High performance of La0.6Sr0.4Co0.2Fe0.8O3-Ce0.9Gd0.1O1.95 nanoparticulate cathode for intermediate temperature microtubular solid oxide fuel cells

被引:80
|
作者
Sumi, Hirofumi [1 ]
Yamaguchi, Toshiaki [1 ]
Hamamoto, Koichi [1 ]
Suzuki, Toshio [1 ]
Fujishiro, Yoshinobu [1 ]
机构
[1] Natl Inst Adv Ind Sci & Technol, Adv Mfg Res Inst, Nagoya, Aichi 4638560, Japan
关键词
Solid oxide fuel cell (SOFC); Perovskite; Cathode; AC impedance; Distribution of relaxation times (DRT); COMPOSITE CATHODES; ELECTROCHEMICAL PERFORMANCE; ELECTRICAL-PROPERTIES; SOFC; ELECTRODES; MECHANISM; LA1-XSRXCO1-YFEYO3; IMPEDANCE; KINETICS;
D O I
10.1016/j.jpowsour.2012.11.015
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The perovskite La0.6Sr0.4Co0.2Fe0.8O3-Ce0.9Gd0.1O1.95 (LSCF-GDC) nanoparticulate cathode was applied for microtubular solid oxide fuel cells operated at intermediate temperatures. For the cell with the cathode sintered at 950 degrees C, maximum power densities of 0.26, 0.54 and 0.73 W cm(-2) were obtained at 550, 600 and 650 degrees C, respectively. The ohmic resistance increased for the cathode sintered at 850 degrees C, and the polarization resistance increased for the cathode sintered at 1050 degrees C. The cathode polarization resistances of ionic conduction process in the LSCF bulk and adsorption/desorption process on the LSCF surface were estimated by the distribution of relaxation times analysis, which were only 0.066 and 0.065 Omega cm(2) at 600 degrees C for the cathode sintered at 950 degrees C. The grain size of the cathode was less than 100 nm, which resulted in high performance due to an overall decrease in cathode polarization resistance. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:354 / 358
页数:5
相关论文
共 50 条
  • [41] Synthesis and characterization of La0.6Sr0.4Fe0.8Cu0.2O3-δ oxide as cathode for Intermediate Temperature Solid Oxide Fuel Cells
    Vazquez, Santiago
    Davyt, Sebastian
    Basbus, Juan E.
    Soldati, Analia L.
    Amaya, Alejandro
    Serquis, Adriana
    Faccio, Ricardo
    Suescun, Leopoldo
    JOURNAL OF SOLID STATE CHEMISTRY, 2015, 228 : 208 - 213
  • [42] TiO2-modified La0.6Sr0.4Co0.2Fe0.8O3-δ cathode for intermediate temperature solid oxide fuel cells
    Liu, Weixing
    Zhao, Zhe
    Tu, Baofeng
    Cui, Daan
    Ou, Dingrong
    Cheng, Mojie
    CHINESE JOURNAL OF CATALYSIS, 2015, 36 (04) : 502 - 508
  • [43] Stability of La0.6Sr0.4Co0.2Fe0.8O3/Ce0.9Gd0.1O2 cathodes during sintering and solid oxide fuel cell operation
    Kiebach, Ragnar
    Zhang, Wei-Wei
    Zhang, Wei
    Chen, Ming
    Norrman, Kion
    Wang, Hsiang-Jen
    Bowen, Jacob R.
    Barfod, Rasmus
    Hendriksen, Peter Yang
    JOURNAL OF POWER SOURCES, 2015, 283 : 151 - 161
  • [44] Liquid plasma sprayed nano-network La0.4Sr0.6Co0.2Fe0.8O3/Ce0.8Gd0.2O2 composite as a high-performance cathode for intermediate-temperature solid oxide fuel cells
    Zhang, Shan-Lin
    Li, Chang-Jiu
    Li, Cheng-Xin
    Yang, Guan-Jun
    Huang, Kevin
    Liu, Meilin
    JOURNAL OF POWER SOURCES, 2016, 327 : 622 - 628
  • [45] Interface engineering of La0.6Sr0.4Co0.2Fe0.8O3-δ/ Gd0.1Ce0.9O1.95 heterostructure oxygen electrode for solid oxide electrolysis cells with enhanced CO2 electrolysis performance
    Yang, Caichen
    Wang, Ziling
    Tan, Yuan
    Pu, Jian
    Chi, Bo
    CHEMICAL ENGINEERING JOURNAL, 2024, 498
  • [46] Silver infiltrated La0.6Sr0.4Co0.2Fe0.8O3 cathodes for intermediate temperature solid oxide fuel cells
    Sakito, Y.
    Hirano, A.
    Imanishi, N.
    Takeda, Y.
    Yamamoto, O.
    Liu, Y.
    JOURNAL OF POWER SOURCES, 2008, 182 (02) : 476 - 481
  • [47] Evaluation of polarization and hydrogen production efficiency of solid oxide electrolysis stack with La0.6Sr0.4Co0.2Fe0.8O3-δ- Ce0.9Gd0.1O1.95 oxygen electrode
    Liu, Tong-Le
    Wang, Cheng
    Hao, Si-Jia
    Fu, Zhi-Qiang
    Peppley, Brant A.
    Mao, Zhi-Ming
    Wang, Jian-Long
    Mao, Zong-Qiang
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2016, 41 (36) : 15970 - 15978
  • [48] Interaction of La0.8Sr0.2MnO3 interlayer with Gd0.1Ce0.9O1.95 electrolyte membrane and Ba0.5Sr0.5Co0.8Fe0.2O3-δ cathode in low-temperature solid oxide fuel cells
    Yang, Min
    Zhang, Min
    Yan, Aiyu
    Yue, Mangling
    Hou, Zhifang
    Dong, Yonglai
    Cheng, Mojie
    JOURNAL OF POWER SOURCES, 2008, 185 (02) : 784 - 789
  • [49] La0.6Sr0.4Co0.2Fe0.8O3-δ Current Collectors via Ag Infiltration for Microtubular Solid Oxide Fuel Cells with Intermediate Temperature Operation
    Mori, Masashi
    Liu, Yu
    Itoh, Takanori
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2009, 156 (10) : B1182 - B1187
  • [50] Fabrication of Ba0.5Sr0.5Co0.8Fe0.2O3-delta (BSCF)/Ce0.9Gd0.1O2-delta (GDC) and La0.6Ba0.4Co0.2Fe0.8O3-delta (LBCF)/Ce0.9Gd0.1O2-delta (GDC) Composite Cathodes for Intermediate Temperature Solid Oxide Fuel Cells
    Lee, Seunghun
    Yoon, Song Seol
    Cha, Young Chul
    Lee, Jun
    Hwang, Hae Jin
    Moon, Ji-Woong
    JOURNAL OF THE KOREAN CERAMIC SOCIETY, 2007, 44 (12) : 740 - 746