0.12 mu m hole pattern formation by KrF lithography for giga bit DRAM

被引:19
作者
Nakao, S
Nakae, A
Yamaguchi, A
Kimura, H
Ohno, Y
Matsui, Y
Hirayama, M
机构
来源
IEDM - INTERNATIONAL ELECTRON DEVICES MEETING, TECHNICAL DIGEST 1996 | 1996年
关键词
D O I
10.1109/IEDM.1996.553122
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Dense 0.10 mu m hole pattern formation has been achieved by optical lithography with KrF wavelength. Double exposure utilizing two alternative phase shift masks of lines and spaces pattern produces dense small hole images with enough focus and exposure latitudes. Applying this method with a KrF stepper and chemically-amplified negative-tone resist, 2-dimensional 0.13 mu m hole array with the pitch of 0.40 mu m has been resolved with 1.0 mu m DOF, and resolution limit size and pitch are less than 0.10 mu m and 0.28 mu m, respectively.
引用
收藏
页码:61 / 64
页数:4
相关论文
共 44 条
[31]   FORMATION OF MONOLITHIC MASKS FOR 0.25-MU-M X-RAY-LITHOGRAPHY [J].
CELLER, GK ;
TRIMBLE, LE ;
FRACKOVIAK, J ;
JURGENSEN, CW ;
KOLA, RR ;
NOVEMBRE, AE ;
WEBER, GR .
APPLIED PHYSICS LETTERS, 1991, 59 (24) :3105-3107
[32]   0.10 μm dense hole pattern formation by double exposure utilizing alternating phase shift mask using KrF excimer laser as exposure light [J].
Nakao, S ;
Nakae, A ;
Yamaguchi, A ;
Tsujita, K ;
Wakamiya, W .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1999, 38 (5A) :2686-2693
[33]   0.10 μm dense hole pattern formation by double exposure utilizing alternating phase shift mask using KrF excimer laser as exposure light [J].
Nakao, Shuji ;
Nakae, Akihiro ;
Yamaguchi, Atsumi ;
Tsujita, Kouichirou ;
Wakamiya, Wataru .
Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 1999, 38 (5 A) :2686-2693
[34]   ANALYSIS OF SUB-0.15 MU-M PATTERN REPLICATION IN SYNCHROTRON-RADIATION LITHOGRAPHY [J].
KIKUCHI, Y ;
KONDO, K ;
NOMURA, H ;
GOMEI, Y .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 1993, 32 (12B) :5960-5965
[35]   CROSS SHAPED PATTERN ON CHROME MASK FOR 0.5 MU-M CONTACT HOLE FABRICATION [J].
LOONG, WA ;
SHY, SL ;
GUO, GC ;
YANG, MT ;
SU, SY .
MICROELECTRONIC ENGINEERING, 1994, 23 (1-4) :175-178
[36]   0.2 mu m hole pattern generation by critical dimension biassing using resin overcoat [J].
Yamauchi, T ;
Matsui, T ;
Kanamori, J ;
Miyakawa, Y ;
Shimoyama, K .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1995, 34 (12B) :6615-6621
[37]   PATTERNING CHARACTERISTICS OF 0.1-MU-M LINE-AND-SPACE PATTERN IN SYNCHROTRON-RADIATION LITHOGRAPHY [J].
SOMEMURA, Y ;
DEGUCHI, K ;
MIYOSHI, K .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 1994, 33 (11) :6389-6395
[38]   A proposal of a composite phase-shifting mask for 0.15-μm hole-pattern delineation using KrF exposure [J].
Hasegawa, N ;
Hayano, K ;
Imai, A ;
Asai, N ;
Okazaki, S .
OPTICAL MICROLITHOGRAPHY XI, 1998, 3334 :522-531
[39]   Below 100-nm hole pattern formation using resolution enhancement lithography assisted by chemical shrink (RELACSTM) [J].
Toyoshima, T ;
Ishibashi, T ;
Yasuda, N ;
Tarutani, S ;
Kanda, T ;
Takahashi, K ;
Takano, Y ;
Tanaka, H .
JOURNAL OF PHOTOPOLYMER SCIENCE AND TECHNOLOGY, 2002, 15 (03) :377-378
[40]   Rapid formation of arsenic-doped layer more than 1.0 mu m deep in Si using two KrF excimer lasers [J].
Jyumonji, M ;
Sugioka, K ;
Takai, H ;
Toyoda, K .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1995, 34 (12B) :6878-6881