Electrochemical characteristics of the dynamic progression of erosion-corrosion under different flow conditions and their effects on corrosion rate calculation

被引:23
|
作者
Xu, Yunze [1 ,2 ]
Liu, Liang [1 ]
Xu, Chenbing [1 ]
Wang, Xiaona [3 ]
Tan, Mike Yongjun [4 ]
Huang, Yi [1 ]
机构
[1] Dalian Univ Technol, Sch Naval Architecture & Ocean Engn, Linggong Rd 2, Dalian 116024, Liaoning, Peoples R China
[2] Dalian Univ Technol, Sch Civil Engn, Dalian 116024, Peoples R China
[3] Dalian Univ Technol, Sch Phys & Optoelect Engn, Dalian 116024, Peoples R China
[4] Deakin Univ, Sch Engn, Geelong, Vic 3216, Australia
基金
中国博士后科学基金;
关键词
Erosion-corrosion; Dynamic progression; Electrochemical parameters; Critical impact energy; CARBON-STEEL; ACCELERATED CORROSION; ENHANCED CORROSION; NACL SOLUTION; SURFACE; RESISTANCE; INITIATION; MECHANISM; VELOCITY; KINETICS;
D O I
10.1007/s10008-020-04795-9
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The erosion-corrosion performance of X65 carbon steel at different flow conditions was electrochemically studied. Results show that the anodic polarization branch would have a significant distortion in the flowing electrolytes, leading to an overestimation of the Stern-Geary coefficient using the traditional Tafel extrapolation. It is found that the critical impact energy for the initiation of erosion-corrosion is around 0.016 mu J. Surface morphology was obviously changed from "flow mark" appearance to continuous craters with the initiation of erosion-corrosion. The results indicate that the synergy of erosion and corrosion is the main factor contributing to the erosion-corrosion damage under active corrosion. The dynamic progression of erosion-corrosion is associated with the propagation of impingement pits at anodic sites and the wear of the corrosion product film at cathodic sites.
引用
收藏
页码:2511 / 2524
页数:14
相关论文
共 50 条
  • [21] The mechanism of erosion-corrosion of API X65 steel under turbulent slurry flow: Effect of nominal flow velocity and oxygen content
    Aguirre, Javiera
    Walczak, Magdalena
    Rohwerder, Michael
    WEAR, 2019, 438
  • [22] Effects of laser surface melting on erosion-corrosion of X65 steel in liquid-solid jet impingement conditions
    Zhao, Weimin
    Wang, Chun
    Zhang, Timing
    Yang, Min
    Han, Bin
    Neville, Anne
    WEAR, 2016, 362 : 39 - 52
  • [23] Determination of the critical flow velocities for erosion-corrosion of passive materials under impingement by NaCl solution containing sand
    Zheng, Z. B.
    Zheng, Y. G.
    Zhou, X.
    He, S. Y.
    Sun, W. H.
    Wang, J. Q.
    CORROSION SCIENCE, 2014, 88 : 187 - 196
  • [24] Design of an elbow for integrated gravimetric, electrochemical and acoustic emission measurements in erosion-corrosion pipe flow environments
    Owen, Joshua
    Ducker, Edward
    Huggan, Michael
    Ramsey, Callum
    Neville, Anne
    Barker, Richard
    WEAR, 2019, 428 : 76 - 84
  • [25] Effects of flow velocity and impact angle on erosion-corrosion of an API-5 L X65 steel coated by plasma nitriding of hard chromium underlayer
    Rameshk, M.
    Soltanieh, M.
    Masoudpanah, S. M.
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (05): : 10054 - 10061
  • [26] Effects of erosion rate on the erosion-corrosion synergism of high velocity oxy-fuel sprayed Ni-based coatings
    Zhang, An-Feng
    Wang, Yu-Yue
    Li, Chang-jiu
    SURFACE ENGINEERING (ICSE 2007), 2008, 373-374 : 585 - +
  • [28] Influence of metallic matrix on erosion-corrosion behaviour of high chromium cast irons under slurry impingement conditions
    Giourntas, L.
    Brownlie, F.
    Hodgkiess, T.
    Galloway, A. M.
    WEAR, 2021, 477
  • [29] Role of the Jet Angle, Particle Size, and Particle Concentration in the Degradation Behavior of Carbon Steel under Slow Slurry Erosion-Corrosion Conditions
    Rasse, Charles
    Mary, Nicolas
    Abe, Hiroshi
    Watanabe, Yutaka
    Normand, Bernard
    METALS, 2021, 11 (08)
  • [30] Synergistic effects of fluid flow and sand particles on erosion-corrosion of aluminum in ethylene glycol-water solutions