Synthesis and hydration of ye'elimite-containing cement (YCC) produced with spent fluid catalytic cracking catalyst

被引:4
作者
Matos, Samile R. C. [1 ]
de Matos, Paulo R. [2 ]
Neto, Jose S. Andrade [3 ]
Campos, Carlos E. M. [4 ]
Kirchheim, Ana Paula [3 ]
Gonsalves, Jardel P. [1 ]
机构
[1] Univ Fed Bahia UFBA, Ctr Interdisciplinar Energia & Meio Ambiente CIEN, Escola Politecn, Programas Grad Engn Civil, Rua Prof Aristides Novis 02, BR-40210630 Salvador, BA, Brazil
[2] Univ Fed Santa Maria UFSM, Santa Maria, Brazil
[3] Univ Fed Rio Grande Sul UFRGS, Ctr Hist, Programa Posgrad Engn Civil Construcao & Infraest, Ave Osvaldo Aranha 99, BR-90035190 Porto Alegre, Rio Grande do S, Brazil
[4] Univ Fed Santa Catarina UFSC, Dept Fis, Lab Difracao Raios X, Santa Catarina, Brazil
关键词
Calcium sulfoaluminate cement; Spent catalyst; Waste management; Clinker; Cement hydration; X-ray diffraction; C-S-H; FCC CATALYST; AMORPHOUS PHASE; SULFOALUMINATE; NICKEL; WASTE; CLINKER; QUANTIFICATION; OPTIMIZATION; VANADIUM;
D O I
10.1016/j.conbuildmat.2022.129364
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The consumption of petroleum products from fluidized bed catalytic cracking (FCC) units has increased worldwide. One of the primary materials used in this process is the zeolitic catalyst which loses its catalytic capacity over time, generating the spent FCC catalyst - SFCC. This work evaluated the feasibility of using SFCC as raw material for ye'elimite-containing cements (YCC) production. Specifically, six types of clinkers were syn-thesized in the laboratory, varying the ye'elimite content, with and without SFCC. Powder and in-situ X-ray diffraction (XRD), isothermal calorimetry, and thermogravimetric analysis (TGA) were conducted in anhydrous and hydrated samples. Clinkers with SFCC stabilized more C4AF than those without SFCC; so there was less Fe3+ available in these systems than in the reference systems to stable the pseudo cubic ye'emelite. As a result, the SFCC-containing cements (with more orthorhombic ye'elimite) had higher reaction rates within the first 12-20 h of hydration. In turn, the higher ye'elimite contents in the high-and medium-ye'elimite reference clinkers led to the further formation of hydrated phases at 28 days of hydration on these samples. The equivalent ye'elimite content in low-ye'elimite clinkers led to equivalent cumulative heat and phase assemblage from 48 h to 28 days. Overall, the use of SFCC allowed to incorporate of up to 20.81 wt% of the residue in raw material replacement, resulting in cements with increased early-age reactivity.
引用
收藏
页数:14
相关论文
共 96 条
[51]   A novel nickel catalyst derived from layered double hydroxides (LDHs) supported on fluid catalytic cracking catalyst residue (FC3R) for rosin hydrogenation [J].
Huang, Yingying ;
Chen, Xiaopeng ;
Deng, Yongfu ;
Zhou, Dan ;
Wang, Linlin .
CHEMICAL ENGINEERING JOURNAL, 2015, 269 :434-443
[52]   Ferritic calcium sulfoaluminate belite cement from metallurgical industry residues and phosphogypsum: Clinker production, scale-up, and microstructural characterisation [J].
Isteri, Visa ;
Ohenoja, Katja ;
Hanein, Theodore ;
Kinoshita, Hajime ;
Kletti, Holger ;
Roessler, Christiane ;
Tanskanen, Pekka ;
Illikainen, Mirja ;
Fabritius, Timo .
CEMENT AND CONCRETE RESEARCH, 2022, 154
[53]   Production and properties of ferrite-rich CSAB cement from metallurgical industry residues [J].
Isteri, Visa ;
Ohenoja, Katja ;
Hanein, Theodore ;
Kinoshita, Hajime ;
Tanskanen, Pekka ;
Illikainen, Mirja ;
Fabritius, Timo .
SCIENCE OF THE TOTAL ENVIRONMENT, 2020, 712 (712)
[54]   Studies on the early hydration of two modifications of ye'elimite with gypsum [J].
Jansen, D. ;
Spies, A. ;
Neubauer, J. ;
Ectors, D. ;
Goetz-Neunhoeffer, F. .
CEMENT AND CONCRETE RESEARCH, 2017, 91 :106-116
[55]   Does Ordinary Portland Cement contain amorphous phase? A quantitative study using an external standard method [J].
Jansen, D. ;
Stabler, Ch ;
Goetz-Neunhoeffer, F. ;
Dittrich, S. ;
Neubauer, J. .
POWDER DIFFRACTION, 2011, 26 (01) :31-38
[56]   A remastered external standard method applied to the quantification of early OPC hydration [J].
Jansen, Daniel ;
Goetz-Neunhoeffer, Friedlinde ;
Stabler, Christopher ;
Neubauer, Juergen .
CEMENT AND CONCRETE RESEARCH, 2011, 41 (06) :602-608
[57]   Solidification/stabilization of gold mine tailings using calcium sulfoaluminate-belite cement [J].
Kiventera, Jenni ;
Piekkari, Katri ;
Isteri, Visa ;
Ohenoja, Katja ;
Tanskanen, Pekka ;
Illikainen, Mirja .
JOURNAL OF CLEANER PRODUCTION, 2019, 239
[58]   On the hydration of Belite-Ye'elimite-Ferrite (BYF) cement pastes: Effect of the water-to-cement ratio and presence of fly ash [J].
Koga, Guilherme Yuuki ;
Albert, Blandine ;
Nogueira, Ricardo Pereira .
CEMENT AND CONCRETE RESEARCH, 2020, 137
[59]   Production of high purity rare earth mixture from iron-rich spent fluid catalytic cracking (FCC) catalyst using acid leaching and two-step solvent extraction process [J].
Le-Phuc Nguyen ;
Yen Thi Hai Pham ;
Phuong Thuy Ngo ;
Tri Van Tran ;
Loc Vinh Tran ;
Nam Thi Hoai Le ;
Luong Huu Nguyen ;
Tung Thanh Dang ;
Duc Anh Nguyen ;
Wenzel, Marco ;
Hartmann, David ;
Gloe, Karsten ;
Weigand, Jan J. ;
Kretschmer, Klaus .
KOREAN JOURNAL OF CHEMICAL ENGINEERING, 2018, 35 (05) :1195-1202
[60]   Effect of ZnO on the whiteness of white Portland cement clinker [J].
Li, Jinzhen ;
Cheng, Geling ;
Huang, Shaowen ;
Lian, Pinghua .
CEMENT AND CONCRETE RESEARCH, 2021, 143 (143)