Failure assessment of ASTM A213-T12 superheater boiler tubes in a natural gas liquid plant

被引:18
作者
Firouzeh, Arezoo [1 ]
Ranjbar, Khalil [1 ]
Baghal, S. M. Lari [1 ]
Kaidan, A. Heidari [2 ]
Mohemi, Enayatolah [3 ]
机构
[1] Shahid Chamran Univ Ahvaz, Mat Sci & Engn Dept, Ahvaz, Iran
[2] Shahid Chamran Univ Ahvaz, Mech Engn Dept, Ahvaz, Iran
[3] NISOC, Corros Lab, Ahvaz, Karoon Industri, Iran
关键词
Failure analysis; Superheater boiler tube; ASTM A213-T12 steel; Iron oxide scale; Temperature simulation;
D O I
10.1016/j.engfailanal.2018.03.005
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This paper presents the results of an investigation into the failure of steam boiler tubes in a liquefied gas treatment plant. The failure appeared in the form of a window rupture in the boiler tubes of 1.25Cr-0.5 Mo grade steel. Study revealed that a thick magnetite iron oxide layer was formed in the inner surface of these tubes, disturbing the heat flow and rising the temperature of the tubes. Consequently, the internal oxide layer led to a series of metallurgical degradation and the loss in mechanical strength of the boiler tubes. Failure analysis of the steam tubes was carried out by optical and scanning electron microscopy examinations, chemical analysis of the tube material and the results showed that the scales were formed in the inner surface of the tubes. Furthermore, the rise in operational temperature and its distribution were simulated using fluent software and the results were compared against the designed temperature of the tubes. The simulation revealed that the operating temperature of the tubes reached beyond the design temperature, confirming the microstructural degradations i.e., oxidation, decarburization and reduction in the effective tube wall thickness. The extensive scale formation on the steam side and the resultant tube wall thinning was identified as the main cause of failure in the superheater tubes.
引用
收藏
页码:15 / 27
页数:13
相关论文
共 19 条
[11]   HIGH-TEMPERATURE HYDROGEN ATTACK OF CARBON-STEEL [J].
ELIEZER, D .
JOURNAL OF MATERIALS SCIENCE, 1981, 16 (11) :2962-2966
[12]  
F Timmins P., 1997, SOLUTIONS HYDROGEN A
[13]  
Fluent F., 2006, F 6 3 US GUID
[14]   Investigation of tubing failure of super-heater boiler from Kuwait desalination electrical power plant [J].
Husain, A ;
Habib, K .
DESALINATION, 2005, 183 (1-3) :203-208
[15]   Creep failures of overheated boiler, superheater and reformer tubes [J].
Jones, DRH .
ENGINEERING FAILURE ANALYSIS, 2004, 11 (06) :873-893
[16]   Failure analysis of bank front boiler tubes [J].
Khajavi, M. R. ;
Abdolmaleki, A. R. ;
Adibi, N. ;
Mirfendereski, S. .
ENGINEERING FAILURE ANALYSIS, 2007, 14 (04) :731-738
[17]  
Purbolaksono J., 2009, J LOSS PREVENT PROC, V22, P719
[18]   Failure analysis of boiler cold and hot reheater tubes [J].
Ranjbar, Khalil .
ENGINEERING FAILURE ANALYSIS, 2007, 14 (04) :620-625
[19]   Potential problems in the identification of the root cause of superheater tube failures in 9Cr martensitic alloys [J].
Starr, F ;
Castle, J ;
Walker, R .
MATERIALS AT HIGH TEMPERATURES, 2004, 21 (03) :147-160