Bioactive glass;
Surfaces;
Chemical properties;
Corrosion;
Apatite;
D O I:
10.1016/j.jeurceramsoc.2012.01.025
中图分类号:
TQ174 [陶瓷工业];
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
In vitro bioactivity of glasses is usually measured in buffered solutions whereby a formation of a hydroxyapatite layer on the surface is taken as an indication of the bioactivity. In this work we compare the layer formation on three glasses in simulated body fluid, Tris buffer solution, sodium phosphate buffered saline and osteoblast medium. Two of the glasses are known bioactive glasses, 45S5 (45 wt.% SiO2) and S53P4 (53 wt.% SiO2), while the third is an experimental composition with a higher silica content (68 wt.% SiO2). Plates of the glasses were immersed in the solutions at 37 degrees C for different times up to two weeks. The results showed clear differences between the layer developments on the three glasses in the different solutions. The results indicated that the relative order of the reactivity depended on the solution. Thus, results gained in different solutions for different glasses cannot be directly compared. (c) 2012 Elsevier Ltd. All rights reserved.
机构:
Chinese Acad Sci, Shanghai Inst Ceram, Biomat & Tissue Engn Res Ctr, Shanghai 200050, Peoples R China
Chinese Acad Sci, Grad Sch, Shanghai 200031, Peoples R ChinaChinese Acad Sci, Shanghai Inst Ceram, Biomat & Tissue Engn Res Ctr, Shanghai 200050, Peoples R China
Gao, Yuan
Chang, Jiang
论文数: 0引用数: 0
h-index: 0
机构:
Chinese Acad Sci, Shanghai Inst Ceram, Biomat & Tissue Engn Res Ctr, Shanghai 200050, Peoples R ChinaChinese Acad Sci, Shanghai Inst Ceram, Biomat & Tissue Engn Res Ctr, Shanghai 200050, Peoples R China