Deterioration of highly filled EPDM rubber by thermal ageing in air: Kinetics and non-destructive monitoring

被引:43
作者
Pourmand, P. [1 ]
Hedenqvist, M. S. [1 ]
Furo, I. [2 ]
Gedde, U. W. [1 ]
机构
[1] KTH Royal Inst Technol, Sch Chem Sci & Engn Fibre & Polymer Technol, SE-10044 Stockholm, Sweden
[2] KTH Royal Inst Technol, Sch Chem Sci & Engn, Dept Chem, SE-10044 Stockholm, Sweden
关键词
EPDM rubber; Air ageing; Structure and property profiling; Portable NMR; Deterioration mechanism separation; Condition monitoring; LONG-TERM PERFORMANCE; MECHANICAL-PROPERTIES; ACRYLATE) NANOCOMPOSITES; PHENOLIC ANTIOXIDANT; LIFETIME PREDICTION; GAMMA-IRRADIATION; ELASTOMERS; DEGRADATION; NMR; POLYETHYLENE;
D O I
10.1016/j.polymertesting.2017.10.019
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effects of air ageing at different temperatures between 110 and 170 degrees C on cable transit seals based on highly filled EPDM rubber used in nuclear power plants were studied. The changes of the macroscopic mechanical properties (Young's modulus, indentation modulus and strain-at-break) were in accordance with the Arrhenius equation with an activation energy of 110 kJ mol(-1). Profiling to assess the structure and property gradients within aged blocks was performed via IR spectroscopy, micro-indentation, gravimetric analysis of n-heptane-extracted samples and non-invasive portable NMR spectroscopy. A previously developed methodology was used to separate the deterioration into three different processes: polymer oxidation that was diffusion-limited at all temperatures, migration of low-molar-mass species to the surrounding media and anaerobic changes to the polymer network. The methodology allowed the assessment of the kinetics (rate as a function of time and temperature) of the different processes. It was noticed that polymer oxidation yielded more crosslinking at higher temperatures than at lower temperatures. The data obtained by both the portable NMR (a non-invasive method) and the indentation modulus profiling showed correlations with strain-at-break data, indicating their usefulness as condition monitoring methods.
引用
收藏
页码:267 / 276
页数:10
相关论文
共 53 条
[21]   MODULUS PROFILING OF POLYMERS [J].
GILLEN, KT ;
CLOUGH, RL ;
QUINTANA, CA .
POLYMER DEGRADATION AND STABILITY, 1987, 17 (01) :31-47
[22]   DENSITY PROFILING OF POLYMERS [J].
GILLEN, KT ;
CLOUGH, RL ;
DHOOGE, NJ .
POLYMER, 1986, 27 (02) :225-232
[23]  
Gillen KT, 1997, TRENDS POLYM SCI, V5, P250
[24]  
Grassie N., 1988, POLYM DEGRADATION ST
[25]   Analysis of polymer materials by surface NMR via the MOUSE [J].
Guthausen, A ;
Zimmer, G ;
Blümler, P ;
Blümich, B .
JOURNAL OF MAGNETIC RESONANCE, 1998, 130 (01) :1-7
[26]   THE PHOTOOXIDATION OF EPDM RUBBER .5. MECHANICAL-PROPERTIES DEGRADATION OF VULCANIZED FILLED SAMPLES [J].
GUZZO, M ;
DEPAOLI, MA .
POLYMER DEGRADATION AND STABILITY, 1992, 38 (01) :41-45
[27]   Characterization of local deformation in filled-silicone elastomers subject to high strain - NMR MOUSE and Magnetic Resonance Imaging as a diagnostic tool for detection of inhomogeneities [J].
Herberg, Julie L. ;
Chinn, Sarah C. ;
Sawvel, April M. ;
Gjersing, Erica ;
Maxwell, Robert S. .
POLYMER DEGRADATION AND STABILITY, 2006, 91 (08) :1701-1710
[28]   STRUCTURAL EFFECTS ON THE VAPORIZATION OF HIGH-MOLECULAR-WEIGHT ESTERS [J].
KISHORE, K ;
SHOBHA, HK ;
MATTAMAL, GJ .
JOURNAL OF PHYSICAL CHEMISTRY, 1990, 94 (04) :1642-1648
[29]   Long-term performance of a DEHP-containing carbon-black-filled NBR membrane [J].
Linde, E. ;
Blomfeldt, T. O. J. ;
Hedenqvist, M. S. ;
Gedde, U. W. .
POLYMER TESTING, 2014, 34 :25-33
[30]   Interactions between a phenolic antioxidant, moisture, peroxide and crosslinking by-products with metal oxide nanoparticles in branched polyethylene [J].
Liu, D. ;
Pourrahimi, A. M. ;
Pallon, L. K. H. ;
Sanchez, C. Cobo ;
Olsson, R. T. ;
Hedenqvist, M. S. ;
Fogelstrom, L. ;
Malmstrom, E. ;
Gedde, U. W. .
POLYMER DEGRADATION AND STABILITY, 2016, 125 :21-32