Improvement on the crack resistance property of semi-flexible pavement by cement-emulsified asphalt mortar

被引:29
作者
Huang Chong [1 ]
Liu Jiaping [1 ]
Hong Jinxiang [1 ]
Liu Zhifei [1 ]
机构
[1] Jiangsu Bote New Mat Co Ltd, Jiangsu Res Inst Bldg Sci, State Key Lab High Performance Civil Engn Mat, Nanjing 210008, Jiangsu, Peoples R China
来源
GREEN BUILDING MATERIALS III | 2012年 / 509卷
关键词
Semi-flexible pavement (SFP); Lag gap asphalt mixture (LGAM); Cement-emulsified asphalt mortar (CEAM); Cement-emulsified asphalt mortar semi-flexible pavement material (CEAMSFP); Crack resistance property;
D O I
10.4028/www.scientific.net/KEM.509.26
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Semi-flexible pavement (SFP) has some excellent characteristic such as high carrying capacity, good wearing resistance, water stability and durability. However, the SFP appears low temperature crack and fatigue cracking seriously because there are large differences in the interfacial bonding property and the elastic modules between its two major parts: Lag gap asphalt mixture (LGAM) and cement mortar. All of these are caused by the large stiffness of cement mortar. In order to improve the crack resistance property of SFP, six kinds of cement-emulsified asphalt mortars (CEAM) were developed to enhance the adhesive property and reduce the elastic modules. The cement-emulsified asphalt mortar semi-flexible pavement material (CEAMSFP) was obtained by using this kind of CEAM. In the CEAM and the CEAMSFP, six emulsified asphalt-to-cement (A/C) ratios were considered in the study: 0, 0.1, 0.2, 0.3, 0.4 and 0.5 by weight of emulsified asphalt. The results indicated that the increasing of the A/C ratio improved the bonding interface and the flexible of the CEAM. The increasing of the A/C ratio improved the low temperature resistance and fatigue life of the CEAMSFP. It was also shown that the A/C ratio of 0.3 was found to be the optimum ratio that achieved a balance in performance and the value of the pavement. In this condition, the adhesion level between LGAM and cement grout reached 5, the elastic modules of mortar decreased by 62.5% and the fatigue life of SFP increased by 43.6%.
引用
收藏
页码:26 / 32
页数:7
相关论文
共 9 条
[1]  
[Anonymous], 2000, 0522000 JTJ MIN COMM, P150
[2]  
Hassan K. E., 2002, P 4 EUROPEAN S PERFO, P113
[3]   Adsorption behaviour between cement and asphalt emulsion in cement-asphalt mortar [J].
Hu, S. -G. ;
Wang, T. ;
Wang, F. -Z. ;
Liu, Z. -C. .
ADVANCES IN CEMENT RESEARCH, 2009, 21 (01) :11-14
[4]  
KATSUOSHI A., 2001, Q REP RITI, V42, P35, DOI DOI 10.2219/RTRIQR.42.35
[5]  
Merrill D., 2006, International Journal of Pavement Engineering, V7, P101
[6]  
Miura S., 1998, JPN RAIL TRANSPORT R, P38
[7]   Charged, semi-flexible polymers under incompatible solvent conditions [J].
Pereira, G. G. .
CURRENT APPLIED PHYSICS, 2008, 8 (3-4) :347-350
[8]  
Technology Fund, 2008, TEMP TECHN COND EM A
[9]  
WU dan, 2009, RES TATIGYE PROPERTY