Bonding strength between a hard chairside reline resin and a denture base material as influenced by surface treatment

被引:43
作者
Leles, CR [1 ]
Machado, AL [1 ]
Vergani, CE [1 ]
Giampaolo, ET [1 ]
Pavarina, AC [1 ]
机构
[1] Univ Estadual Paulista, Fac Odontol Araraquara, Dept Dent Mat & Prosthodont, Araraquara Dent Sch, Sao Paulo, Brazil
关键词
reline resin; bond strength; denture base resin; removable prosthodontics;
D O I
10.1046/j.1365-2842.2001.00786.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Direct relining of dentures made with hard chairside reline resins is faster than laboratory-processed reline systems and the patient is not without the prosthesis for the time necessary to perform the laboratory procedures. However, a weak bond between the autopolymerizing acrylic reline resins and the denture base material has been observed. This study evaluated the effect of six different surface treatments on the bond strength between a hard chairside reline acrylic resin and ia heat-cured acrylic resin. Specimens of the heat-cured acrylic resin were divided into seven groups. one of these groups remained intact. In the other groups, a 10-mm square section was removed from the centre of each specimen. The bonding surfaces were then treated with (i) methyl methacrylate monomer, (ii) isobutyl methacrylate monomer, (iii) chloroform, (iv) acetone, (v) experimental adhesive and (vi) no surface treatment-control group. Kooliner acrylic resin was packed,into the square sections and polymerized. The bonding strength was evaluated by a three-point loading test. The results were submitted to one-way analysis of variance (ANOVA) followed by a Tukey multiple range test at a 5% level of significance. No significant difference was found between the surface treatment with Lucitone 550 monomer or chloroform, but both were stronger than the majority of the other groups. The bond strength provided by all the surface treatments was lower than that of the intact heat-cured resin.
引用
收藏
页码:1153 / 1157
页数:5
相关论文
共 19 条
[1]  
[Anonymous], 1975, J AM DENT ASSOC, V90, P451
[2]   A COMPARISON OF BOND STRENGTHS AMONG CHAIRSIDE HARD RELINE MATERIALS [J].
ARENA, CA ;
EVANS, DB ;
HILTON, TJ .
JOURNAL OF PROSTHETIC DENTISTRY, 1993, 70 (02) :126-131
[3]   Composition and effect of denture base resin surface primers for reline acrylic resins [J].
Arima, T ;
Nikawa, H ;
Hamada, T .
JOURNAL OF PROSTHETIC DENTISTRY, 1996, 75 (04) :457-462
[4]   Analysis of composition and structure of hard autopolymerizing reline resins [J].
Arima, T ;
Murata, H ;
Hamada, T .
JOURNAL OF ORAL REHABILITATION, 1996, 23 (05) :346-352
[5]   EVALUATION OF HARD DIRECT RELINE RESINS [J].
BUNCH, J ;
JOHNSON, GH ;
BRUDVIK, JS .
JOURNAL OF PROSTHETIC DENTISTRY, 1987, 57 (04) :512-519
[6]   Tensile bond strengths of hard chairside reline resins as influenced by water storage [J].
Cucci, ALM ;
Rached, RN ;
Giampaolo, ET ;
Vergani, CE .
JOURNAL OF ORAL REHABILITATION, 1999, 26 (08) :631-634
[7]   Unrestricted linear dimensional changes of two hard chairside reline resins and one heat-curing acrylic resin [J].
Cucci, ALM ;
Giampaolo, ET ;
Leonardi, P ;
Vergani, CE .
JOURNAL OF PROSTHETIC DENTISTRY, 1996, 76 (04) :414-417
[8]   Water sorption, solubility, and bond strength of two autopolymerizing acrylic resins and one heat-polymerizing acrylic resin [J].
Cucci, ALM ;
Vergani, CE ;
Giampaolo, ET ;
Afonso, MCDF .
JOURNAL OF PROSTHETIC DENTISTRY, 1998, 80 (04) :434-438
[9]   SHEAR BOND STRENGTH OF VISIBLE-LIGHT-CURED RESIN RELATIVE TO HEAT-CURED RESIN [J].
CURTIS, DA ;
EGGLESTON, TL ;
MARSHALL, SJ ;
WATANABE, LG .
DENTAL MATERIALS, 1989, 5 (05) :314-318
[10]  
*INT ORG STAND, 1988, 1567 ISO