers using 17O NMR spectroscopy [J].
Alam, TM ;
Celina, M ;
Assink, RA ;
Clough, RL ;
Gillen, KT ;
Wheeler, DR .
MACROMOLECULES, 2000, 33 (04) :1181-1190
[8]   SYNTHESIS, CHARACTERIZATION AND DEGRADATION OF ALIPHATIC POLYANHYDRIDES [J].
ALBERTSSON, AC ;
LUNDMARK, S .
BRITISH POLYMER JOURNAL, 1990, 23 (03) :205-212
[9]   BIODEGRADATION OF SYNTHETIC-POLYMERS .3. LIBERATION OF (CO-2)-C-14 BY MOLDS LIKE FUSARIUM-REDOLENS FROM C-14-LABELED PULVERIZED HIGH-DENSITY POLYETHYLENE [J].
ALBERTSSON, AC ;
BANHIDI, ZG ;
BEYERERICSSON, LL .
JOURNAL OF APPLIED POLYMER SCIENCE, 1978, 22 (12) :3435-3447