摘要
The fracture toughness was investigated using in an extruded AZ31 magnesium alloy with an initial grain size of 1.0 mu m. Since the small scale yielding condition was not satisfied with the present thin thickness, the value of plane-strain fracture toughness, K-IC = 27.9 MPam(1/2), was measured from Stretched Zone analysis. The values of K-IC in AZ31 magnesium alloys were dependent on the grain size. The grain refinement was found to be one of the improvement methods for fracture toughness in magnesium alloy.
引用
收藏
页码:155 / 160
页数:6
相关论文
共 25 条
[1]   Enhanced ductility in strongly textured magnesium produced by equal channel angular processing [J].
Agnew, SR ;
Horton, JA ;
Lillo, TM ;
Brown, DW .
SCRIPTA MATERIALIA, 2004, 50 (03) :377-381
[2]   PLASTIC DEFORMATION OF POLYCRYSTALLINE AGGREGATES [J].
ARMSTRONG, R ;
DOUTHWAITE, RM ;
CODD, I ;
PETCH, NJ .
PHILOSOPHICAL MAGAZINE, 1962, 7 (73) :45-&
[3]  
ASTM, ASTM E399
[4]  
Avedesian M. M., 1999, ASM SPECIALTY HDB MA
[5]   Evaluation of the KIC and JIC fracture parameters in a sand cast AZ91 magnesium alloy [J].
Barbagallo, S ;
Cerri, E .
ENGINEERING FAILURE ANALYSIS, 2004, 11 (01) :127-140
[6]   Issues that influence magnesium's use in the automotive industry [J].
Cole, GS .
MAGNESIUM ALLOYS 2003, PTS 1 AND 2, 2003, 419-4 :43-49
[7]  
GREENFIELD K, 1997, PERSPECTIVES CO LAW, V2, P1
[8]  
HIGASHI K, 1985, J JPN I LIGHT METALS, V35, P520, DOI DOI 10.2464/JILM.35.520
[9]   Mechanical properties and microstructures of an AZ61 Mg Alloy produced by equal channel angular pressing [J].
Kim, WJ ;
An, CW ;
Kim, YS ;
Hong, SI .
SCRIPTA MATERIALIA, 2002, 47 (01) :39-44
[10]   Effect of Y, Sr, and Nd additions on the microstructure and microfracture mechanism of squeeze-cast AZ91-X magnesium alloys [J].
Lee, S ;
Lee, SH ;
Kim, DH .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1998, 29 (04) :1221-1235