Atomic-scale analysis of the oxygen configuration at a SrTiO3 dislocation core -: art. no. 225506

被引:110
作者
Jia, CL [1 ]
Thust, A
Urban, K
机构
[1] Forschungszentrum Julich, Inst Solid State Res, D-52425 Julich, Germany
[2] Forschungszentrum Julich, Ernst Ruska Ctr Microscopy & Spect Elect, ERC, D-52425 Julich, Germany
关键词
D O I
10.1103/PhysRevLett.95.225506
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
The atomic structure of a SrTiO3 dislocation is revealed directly by phase-retrieval electron microscopy. In particular, atomic columns of light oxygen are observed simultaneously with the columns of considerably heavier Sr and Ti. A distinct structural modification of the oxygen octahedra at the dislocation core as well as a significant nonstoichiometry, including a deficiency of oxygen, are observed. Deviations from the bulk chemical concentration are quantified column by column by means of structure modeling and quantum-mechanical simulations of the electron scattering process.
引用
收藏
页数:4
相关论文
共 23 条
  • [1] Can interface dislocations degrade ferroelectric properties?
    Alpay, SP
    Misirlioglu, IB
    Nagarajan, V
    Ramesh, R
    [J]. APPLIED PHYSICS LETTERS, 2004, 85 (11) : 2044 - 2046
  • [2] Bock O, 2002, ACTA CRYSTALLOGR B, V58, P594, DOI 10.1107/S0108768102001490
  • [3] Impact of misfit dislocations on the polarization instability of epitaxial nanostructured ferroelectric perovskites
    Chu, MW
    Szafraniak, I
    Scholz, R
    Harnagea, C
    Hesse, D
    Alexe, M
    Gösele, U
    [J]. NATURE MATERIALS, 2004, 3 (02) : 87 - 90
  • [4] Maximum-likelihood method for focus-variation image reconstruction in high resolution transmission electron microscopy
    Coene, WMJ
    Thust, A
    deBeeck, M
    VanDyck, D
    [J]. ULTRAMICROSCOPY, 1996, 64 (1-4) : 109 - 135
  • [5] Room-temperature ferroelectricity in strained SrTiO3
    Haeni, JH
    Irvin, P
    Chang, W
    Uecker, R
    Reiche, P
    Li, YL
    Choudhury, S
    Tian, W
    Hawley, ME
    Craigo, B
    Tagantsev, AK
    Pan, XQ
    Streiffer, SK
    Chen, LQ
    Kirchoefer, SW
    Levy, J
    Schlom, DG
    [J]. NATURE, 2004, 430 (7001) : 758 - 761
  • [6] Electron microscopy image enhanced
    Haider, M
    Uhlemann, S
    Schwan, E
    Rose, H
    Kabius, B
    Urban, K
    [J]. NATURE, 1998, 392 (6678) : 768 - 769
  • [7] THE USE OF NONLINEAR CHARACTERISTICS OF A LATTICE FRINGE IMAGE FOR THE CHARACTERIZATION OF IMAGING PARAMETERS
    HYTCH, MJ
    STOBBS, WM
    [J]. ULTRAMICROSCOPY, 1994, 53 (01) : 63 - 72
  • [8] Investigation of atomic displacements at a Σ3 {111} twin boundary in BaTiO3 by means of phase-retrieval electron microscopy
    Jia, CL
    Thust, A
    [J]. PHYSICAL REVIEW LETTERS, 1999, 82 (25) : 5052 - 5055
  • [9] Atomic-resolution measurement of oxygen concentration in oxide materials
    Jia, CL
    Urban, K
    [J]. SCIENCE, 2004, 303 (5666) : 2001 - 2004
  • [10] High-resolution transmission electron microscopy using negative spherical aberration
    Jia, CL
    Lentzen, M
    Urban, K
    [J]. MICROSCOPY AND MICROANALYSIS, 2004, 10 (02) : 174 - 184