Structural properties and stability of Zr and Ti germanosilicides formed by rapid thermal annealing

被引:8
作者
Aubry-Fortuna, V
Chaix-Pluchery, O
Fortuna, F
Hernandez, C
Campidelli, Y
Bensahel, D
机构
[1] Univ Paris 11, Inst Elect Fondamentale, CNRS, UMR 8622, F-91405 Orsay, France
[2] Ecole Natl Super Phys Grenoble, Mat & Genie Phys Lab, CNRS, UMR 5628, F-38402 St Martin Dheres, France
[3] Univ Paris 11, Ctr Spectrometrie Nucl & Spectrometrie Masse, CNRS, IN2P3, F-91405 Orsay, France
[4] France Telecom, Res & Dev, F-38243 Meylan, France
关键词
D O I
10.1063/1.1462855
中图分类号
O59 [应用物理学];
学科分类号
摘要
Because of their good ohmic and rectifying properties, silicides are routinely used in Si technology. This approach has been recently extended to the novel devices produced using Si1-xGex alloys. Here, we study the Zr and Ti germanosilicides produced in the low thermal budget contact formation during Si/Si1-xGex heterodevice processing. Phase formation was monitored by combining a range of spectrometries with electron microscopy and x-ray diffraction techniques, while sheet resistance measurements allowed correlation of phase formation with film conductance. After completion of the reaction, the final crystalline phase was either C49-Zr(Si1-yGey)(2) in the entire Ge composition (x) range, or C54-Ti(Si1-yGey)(2) in the Ge composition range 0-0.47. In the Zr-Si-Ge system, the C49-Zr(Si1-yGey)(2) formation temperature (T-f) decreases as x increases, and films formed at this temperature are continuous. Excess heating (above T-f) produces islanded films with embedded grains. A most significant feature of the results was that no Ge segregation was detected at any annealing temperature and that the Ge content in the C49 phase (y) remained equal to x for all x. This is in contrast to results on the C54-Ti(Si1-yGey)(2) films, which were discontinuous when x>0.10, and in which Ge segregation occurred in the form of Ge-rich SiGe decorations separating the germanosilicide grains. The Ge content in the final C54 phase (y) was always lower than the value of x in the initial SiGe alloy, and the measured sheet resistance of the corresponding contacts was large. Our results indicate that the alloys formed between Zr and Si1-xGex are good candidates as stable contacts on Si1-xGex, and hence that Zr should be preferred for contacting in Ge-rich SiGe-based applications. (C) 2002 American Institute of Physics.
引用
收藏
页码:5468 / 5473
页数:6
相关论文
共 37 条
[21]   Effects of composition on the formation temperatures and electrical resistivities of C54 titanium germanosilicide in Ti-Si1-xGex systems [J].
Lai, JB ;
Chen, LJ .
JOURNAL OF APPLIED PHYSICS, 1999, 86 (03) :1340-1345
[22]   Pulsed KrF laser annealing of Ni/Si0.76Ge0.24 films [J].
Luo, JS ;
Lin, WT ;
Chang, CY ;
Tsai, WC .
JOURNAL OF APPLIED PHYSICS, 1997, 82 (07) :3621-3623
[23]  
LYUTOVICH K, 1997, P I PHYSICS C SERIES, V157, P131
[24]   HIGH-QUALITY SI1-X-YGEXCY EPITAXIAL LAYERS GROWN ON (100) SI BY RAPID THERMAL CHEMICAL-VAPOR-DEPOSITION USING METHYLSILANE [J].
MI, J ;
WARREN, P ;
LETOUMEAU, P ;
JUDELEWICZ, M ;
GAILHANOU, M ;
DUTOIT, M ;
DUBOIS, C ;
DUPUY, JC .
APPLIED PHYSICS LETTERS, 1995, 67 (02) :259-261
[25]   REFRACTORY SILICIDES FOR INTEGRATED-CIRCUITS [J].
MURARKA, SP .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY, 1980, 17 (04) :775-792
[26]   CoSi2/Si1-xGex/Si(001) heterostructures formed through different reaction routes: Silicidation-induced strain relaxation, defect formation, and interlayer diffusion [J].
Nur, O ;
Willander, M ;
Hultman, L ;
Radamson, HH ;
Hansson, GV ;
Sardela, MR ;
Greene, JE .
JOURNAL OF APPLIED PHYSICS, 1995, 78 (12) :7063-7069
[27]   Schottky and ohmic contacts to doped Si1-x-yGexCy layers [J].
Peterson, JJ ;
Hunt, CE ;
Robinson, M .
SOLID-STATE ELECTRONICS, 1999, 43 (09) :1725-1734
[28]   STRUCTURAL AND ELECTRICAL-PROPERTIES OF ZRSI2 AND ZR2CUSI4 FORMED BY RAPID THERMAL-PROCESSING [J].
SETTON, M ;
VANDERSPIEGEL, J .
JOURNAL OF APPLIED PHYSICS, 1991, 70 (01) :193-197
[29]  
SUKOW CA, 1992, MATER RES SOC SYMP P, V260, P251, DOI 10.1557/PROC-260-251
[30]   INTERFACIAL REACTIONS IN THE ZR-SI SYSTEM STUDIED BY IN-SITU TRANSMISSION ELECTRON-MICROSCOPY [J].
TANAKA, H ;
KONNO, TJ ;
SINCLAIR, R ;
HIRASHITA, N .
JOURNAL OF APPLIED PHYSICS, 1995, 78 (08) :4982-4987