AlCl3•6H2O recovery from the acid leaching liquor of coal gangue by using concentrated hydrochloric inpouring

被引:51
作者
Guo, Yanxia [1 ]
Lv, Huibin [1 ]
Yang, Xi [1 ]
Cheng, Fangqin [1 ]
机构
[1] Shanxi Univ, Inst Resources & Environm Engn, State Environm Protect Key Lab Efficient Utilizat, Taiyuan 030006, Peoples R China
关键词
Alumina recovery; AlC3 center dot 6H(2)O; Crystallization; Concentrated hydrochloric acid; Coal gangue; ALUMINA; TEMPERATURE; EXTRACTION;
D O I
10.1016/j.seppur.2015.07.043
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Alumina extraction from coal gangue is hopeful to solve the stockpile and pollution problems of it in China. The impurities such as Fe, Ca, K and Mg in coal gangue would be dissolved in the acid leaching liquor in the process of alumina extraction using hydrochloric acid leaching, resulting in the difficulty in the separation of Aluminum. AlCl3 center dot 6H(2)O recovery from the recycled AlCl3-containing acid leaching liquor of coal gangue by concentrated hydrochloric acid inpouring was discussed in this paper. It showed that the saturated AlCl3 solution or leaching liquor presented high recovery and the maximum reached more than 80% at <45 degrees C. The recovery increased with increasing the volume of concentrated HCl. It reached >85% of the maximum crystallization at the volume ratio of concentrated HCl to the solution exceeding 2.25. The effect of the recycled crystallized liquor on the comprehensive dissolution of alumina is negligible. The contents of Al and levels of impurities such as Fe, Ca, K and Mg in the leaching liquor increased with the cycles, which had a significant effect on the recovery and quality of AlCl3 center dot 6H(2)O. The recovery of AlCl3 center dot 6H(2)O decreased gradually with the cycles and it decreased to 59.5% after 10th cycle. The contents of AlCl3 center dot 6H(2)O in crystals decreased since the levels of impurities in it increased with the cycles, which would limit the cycle times of the crystallized liquor. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:177 / 183
页数:7
相关论文
共 29 条
[1]  
Al-Sindy S., 2006, B GEOL MIN, V2, P67
[2]   Extraction of metal values from waste spent petroleum catalyst using acidic solutions [J].
Barik, S. P. ;
Park, K. H. ;
Parhi, P. K. ;
Park, J. T. ;
Nam, C. W. .
SEPARATION AND PURIFICATION TECHNOLOGY, 2012, 101 :85-90
[3]  
Bauer D.J., 1984, US DEP INTERIOR BUR, V8908, P1
[4]  
Brown R.R., 1979, BUR MINES REP INVEST, V8379, P1
[5]   Thermodynamic modeling of aqueous aluminum chemistry and solid-liquid equilibria to high solution concentration and temperature.: I.: The acidic H-Al-Na-K-Cl-H2O system from 0 to 100°C [J].
Christov, Christomir ;
Dickson, Andrew G. ;
Moller, Nancy .
JOURNAL OF SOLUTION CHEMISTRY, 2007, 36 (11-12) :1495-1523
[6]  
Cui H., 2013, INORG CHEM IND CHIN, V45, P9
[7]  
Cui L, 2009, THESIS SHANXI U CHIN
[8]   Dissolution kinetics of aluminum and iron from coal mining waste by hydrochloric acid [J].
Cui, Li ;
Guo, Yanxia ;
Wang, Xuming ;
Du, Zhiping ;
Cheng, Fangqin .
CHINESE JOURNAL OF CHEMICAL ENGINEERING, 2015, 23 (03) :590-596
[9]   Effect of activated coal mining wastes on the properties of blended cement [J].
Frias, M. ;
Sanchez de Rojas, M. I. ;
Garcia, R. ;
Juan Valdes, A. ;
Medina, C. .
CEMENT & CONCRETE COMPOSITES, 2012, 34 (05) :678-683
[10]   Comparative Study on Extracting Alumina from Circulating Fluidized-Bed and Pulverized-Coal Fly Ashes through Salt Activation [J].
Guo, Chunbin ;
Zou, Jingjing ;
Wei, Cundi ;
Jiang, Yinshan .
ENERGY & FUELS, 2013, 27 (12) :7868-7875