Fatigue and fracture behaviour of austenitic-martensitic high carbon steel under high cycle fatigue: An experimental investigation

被引:28
作者
Banerjee, Amborish [1 ]
Prusty, B. Gangadhara [1 ]
机构
[1] UNSW Sydney, Sch Mech & Mfg Engn, ARC Training Ctr Automated Mfg Adv Composites AMA, Sydney, NSW, Australia
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2019年 / 749卷
基金
澳大利亚研究理事会;
关键词
High cycle fatigue; Steel; S-N curve; Microstructure; Stress intensity factor; Bright granular facet; HIGH-STRENGTH STEEL; CRACK INITIATION; BEARING STEEL; LIFE REGIME; MICROSTRUCTURE; MECHANISM; DEFORMATION; PROPAGATION; INCLUSION; DEFECT;
D O I
10.1016/j.msea.2019.02.010
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Dual-phase high carbon steels are widely used in mining industries for grinding applications and are thus subjected to repetitive loading for a very large number of cycles. This paper presents the high-cycle fatigue behaviour of austenitic-martensitic high carbon steel and establishes a concurrent structure-property relationship. Cantilever-type rotating bending fatigue test was carried out on hourglass specimens in the high cycle and very high cycle fatigue (VHCF) regime under ambient condition. The S-N curve exhibited a bilinear slope indicating a change in the mode of crack initiation and micromechanism of cyclic deformation. Based on the fracture surface examination, the initiation of the fatigue cracks was categorised into two groups: (a) surface induced (SI) cracks in short life region and (b) non-inclusion (NI) induced subsurface cracks with a fish-eye formation for the long life region. The stress intensity factor at the periphery of the GBF (Delta K-GBF) was observed in the range of 5.2-5.75 MPa m(1/2) which is close to the crack growth effective threshold value. The Kernel average misorientation (KAM) maps revealed that intense localised deformation occurred at the interface of the austenite-martensite phases and then gradually decreased at the interior of the austenite grains. This observation was supported by the transmission electron microscopy (TEM) studies which showed the pile-up of dislocation at the phase boundaries. The three-dimensional surface roughness parameters were found to be increasing with an increase in the number of fatigue cycles thus indicating the increase in the dislocation activity of the material in the long life regime.
引用
收藏
页码:79 / 88
页数:10
相关论文
共 50 条
[31]   The role of extrusions and intrusions in fatigue crack initiation [J].
Polak, J. ;
Mazanova, V. ;
Heczko, M. ;
Petras, R. ;
Kubena, I. ;
Casalena, L. ;
Man, J. .
ENGINEERING FRACTURE MECHANICS, 2017, 185 :46-60
[32]   High-cycle fatigue behavior of low-C medium-Mn high strength steel with austenite-martensite submicron-sized lath-like structure [J].
Qi, X. Y. ;
Du, L. X. ;
Hu, J. ;
Misra, R. D. K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 718 :477-482
[33]   Investigating the effect of applied strain rate in a single breakage event [J].
Saeidi, Fatemeh ;
Yahyaei, Mohsen ;
Powell, Malcolm ;
Tavares, Luis Marcelo .
MINERALS ENGINEERING, 2017, 100 :211-222
[34]   Fatigue crack initiation behavior in embrittled austenitic-ferritic stainless steel [J].
Sahu, J. K. ;
Krupp, U. ;
Christ, H. -J. .
INTERNATIONAL JOURNAL OF FATIGUE, 2012, 45 :8-14
[35]   Low cycle fatigue behaviour of duplex stainless steel: influence of isothermal aging treatment [J].
Sahu, J. K. ;
Ghosh, R. N. ;
Christ, H. -J. .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2010, 33 (02) :77-86
[36]   Microscopic and nanoscopic observations of metallurgical structures around inclusions at interior crack initiation site for a bearing steel in very high-cycle fatigue [J].
Sakai, T. ;
Oguma, N. ;
Morikawa, A. .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2015, 38 (11) :1305-1314
[37]   Characteristic S-N properties of high-carbon-chromium-bearing steel under axial loading in long-life fatigue [J].
Sakai, T ;
Sato, Y ;
Oguma, N .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2002, 25 (8-9) :765-773
[38]   Twinning and martensite in a 304 austenitic stainless steel [J].
Shen, Y. F. ;
Li, X. X. ;
Sun, X. ;
Wang, Y. D. ;
Zuo, L. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 552 :514-522
[39]   Subsurface crack initiation and propagation mechanism in high-strength steel in a very high cycle fatigue regime [J].
Shiozawa, K. ;
Morii, Y. ;
Nishino, S. ;
Lu, L. .
INTERNATIONAL JOURNAL OF FATIGUE, 2006, 28 (11) :1521-1532
[40]   Transition of fatigue failure mode of Ni-Cr-Mo low-alloy steel in very high cycle regime [J].
Shiozawa, K. ;
Murai, M. ;
Shimatani, Y. ;
Yoshimoto, T. .
INTERNATIONAL JOURNAL OF FATIGUE, 2010, 32 (03) :541-550