Oxidation behavior and corrosion resistance of Ti-10Ta-10Nb alloy

被引:29
作者
Ahn, Hoon [2 ]
Lee, Dohjae [3 ]
Lee, Kwang-Min [3 ]
Lee, Kyungku [3 ]
Baek, Daehwa [4 ]
Park, Sang-Won [1 ]
机构
[1] Chonnam Natl Univ, Sch Dent, Kwangju 501746, South Korea
[2] Chosun Univ, Coll Dent, Kwangju 501759, South Korea
[3] Chonnam Natl Univ, Dept Mat Sci, Kwangju 500757, South Korea
[4] Small & Medium Business Adm, Kwangju 502200, South Korea
关键词
Ti-10Ta-10Nb alloys; Ti-6Al-4V alloys; Corrosion resistance; Cytotoxicity;
D O I
10.1016/j.surfcoat.2008.06.074
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
We have examined and discovered that a more passive oxide film by oxidation treatment can be formed on the newly designed Ti-10Ta-10Nb alloy, which is closely related to corrosion resistance and biocompatibility. Ti-6Al-4 V and Ti-10Ta-10Nb alloys were prepared by consumable vacuum arc melting and homogenized at 1050 degrees C for 24 h, and then both alloys were hot rolled at approximately 1000 degrees C. The alloy specimens were oxidized at temperatures between 400 to 750 degrees C for 30 min. The oxide films on the Ti alloys Were analyzed by optical microscope, SEM/EDX, XRD, XPS and TGA. The Corrosion resistances of the Ti alloys were evaluated by performing potentiodynamic polarization test in 0.9% NaCl and immersion test in 0.9% NaCl, 5% HCl and 1% lactic acid. Cytotoxicity test was performed in MTT assay treated L929 fibroblast cell culture by indirect method. We discovered that the oxide film on Ti-10Ta-10Nb alloy was denser and thinner compared to the oxide film on Ti-6Al-4 V alloy. The rapid increase in mass during oxidation was observed at temperatures above 650 degrees C for Ti-6Al-4 V alloy and above 700 degrees C for Ti-10Ta-10Nb alloy respectively. According to XRD results, both oxide layers were composed of mostly TiO2 (rutile) phase. The corrosion resistance of Ti-10Ta-10Nb alloy was improved by oxidation treatment. Furthermore, cytotoxicity test results indicated that moderate oxidation treatment lowers cell toxicity with the Ti-10Ta-10Nb alloy showing a more promising result compared to Ti-6Al-4 V alloy. (c) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:5784 / 5789
页数:6
相关论文
共 19 条
[1]  
AHMED T, 1995, SCI TECHNOL, V2, P1760
[2]   Effectiveness of uncoated WC-Co and PCD inserts in end milling of titanium alloy-Ti-6Al-4V [J].
Amin, A. K. M. Nurul ;
Ismail, Ahmad F. ;
Khairusshima, M. K. Nor .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 192 :147-158
[3]  
BLACK G, 1998, HDB BIOMATERIAL PROP, P1356
[4]   Cytocompatibility of Ti-6Al-4V and Ti-5Al-2.5Fe alloys according to three surface treatments, using human fibroblasts and osteoblasts [J].
Bordji, K ;
Jouzeau, JY ;
Mainard, D ;
Payan, E ;
Netter, P ;
Rie, KT ;
Stucky, T ;
HageAli, M .
BIOMATERIALS, 1996, 17 (09) :929-940
[5]   Nickel-titanium alloy: Cytotoxicity evaluation on microorganism culture [J].
Dinca, V. C. ;
Soare, S. ;
Barbalat, A. ;
Dinu, C. Z. ;
Moldovan, A. ;
Stoica, I. ;
Vassu, T. ;
Purice, A. ;
Scarisoareanu, N. ;
Birjega, R. ;
Craciun, V. ;
DeStefano, V. Ferrari ;
Dinescu, M. .
APPLIED SURFACE SCIENCE, 2006, 252 (13) :4619-4624
[6]   Enhanced wear resistance of titanium surfaces by a new thermal oxidation treatment [J].
Dong, H ;
Bell, T .
WEAR, 2000, 238 (02) :131-137
[7]   Performance of alloyed uncoated and CVD-coated carbide tools in dry milling of titanium alloy Ti-6242S [J].
Haron, C. H. Che ;
Ginting, A. ;
Arshad, H. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2007, 185 (1-3) :77-82
[8]  
HURLEN T, 1960, J I MET, V89, P128
[9]   The effect of annealing temperatures and cooling rates on microstructure and mechanical properties of investment cast Ti-6Al-4V alloy [J].
Jovanovic, MT ;
Tadic, S ;
Zec, S ;
Miskovic, Z ;
Bobic, I .
MATERIALS & DESIGN, 2006, 27 (03) :192-199
[10]   BIOCOMPATIBILITY OF TITANIUM IMPLANTS - SURFACE SCIENCE ASPECTS [J].
KASEMO, B .
JOURNAL OF PROSTHETIC DENTISTRY, 1983, 49 (06) :832-837