Spark plasma sintering of W-10Ti high-purity sputtering target: Densification mechanism and microstructure evolution

被引:21
作者
Huang, Lei [1 ]
Zhang, Jiuxing [1 ]
Pan, Yafei [1 ]
Du, Yong [2 ]
机构
[1] Hefei Univ Technol, Sch Mat Sci & Engn, Hefei 230009, Anhui, Peoples R China
[2] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Hunan, Peoples R China
关键词
Spark plasma sintering; W-10Ti sputtering target; Densification mechanism; Microstructure; TITANIUM DIFFUSION-BARRIERS; POWDER DENSIFICATION; TUNGSTEN; CREEP; GENERATION; KINETICS;
D O I
10.1016/j.ijrmhm.2020.105313
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The densification mechanism and microstructure evolution of W-10Ti sputtering target prepared by spark plasma sintering (SPS) method at a temperature ranges from 900 to 1600 degrees C, with dwelling time of 6 min and fixed pressure of 30 MPa were investigated. Densification occurs mainly at low temperatures (900 to 1300 degrees C), while grain growth occurs at high temperatures (1400 to 1600 degrees C). The creep model has been used to reveal the densification process. The effective stress exponent n is calculated systematically, which indicates that the densification process is mainly due to the particle rearrangement (n < 1), grain boundary diffusion (n = 1-2), and dislocation climbing (n = 3.77 or 4.14). In addition, the apparent activation energy Q(d) is calculated to be 119.30 and 271.79 kJ/mol when the effective stress exponent n is equal to 1 and 2, respectively. It is also found that the microstructure of W-10Ti alloys is greatly affected by the sintering temperatures. The solution between W and Ti significantly improves with the increase of the sintering temperature. The solubility of W in beta Ti(W) exceeded the eutectoid point (28.97 wt% W) and the eutectoid structure (beta W(Ti) + alpha Ti) forms in cooling process when the temperature is up to 1300 degrees C. With the temperature increasing to 1500 degrees C, the composition of the beta Ti(W) phase is located in the miscibility gap of the (beta Ti(W), beta W(Ti)) system, which tends to decompose in to beta Ti(W) and beta W(Ti) phases.
引用
收藏
页数:10
相关论文
共 42 条
[1]  
[Anonymous], 1999, MECH SPARK PLASMA SI
[2]   Elastic and plastic strains in Al/TiW/Si contacts during thermal cycles [J].
Berger, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 288 (02) :164-167
[3]   Spark plasma sintering of a commercially available granulated zirconia powder: I. Sintering path and hypotheses about the mechanism(s) controlling densification [J].
Bernard-Granger, Guillaume ;
Guizard, Christian .
ACTA MATERIALIA, 2007, 55 (10) :3493-3504
[4]   Spark plasma sintering of a commercially available granulated zirconia powder: Comparison with hot-pressing [J].
Bernard-Granger, Guillaume ;
Addad, Ahmed ;
Fantozzi, Gilbert ;
Bonnefont, Guillaume ;
Guizard, Christian ;
Vernat, Dorothee .
ACTA MATERIALIA, 2010, 58 (09) :3390-3399
[5]   Phenomenological analysis of densification mechanism during spark plasma sintering of MgAl2O4 [J].
Bernard-Granger, Guillaume ;
Benameur, Nassira ;
Addad, Ahmed ;
Nygren, Mats ;
Guizard, Christian ;
Deville, Sylvain .
JOURNAL OF MATERIALS RESEARCH, 2009, 24 (06) :2011-2020
[6]   Thermal stability of tungsten-titanium diffusion barriers for silver metallization [J].
Bhagat, S. K. ;
Theodore, N. D. ;
Alford, T. L. .
THIN SOLID FILMS, 2008, 516 (21) :7451-7457
[7]   Tungsten-titanium diffusion barriers for silver metallization [J].
Bhagat, Shekhar ;
Han, Hauk ;
Alford, T. L. .
THIN SOLID FILMS, 2006, 515 (04) :1998-2002
[8]  
Brook R. J., 1982, Sintering - Theory and Practice. Proceedings of the 5th International Round Table Conference on Sintering, P585
[9]   Densification of nanocrystalline NiO ceramics by spark plasma sintering [J].
Chaim, R. ;
Bar-Hama, O. Reinharz .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (03) :462-468
[10]   Effect of tungsten dissolution on the mechanical properties of Ti-W composites [J].
Choe, H ;
Abkowitz, SM ;
Abkowitz, S ;
Dunand, DC .
JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 390 (1-2) :62-66