Electrochemical characteristics of the dynamic progression of erosion-corrosion under different flow conditions and their effects on corrosion rate calculation

被引:23
作者
Xu, Yunze [1 ,2 ]
Liu, Liang [1 ]
Xu, Chenbing [1 ]
Wang, Xiaona [3 ]
Tan, Mike Yongjun [4 ]
Huang, Yi [1 ]
机构
[1] Dalian Univ Technol, Sch Naval Architecture & Ocean Engn, Linggong Rd 2, Dalian 116024, Liaoning, Peoples R China
[2] Dalian Univ Technol, Sch Civil Engn, Dalian 116024, Peoples R China
[3] Dalian Univ Technol, Sch Phys & Optoelect Engn, Dalian 116024, Peoples R China
[4] Deakin Univ, Sch Engn, Geelong, Vic 3216, Australia
基金
中国博士后科学基金;
关键词
Erosion-corrosion; Dynamic progression; Electrochemical parameters; Critical impact energy; CARBON-STEEL; ACCELERATED CORROSION; ENHANCED CORROSION; NACL SOLUTION; SURFACE; RESISTANCE; INITIATION; MECHANISM; VELOCITY; KINETICS;
D O I
10.1007/s10008-020-04795-9
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The erosion-corrosion performance of X65 carbon steel at different flow conditions was electrochemically studied. Results show that the anodic polarization branch would have a significant distortion in the flowing electrolytes, leading to an overestimation of the Stern-Geary coefficient using the traditional Tafel extrapolation. It is found that the critical impact energy for the initiation of erosion-corrosion is around 0.016 mu J. Surface morphology was obviously changed from "flow mark" appearance to continuous craters with the initiation of erosion-corrosion. The results indicate that the synergy of erosion and corrosion is the main factor contributing to the erosion-corrosion damage under active corrosion. The dynamic progression of erosion-corrosion is associated with the propagation of impingement pits at anodic sites and the wear of the corrosion product film at cathodic sites.
引用
收藏
页码:2511 / 2524
页数:14
相关论文
共 50 条
  • [41] Erosion-Corrosion of AISI 302 Stainless Steel Sudden Expansion Pipes in High Salt Wastewater: Effect of Fluid Flow on Different Positions of a Sudden Expansion Pipe
    Wang, Weibing
    Ren, Yongsheng
    CORROSION, 2021, 77 (04) : 461 - 469
  • [42] Erosion corrosion characteristics of X80 pipeline steel in two-phase flow under the influence of multiple factors
    Ye F.
    Yao J.
    Liu Y.
    Zhao Y.
    Dong S.
    Zhao, Yanlin (ylzhao@cup.edu.cn), 1600, Materials China (40): : 6450 - 6459
  • [43] Erosion Corrosion Characteristics of Al5052-O and Al6061-T6 Aluminum Alloys with Flow Rate of Seawater
    Kim, Young-Bok
    Kim, Seong-Jong
    CORROSION SCIENCE AND TECHNOLOGY-KOREA, 2019, 18 (06): : 292 - 299
  • [44] Electrochemical Corrosion Characteristics of 316L Stainless Steel in Simulated Coastal Gold Mine Wastewater under Different pH
    Zhu, Liyi
    Yang, Peng
    Lyu, Wensheng
    Wang, Qixuan
    Wang, Kun
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2022, 17 (09):
  • [45] Effects of the Area of a Duplex Stainless Steel Exposed to Corrosion on the Cathodic and Anodic Reactions in a LiBr Solution Under Static and Dynamic Conditions
    Garcia-Garcia, D. M.
    Blasco-Tamarit, E.
    Garcia-Anton, J.
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2011, 6 (05): : 1237 - 1249
  • [46] Dynamic corrosion behavior of 316L stainless steel in quaternary nitrate-nitrite salts under different flow rates
    Ma, Lina
    Zhang, Cancan
    Wu, Yuting
    Lu, Yuanwei
    Ma, Chongfang
    SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2020, 218
  • [47] Reliability of the estimation of uniform corrosion rate of Q235B steel under simulated marine atmospheric conditions by electrochemical noise (EN) analyses
    Xia, Da-Hai
    Ma, Chao
    Behnamian, Yashar
    Ao, Sansan
    Song, Shizhe
    Xu, Likun
    MEASUREMENT, 2019, 148
  • [48] Flow accelerated corrosion rate on carbon steel pipe bend by thin layer activation technique and computational modeling: Under PHWR operating conditions
    Madasamy, P.
    Chandramohan, P.
    Mukunthan, M.
    Mohan, T. V. Krishna
    Rangarajan, S.
    Uttam, Niraj
    Ramakrishnan, R.
    Babulal, G.
    Rani, H. P.
    Surendran, P.
    Gupta, A. K.
    Nair, J. P.
    ENGINEERING FAILURE ANALYSIS, 2021, 121
  • [49] 2-Benzylsulfanyl-1H-benzimidazole and its mixture as highly efficient corrosion inhibitors for carbon steel under dynamic supercritical CO2 flow conditions
    Wang, Xintong
    Yang, Jiang
    Chen, Xu
    CORROSION SCIENCE, 2024, 235
  • [50] Role of Chloride Ion and Dissolved Oxygen in Electrochemical Corrosion of AA5083-H321 Aluminum-Magnesium Alloy in NaCl Solutions under Flow Conditions
    K.Jafarzadeh
    T.Shahrabi
    S.M.M.Hadavi
    M.G.Hosseini
    Journal of Materials Science & Technology, 2007, (05) : 623 - 628