摘要
The paper presents the deformation and fracture analysis of coating-substrate systems dining spherical indentation. CrN and TiN ceramic coatings with a thickness of 1-5 mu m were tested using 10 to 200 pm tip radius spherical indenters. The typical results of indentation tests i.e. force-penetration depth curves were transformed into stress-strain curves using an algorithm developed by the author. The test results are compared with the results of numerical analysis conducted using FEM modelling Such a complex analysis allows users to determine the level of tensile stress leading to the formation of cracks observed using SEM and TEM microscopy, and to define the failure maps for the coating substrate-systems.
引用
收藏
页码:2307 / 2317
页数:11
相关论文
共 50 条
  • [1] Analysis of spherical indentations of coating-substrate systems: Experiments and finite element modeling
    Kot, Marcin
    Rakowski, Wieslaw
    Lackner, Juergen M.
    Major, Lukasz
    MATERIALS & DESIGN, 2013, 43 : 99 - 111
  • [2] In-depth numerical analysis of crack initiation and evolution in coating-substrate systems under spherical indentation
    Lu, Kegu
    Zhang, Sun
    Li, Jinyang
    Huang, Yin
    Zhu, Minhao
    JOURNAL OF MATERIALS RESEARCH, 2022, 37 (03) : 747 - 762
  • [3] Effect of local curvature of the coating-substrate interface on deformation and fracture of ceramic coatings under uniaxial tension
    Shugurov, A. R.
    Panin, A. V.
    PHYSICAL MESOMECHANICS, 2017, 20 (04) : 472 - 479
  • [4] Effect of local curvature of the coating-substrate interface on deformation and fracture of ceramic coatings under uniaxial tension
    A. R. Shugurov
    A. V. Panin
    Physical Mesomechanics, 2017, 20 : 472 - 479
  • [5] Load-bearing capacity of coating-substrate systems obtained from spherical indentation tests
    Kot, Marcin
    Rakowski, Wieslaw
    Major, Lukasz
    Lackner, Juergen
    MATERIALS & DESIGN, 2013, 46 : 751 - 757
  • [6] Deformation and fracture of TiN coating on a Si(111) substrate during nanoindentation
    An, T.
    Wang, L. L.
    Tian, H. W.
    Wen, M.
    Zheng, W. T.
    APPLIED SURFACE SCIENCE, 2011, 257 (17) : 7475 - 7480
  • [7] CONTACT MECHANICS OF COATING-SUBSTRATE SYSTEMS. II. NANOINDENTATION EXPERIMENTS
    Kot, M.
    JOURNAL OF THE BALKAN TRIBOLOGICAL ASSOCIATION, 2012, 18 (04): : 615 - 626
  • [9] CONTACT MECHANICS OF COATING-SUBSTRATE SYSTEMS. I. METHODS OF ANALYSIS AND FEM MODELLING OF NANOINDENTATION TESTS
    Kot, M.
    Lacki, P.
    JOURNAL OF THE BALKAN TRIBOLOGICAL ASSOCIATION, 2012, 18 (04): : 598 - 614
  • [10] Understanding adhesive sliding nanocontact mechanics in an exponentially graded coating-substrate structure
    Ban, Youxue
    Yan, Jie
    Li, Zhiqiang
    Mi, Changwen
    EUROPEAN JOURNAL OF MECHANICS A-SOLIDS, 2025, 109