Role of pre-width reduction in deformation behavior of AZ31B alloy during break-down rolling and finish rolling

被引:41
|
作者
Jia, Weitao [1 ]
Ning, Fangkun [1 ]
Ding, Yunpeng [1 ]
Le, Qichi [1 ]
Tang, Yan [1 ]
Cui, Jianzhong [1 ]
机构
[1] Northeastern Univ, Minist Educ, Key Lab Electromagnet Proc Mat, Shenyang 110819, Liaoning, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2018年 / 720卷
基金
中国国家自然科学基金;
关键词
Pre-width reduction; Rolling formability; Pre-rolling; Shear bands; Tensile twins; SEVERE PLASTIC-DEFORMATION; MECHANICAL-PROPERTIES; MAGNESIUM ALLOY; DYNAMIC RECRYSTALLIZATION; ROOM-TEMPERATURE; TEXTURE EVOLUTION; MG ALLOYS; SHEAR BANDS; GRAIN-SIZE; MICROSTRUCTURE;
D O I
10.1016/j.msea.2018.02.015
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Present study aimed at investigating the effect of introducing pre-width reduction (Pre-WR) on microstructure evolution and rolling formability variation during both the break-down rolling and finish rolling of AZ31B alloy. Different rolling routes relevant to the above two rolling processes were performed and compared. Results show that pre-induced twins by pre-rolling (8% thickness reduction) can significantly reduce the edge-cracking depth level during subsequent super-high reduction rolling (SHRR) (80% thickness reduction) through replacing the formation of shear bands by the promotion of the twinning-induced recrystallization to coordinate the severe deformation. However, the dominant behavior of twinning and twinning-induced DRX within the edge region induced a unique partial recrystallization with coarse grains and further a poor rolling formability in SHRR. Introducing more {1012} tensile twins at the edge by Inter-WR (a Pre-WR type with 10% width reduction) before the SHRR can significantly refine the grains and obtain almost a recrystallized homogeneous microstructure. It can also weaken the basal texture of the edge material and further decrease the number/depth level of edge crack by enhancing the activity of both non-basal slips and dominant continuous dynamic recrystallization (CDRX). During finish rolling, heavy twins and shear bands resulted in the larger edge crack level. The improvement of Pre-WR on rolling formability can be inherited to the strip finishing rolling process by evidently reducing the twins and shear bands.
引用
收藏
页码:11 / 23
页数:13
相关论文
共 50 条
  • [1] Role of pre-vertical compression in deformation behavior of Mg alloy AZ31B during super-high reduction hot rolling process
    Jia, Weitao
    Le, Qichi
    Tang, Yan
    Ding, Yunpeng
    Ning, Fangkun
    Cui, Jianzhong
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 34 (11) : 2069 - 2083
  • [2] Optimum rolling speed and relevant temperature-and reduction-dependent interfacial friction behavior during the break-down rolling of AZ31B alloy
    Jia, Weitao
    Tang, Yan
    Ning, Fangkun
    Le, Qichi
    Bao, Lei
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 34 (11) : 2051 - 2062
  • [3] Microstructural and mechanical responses to various rolling speeds determined in multi-pass break-down rolling of AZ31B alloy
    Jia, Weitao
    Tang, Yan
    Ning, Fangkun
    Le, Qichi
    Cui, Jianzhong
    MATERIALS RESEARCH EXPRESS, 2018, 5 (04):
  • [4] Role of pre-vertical compression in deformation behavior of Mg alloy AZ31B during super-high reduction hot rolling process
    Weitao Jia
    Qichi Le
    Yan Tang
    Yunpeng Ding
    Fangkun Ning
    Jianzhong Cui
    Journal of Materials Science & Technology, 2018, 34 (11) : 2069 - 2083
  • [5] Recrystallization behavior and mechanical properties of AZ31B alloy during the hot-rolling process
    Li, Chenhui
    Hou, Hua
    Dong, Ruifeng
    Zhang, Xiaoyang
    Xu, Xiaolong
    Zhao, Yuhong
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 24 : 1005 - 1014
  • [6] Temperature Rise Effect of AZ31B Mg Alloy during Rolling
    Ding Yunpeng
    Zhu Qiang
    Ma Qingwu
    Zhang Zhiqiang
    Le Qichi
    Cui Jianzhong
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (03) : 722 - 727
  • [7] The microstructure evolution in AZ31B alloy during multi-pass cold rolling to a high reduction
    Duan, G. S.
    Wu, B. L.
    Du, X. H.
    Zhao, G.
    Zhang, Y. D.
    Zhao, X.
    Zuo, L.
    Esling, C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 620 : 120 - 128
  • [8] Effect of rolling speed on microstructure and mechanical properties of as-cast AZ31B alloy under different reduction schedules
    Ding, Yunpeng
    Le, Qichi
    Zhang, Zhiqiang
    Cui, Jianzhong
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2016, 233 : 161 - 173
  • [9] EFFECT OF ROLLING TEMPERATURE ON THE AZ31B MAGNESIUM ALLOY MICROSTRUCTURE
    Choquechambi Catorceno, Litzy L.
    Padillha, Angelo F.
    MAGNESIUM TECHNOLOGY 2012, 2012, : 283 - 287
  • [10] Effect of vertical rolling at various temperatures on subsequent multi-pass severe rolling of AZ31B alloy sheet
    Ding, Yunpeng
    Le, Qichi
    Zhang, Zhiqiang
    Bao, Lei
    Cao, Jing
    Cui, Jianzhong
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2013, 213 (12) : 2101 - 2108