Pyroelectric energy conversion using PLZT ceramics and the ferroelectric-ergodic relaxor phase transition

被引:62
作者
Lee, Felix Y. [1 ]
Jo, Hwan Ryul [1 ]
Lynch, Christopher S. [1 ]
Pilon, Laurent [1 ]
机构
[1] Univ Calif Los Angeles, Dept Mech & Aerosp Engn, Henry Samueli Sch Engn & Appl Sci, Los Angeles, CA 90095 USA
关键词
LEAD-ZIRCONATE-TITANATE; ELECTRICAL ENERGY; WORKING FLUIDS; HEAT; CYCLE; CONVERTER; TEMPERATURE; EFFICIENCY; DIAGRAM;
D O I
10.1088/0964-1726/22/2/025038
中图分类号
TH7 [仪器、仪表];
学科分类号
0804 ; 080401 ; 081102 ;
摘要
This paper is concerned with direct conversion of waste heat into electricity by executing the Olsen cycle on lead lanthanum zirconate titanate (PLZT) ceramics undergoing a relaxor-ferroelectric phase transition. The Olsen cycle consists of two isothermal and two isoelectric field processes. First, the temperature-dependent dielectric properties were measured for x/65/35 PLZT. The polarization transition temperature of x/65/35 PLZT was found to decrease from 240 to 10 degrees C as x increased from 5 to 10 mol%. This suggests that the different compositions should be operated over different temperature ranges for maximum thermal to electrical energy conversion. The energy and power densities generated by the Olsen cycle using x/65/35 PLZT samples were measured by successively dipping the samples in isothermal dielectric oil baths. Large energy and power densities were obtained when the samples underwent the ergodic relaxor-ferroelectric phase transition. A maximum energy density of 1014 J l(-1) per cycle was obtained with a 190 mu m thick 7/65/35 PLZT sample cycled at 0.026 Hz between 30 and 200 degrees C and between 0.2 and 7.0 MV m(-1). To the best of our knowledge, this is the largest pyroelectric energy density ever demonstrated experimentally with ceramics, single crystals, or polymers. A maximum power density of 48 W l(-1) was achieved using a 200 mu m thick 6/65/35 PLZT sample for temperatures between 40 and 210 degrees C and electric fields between 0 and 8.5 MV m(-1) at a frequency of 0.060 Hz. The maximum applied electric field and temperature swings of these materials were physically limited by dielectric breakdown and thermomechanical stress.
引用
收藏
页数:16
相关论文
共 76 条
[1]   Domain structure-property relations in lead lanthanum zirconate titanate ceramics [J].
Akbas, MA ;
Reaney, IM ;
Lee, WE .
JOURNAL OF MATERIALS RESEARCH, 1996, 11 (09) :2293-2301
[2]   Electric-field-temperature phase diagram of the relaxor ferroelectric lanthanum-modified lead zirconate titanate [J].
Bobnar, V ;
Kutnjak, Z ;
Pirc, R ;
Levstik, A .
PHYSICAL REVIEW B, 1999, 60 (09) :6420-6427
[3]   Recent progress in relaxor ferroelectrics with perovskite structure [J].
Bokov, AA ;
Ye, ZG .
JOURNAL OF MATERIALS SCIENCE, 2006, 41 (01) :31-52
[4]   Pyroelectric and sensor properties of ferroelectric thin films for energy conversion [J].
Buchanan, RC ;
Huang, J .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1999, 19 (6-7) :1467-1471
[5]   ELECTRIC-FIELD-INDUCED FATIGUE-CRACK GROWTH IN PIEZOELECTRICS [J].
CAO, HC ;
EVANS, AG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1994, 77 (07) :1783-1786
[6]   Electric field dependence of the Curie temperature of ferroelectric poly(vinylidenefluoride-trifluoroethylene) co-polymers for pyroelectric energy harvesting [J].
Cha, Gilhwan ;
Ju, Y. Sungtaek .
SMART MATERIALS & STRUCTURES, 2012, 21 (02)
[7]  
Chemicals M G, 2012, TECHN SPEC SIL CONF
[8]   A review of thermodynamic cycles and working fluids for the conversion of low-grade heat [J].
Chen, Huijuan ;
Goswami, D. Yogi ;
Stefanakos, Elias K. .
RENEWABLE & SUSTAINABLE ENERGY REVIEWS, 2010, 14 (09) :3059-3067
[9]   Direct Thermal to Electrical Energy Conversion Using 9.5/65/35 PLZT Ceramics in the Ergodic Relaxor Phase [J].
Chin, Thomas K. ;
Lee, Felix Y. ;
McKinley, Ian M. ;
Goljahi, Sam ;
Lynch, Christopher S. ;
Pilon, Laurent .
IEEE TRANSACTIONS ON ULTRASONICS FERROELECTRICS AND FREQUENCY CONTROL, 2012, 59 (11) :2373-2385
[10]  
Clearco Products, 2012, SIL TRANSF OIL