Influence of oxide films on primary water stress corrosion cracking initiation of alloy 600

被引:164
作者
Panter, J
Viguier, B
Cloué, JM
Foucault, M
Combrade, P
Andrieu, E
机构
[1] CNRS, ENSIACET, UPS, Ctr Inter Univ Rech & Ingn Mat,INPT, F-31077 Toulouse 04, France
[2] Framatome France, Ctr Tech, F-71205 Le Creusot, France
关键词
D O I
10.1016/j.jnucmat.2005.10.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study alloy 600 was tested in simulated pressurised water reactor (PWR) primary water, at 360 degrees C, under an hydrogen partial pressure of 30 kPa. These testing conditions correspond to the maximum sensitivity of alloy 600 to crack initiation. The resulting oxidised structures (corrosion scale and underlying metal) were characterised. A chromium rich oxide layer was revealed, the underlying metal being chromium depleted. In addition, analysis of the chemical composition of the metal close to the oxide scale had allowed to detect oxygen under the oxide scale and particularly in a triple grain boundary. Implication of such a finding on the crack initiation of alloy 600 is discussed. Significant diminution of the crack initiation time was observed for sample oxidised before stress corrosion tests. In view of these results, a mechanism for stress corrosion crack initiation of alloy 600 in PWR primary water was proposed. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:213 / 221
页数:9
相关论文
共 30 条
[1]  
ANDRIEU E, 1996, CORROSION DEFORMATIO, P294
[2]  
[Anonymous], ASTM STP
[3]   STRESS-CORROSION CRACKING OF INCONEL ALLOY-600 IN HIGH-TEMPERATURE WATER - AN UPDATE [J].
BANDY, R ;
VANROOYEN, D .
CORROSION, 1984, 40 (08) :425-430
[4]   INTERGRANULAR CORROSION IN WATER VAPOR OF ALLOY OF TYPE INCONEL 600 [J].
BERGE, P .
CORROSION SCIENCE, 1970, 10 (04) :185-&
[5]   THE EMBRITTLEMENT OF NICKEL FOLLOWING HIGH-TEMPERATURE AIR EXPOSURE [J].
BRICKNELL, RH ;
WOODFORD, DA .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (03) :425-433
[6]   THE MECHANISM OF CAVITY FORMATION DURING HIGH-TEMPERATURE OXIDATION OF NICKEL [J].
BRICKNELL, RH ;
WOODFORD, DA .
ACTA METALLURGICA, 1982, 30 (01) :257-264
[7]   Analysis and TEM examination of corrosion scales grown on Alloy 690 exposed to pressurized water at 325°C [J].
Carrette, F ;
Lafont, MC ;
Chatainier, G ;
Guinard, L ;
Pieraggi, B .
SURFACE AND INTERFACE ANALYSIS, 2002, 34 (01) :135-138
[8]  
Cassagne T, 1997, PROCEEDINGS OF THE EIGHTH INTERNATIONAL SYMPOSIUM ON ENVIRONMENTAL DEGRADATION OF MATERIALS IN NUCLEAR POWER SYSTEMS - WATER REACTORS, VOLS 1 AND 2, P307
[9]  
GARDEY S, 1998, THESIS U PM CURIE
[10]  
GATE R, 1993, P PROGR UND PREV COR, P1542