Oxide composites of Al2O3 and LaPO4

被引:51
作者
Davis, JB [1 ]
Marshall, DB [1 ]
Morgan, PED [1 ]
机构
[1] Rockwell Int Corp, Ctr Sci, Thousand Oaks, CA 91360 USA
关键词
LaPO4; composites; fibres; mechanical properties; Al2O3;
D O I
10.1016/S0955-2219(99)00112-0
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Some properties of oxide composites based on Al2O3 and LaPO4 (La-monazite) are examined. A composite consisting of woven Al2O3 fibers with a porous matrix of Al2O3 and LaPO4 is shown to be damage tolerant and notch insensitive. The feasibility of achieving fiber sliding and pullout in a composite with a fully dense matrix is investigated using a small hot-pressed composite of sapphire fibers and LaPO4 matrix. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2421 / 2426
页数:6
相关论文
共 23 条
[1]   SILICON-CARBIDE FIBER REINFORCED GLASS-CERAMIC MATRIX COMPOSITES EXHIBITING HIGH-STRENGTH AND TOUGHNESS [J].
BRENNAN, JJ ;
PREWO, KM .
JOURNAL OF MATERIALS SCIENCE, 1982, 17 (08) :2371-2383
[2]  
BUCKLEY JD, 1988, AM CERAM SOC BULL, V67, P364
[3]   Structure and stability of synthetic interphases in CMCs [J].
Cain, MG ;
Cain, RL ;
Tye, A ;
Rian, P ;
Lewis, MH ;
Gent, J .
CMMC 96 - PROCEEDINGS OF THE FIRST INTERNATIONAL CONFERENCE ON CERAMIC AND METAL MATRIX COMPOSITES, PTS 1 AND 2, 1997, 127-3 :37-49
[4]  
CINIBULK MK, 1994, CERAM ENG SCI P, V15, P721
[5]   REACTIONS BETWEEN SYNTHETIC MICA AND SIMPLE OXIDE COMPOUNDS WITH APPLICATION TO OXIDATION-RESISTANT CERAMIC COMPOSITES [J].
COOPER, RF ;
HALL, PC .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (05) :1265-1273
[6]  
GOETTLER RW, 1997, CERAM ENG SCI P, V18, P279
[7]  
HARRISON MG, Patent No. 5306554
[8]  
HARRISON MG, 1994, Patent No. 2230259
[9]  
Keith WP, 1997, J AM CERAM SOC, V80, P357, DOI 10.1111/j.1151-2916.1997.tb02838.x
[10]   THE ROLE OF COATING COMPLIANCE AND FIBER-MATRIX INTERFACIAL TOPOGRAPHY ON DEBONDING IN CERAMIC COMPOSITES [J].
KERANS, RJ .
SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (04) :505-509