Effects of pressure and plastic addition on sticking of fine iron ore particles in fluidized bed reduction

被引:4
作者
Xu, Qi-yan [1 ]
Gu, Zhang-han [1 ]
Li, Zhi-ping [1 ]
Zhang, Ying-yi [1 ]
Wang, Hai-chuan [1 ]
机构
[1] Anhui Univ Technol, Sch Met Engn, Maanshan 243002, Anhui, Peoples R China
基金
中国国家自然科学基金;
关键词
Fine iron ore; Fluidized bed; Reduction pressure; Plastic particle; Sticking; Reduction; FE2O3; PARTICLES; COATING MGO; MECHANISM; KINETICS; HYDROGEN; CARBON;
D O I
10.1007/s42243-020-00449-2
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The adhesion of fine iron ore particles during fluidized bed reduction was studied using pressurized visible fluidized bed laboratory equipment. The results showed that the optimal operating parameters for pure hydrogen reduction under high pressure were reduction temperature of 1073 K, particle size of 0.18-0.66 mm, pure H(2)linear velocity of 0.8 m/s, reduction pressure of 200 kPa, and reduction time of 50 min. When plastic particles were mixed into the fluidized bed, the optimal parameters were reduction temperature of 973 K, particle size of 0.18-0.66 mm, pure H(2)linear velocity of 0.8 m/s, reduction pressure of 100 kPa, mass content of plastic particles of 8%, and reduction time of 65 min. The chemical reaction resistance is much higher than the inner diffusion resistance at the initial stage of the reaction, whereas, in later stage, the inner diffusion resistance exceeds the chemical reaction resistance. The contact area of iron atoms or iron whiskers gradually decreases with the increase in reduction pressure from 0.20 to 0.45 MPa, and the sticking trend gradually decreases. Adding plastic particles in the fluidized reduction process of fine iron ore can effectively inhibit the adhesion among fine iron ore particles.
引用
收藏
页码:140 / 151
页数:12
相关论文
共 24 条
  • [21] Parameters Optimization, Sticking Mechanism and Kinetics Analysis of Fine Iron Ore in Fluidized-Reduction Process
    Xu, Qiyan
    Wang, Haichuan
    Fu, Yuankun
    Wang, Jianjun
    [J]. ISIJ INTERNATIONAL, 2016, 56 (11) : 1929 - 1937
  • [22] Evolution of microstructure and phase composition of Ti-3Al-5Mo-4.5V alloy with varied β phase stability
    Xue, Q.
    Ma, Y. J.
    Lei, J. F.
    Yang, R.
    Wang, C.
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 34 (12) : 2325 - 2330
  • [23] Characterization of Precipitated Carbon by XPS and Its Prevention Mechanism of Sticking during Reduction of Fe2O3 Particles in the Fluidized Bed
    Zhang, Ben
    Wang, Zhi
    Gong, Xuzhong
    Guo, Zhancheng
    [J]. ISIJ INTERNATIONAL, 2013, 53 (03) : 411 - 418
  • [24] Zhang B, 2011, ISIJ INT, V51, P1403, DOI 10.2355/isijinternational.51.1403