Nanoscale zero-valent iron (nZVI) synthesis in a Mg-aminoclay solution exhibits increased stability and reactivity for reductive decontamination

被引:63
|
作者
Hwang, Yuhoon [1 ]
Lee, Young-Chul [2 ,3 ]
Mines, Paul D. [1 ]
Huh, Yun Suk [3 ]
Andersen, Henrik R. [1 ]
机构
[1] Tech Univ Denmark, Dept Environm Engn, DK-2800 Lyngby, Denmark
[2] Korea Adv Inst Sci & Technol, Dept Civil & Environm Engn, Taejon 305701, South Korea
[3] Inha Univ, Coll Engn, Dept Biol Engn, Inchon 402751, South Korea
基金
新加坡国家研究基金会;
关键词
Mg-aminoclay (MgAC); Nanoscale zero-valent iron (nZVI); Nanotechnology; Colloidal stability; CORE-SHELL NANOWIRES; ORGANO-BUILDING BLOCKS; FUNCTIONALIZED MAGNESIUM PHYLLOSILICATE; OLEAGINOUS CHLORELLA SP; FE-0; NANOPARTICLES; POROUS-MEDIA; HUMIC-ACID; NEUTRAL PH; WATER; DEGRADATION;
D O I
10.1016/j.apcatb.2013.10.017
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Nanoscale zero-valent iron (nZVI) has often been explored as a reductant for detoxification of pollutants in environmental clean-ups. Despite the large surface area and superior reactivity of nZVI, its limited stability is a major obstacle in applying nZVI for in situ subsurface remediation, e.g. for chlorinated solvents hotspots. In this study, water-solubilized magnesium-aminoclay (MgAC) was applied for the first time as a stabilizing agent in the synthesis of nZVI. With increased doses of Mg-aminoclay applied in the synthesis mixture, nZVI particle growth was inhibited and thin sheathed grape-like nZVI particles with higher crystallinity were produced. Stability of nZVI particles were evaluated using a sedimentation test and a dynamic light scattering technique. The characteristic time increased from 6.71 to 83.8 min, and particle (aggregate diameter) size decreased from 5132 to 186 nm with increasing amounts of applied MgAC. The higher stability of MgAC coated nZVI could be explained from the higher zeta potential, which indicates that the stabilization mechanism is increased electrostatic repulsion from the positively charged MgAC coating. The optimal weight ratio between MgAC and iron was found to be 7.5:1. The MgAC coated nZVI exhibited higher reactivity for nitrate reduction with the observed first order rate constants increasing from 1.17 to 42.0h(-1), and Fe(0)-normalized rate constants from 0.124 to 43.8 h(-1) mg-Fe(0)(-1). Consequently, the MgAC coated nZVI showed increased feasibility, compared to uncoated nZVI, for application in remediation of subsurface contaminations; where high stability and mobility as well as high reactivity for degradation of contaminants is desired. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:748 / 755
页数:8
相关论文
共 50 条
  • [11] The colorful chemistry of nanoscale zero-valent iron (nZVI)
    Hua, Yilong
    Liu, Jing
    Gu, Tianhang
    Wang, Wei
    Zhang, Wei-xian
    JOURNAL OF ENVIRONMENTAL SCIENCES, 2018, 67 : 1 - 3
  • [12] Stabilization of biosolids with nanoscale zero-valent iron (nZVI)
    Xiao-qin Li
    Derick G. Brown
    Wei-xian Zhang
    Journal of Nanoparticle Research, 2007, 9 : 233 - 243
  • [13] The colorful chemistry of nanoscale zero-valent iron(nZVI)
    Yilong Hua
    Jing Liu
    Tianhang Gu
    Wei Wang
    Wei-xian Zhang
    Journal of Environmental Sciences, 2018, (05) : 1 - 3
  • [14] Removal of U(VI) in Aqueous Solution by Nanoscale Zero-Valent Iron(nZVI)
    Li, Xiaoyan
    Zhang, Ming
    Liu, Yibao
    Li, Xun
    Liu, Yunhai
    Hua, Rong
    He, Caiting
    WATER QUALITY EXPOSURE AND HEALTH, 2013, 5 (01): : 31 - 40
  • [15] Removal of U(VI) in Aqueous Solution by Nanoscale Zero-Valent Iron(nZVI)
    Xiaoyan Li
    Ming Zhang
    Yibao Liu
    Xun Li
    Yunhai Liu
    Rong Hua
    Caiting He
    Water Quality, Exposure and Health, 2013, 5 : 31 - 40
  • [16] Reductive remediation of trichloroethylene (TCE) solution by granulated nano zero-valent iron (nZVI)
    Shih, Yu-Jen
    Su, Chia-Chi
    Chen, Chiu-Wen
    Chen, Chih-Feng
    Dong, Cheng-Di
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2015, 249
  • [17] Removal of Arsenic and Selenium with Nanoscale Zero-Valent Iron (nZVI)
    Xia Xuefen
    Hua Yilong
    Huang Xiaoyue
    Ling Lan
    Zhang Weixian
    ACTA CHIMICA SINICA, 2017, 75 (06) : 594 - 601
  • [18] Sequestration of metal cations with nanoscale zero-valent iron (nZVI)
    Li, Xiao-Qin
    Zhang, Weixian
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2007, 233
  • [19] Kinetics of reductive denitrification by nanoscale zero-valent iron
    Choe, S
    Chang, YY
    Hwang, KY
    Khim, J
    CHEMOSPHERE, 2000, 41 (08) : 1307 - 1311
  • [20] Effect of Surfactants on Zero-Valent Iron Nanoparticles (NZVI) Reactivity
    Wang, Ziheng
    Choi, Francis
    Acosta, Edgar
    JOURNAL OF SURFACTANTS AND DETERGENTS, 2017, 20 (03) : 577 - 588