Microstructure and oxidation behaviour of Pt modified NiCrAlYSi coating on a Ni-based single crystal superalloy

被引:15
作者
Sun, J. [1 ]
Xiao, H. [3 ]
Li, W. [2 ]
Liu, S. B. [2 ]
Fu, L. B. [2 ]
Jiang, S. M. [2 ]
机构
[1] Qilu Univ Technol, Adv Res Inst Multidisciplinary Sci, Shandong Acad Sci, 3501 Daxue Rd, Jinan 250353, Peoples R China
[2] Chinese Acad Sci, Inst Met Res, 72 Wenhua Rd, Shenyang 110016, Peoples R China
[3] Beihang Univ, Sch Chem, Beijing 100191, Peoples R China
关键词
NiCrAlYSi coating; Superalloys; Arc ion plating; Platinum; Oxidation; THERMAL BARRIER SYSTEMS; BOND COAT; INTERDIFFUSION BEHAVIOR; CYCLIC OXIDATION; NICOCRAL ALLOY; EVOLUTION; PLATINUM; CORROSION; NICKEL; GROWTH;
D O I
10.1016/j.surfcoat.2020.126164
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, the N + NiCrAlYSi coating and NiCrAlYSi + N coating were produced onto the Ni-based single crystal superalloy by using the arc ion plating (AIP) and electroplating. For the N + NiCrAlYSi coating, the N mainly distributed in substrate and the bottom of coating, while the N primarily located at the outer part of NiCrAlYSi + N coating. After isothermal oxidation at 1100 degrees C, the weight gains for the NiCrAlYSi coating, N + NiCrAlYSi coating and NiCrAlYSi + N coating were 1.81 mg/cm(2), 1.68 mg/cm(2) and 1.37 mg/cm(2), respectively. The parabolic rate constant of the NiCrAlYSi +N coating was 6.2 x 10(-3) mg(2) cm(-4) h(-1), which was the smallest among three kinds of coatings. The mass of spalled oxides for the NiCrAlYSi coating, N + NiCrAlYSi coating and NiCrAlYSi + N coating were 2.07 mg/cm(2), 0.937 mg/cm(2) and 0.801 mg/cm(2) after cyclic oxidation at 1150 degrees C. So, the addition of N in the NiCrA1YSi coating can significantly improve the adhesion of alumina scale. The oxidation WA results indicated that the NiCrAlYSi + N coating showed the best oxidation resistance. Some Pt-rich particles were observed on the surface of the NiCrAlYSi + N coating after 1 cycle at 1150 degrees C. The enrichment of N on the outer part of NiCrAlYSi + N coating can increase the out diffusion flux of Al and promote the fast formation of pure Al2O3 at the early stage of oxidation.
引用
收藏
页数:13
相关论文
共 50 条
[41]   Hot corrosion of sputtered nanocrystalline coating with and without preoxidation and arc ion plating coating on a Ni-based single-crystal superalloy [J].
Yang, Xiaowen ;
Lu, Yiliang ;
Wang, Jinlong ;
Chen, Zehao ;
Zhang, Qiang ;
Chen, Minghui ;
Zhang, Jianqiang ;
Wang, Fuhui .
APPLIED SURFACE SCIENCE, 2025, 679
[42]   Effect of Y on Oxidation Behavior of Directionally Solidified Ni-Based Single-Crystal Superalloy [J].
Zhao, Zihan ;
Guan, Kai ;
Cui, Renjie ;
Qin, Jianchao ;
Huang, Zhaohui .
CHINESE JOURNAL OF MECHANICAL ENGINEERING, 2024, 37 (01)
[43]   Synthesis and characterization of a Pt-Al-Cr-Ni γ/γ′-coating on the Ni-based superalloy CMSX-4 [J].
Terock, M. ;
Fleischmann, E. ;
Hochmuth, C. ;
Voelkl, R. ;
Glatzel, U. .
SURFACE & COATINGS TECHNOLOGY, 2013, 236 :347-352
[44]   Oxidation behavior of GTD111 Ni-based superalloy at 900 °C in air [J].
Brenneman, J. ;
Wei, J. ;
Sun, Z. ;
Liu, L. ;
Zou, G. ;
Zhou, Y. .
CORROSION SCIENCE, 2015, 100 :267-274
[45]   Isothermal oxidation of Pt modified and Ru modified aluminide coating on a fourth generation single crystal superalloy [J].
Matsuoka, Yuki ;
Matsunaga, Yasuo ;
Nakagawa, Kiyokazu ;
Taniguchi, Shigeji .
HIGH-TEMPERATURE OXIDATION AND CORROSION 2005, 2006, 522-523 :301-308
[46]   ISOTHERMAL OXIDATION BEHAVIOR OF Al-Cr COATING ON Ni-BASED SUPERALLOY [J].
Wu Duoli ;
Jiang Sumeng ;
Fan Qixiang ;
Gong Jun ;
Sun Chao .
ACTA METALLURGICA SINICA, 2014, 50 (10) :1170-1178
[47]   Role of as-cast dendritic microstructure in recrystallization of a Ni-based single crystal superalloy [J].
Li Zhonglin ;
Zhang Dandan ;
Su Xianglin ;
Xu Qingyan ;
Liu Baicheng .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 660 :115-124
[48]   Microstructure evolution and analysis of a single crystal Ni-based superalloy during heat treatment [J].
Wang, Chuntao ;
Tian, Sugui ;
Wang, Minggang ;
Yu, Xingfu ;
Zhang, Luting .
Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2007, 36 (01) :46-49
[49]   Steam oxidation behaviour of Ni-based single crystalline superalloy for the advanced gas turbine [J].
Fujikawa, H. ;
Murakumo, T. ;
Newcomb, S. B. ;
Harada, H. .
DIFFUSION AND THERMODYNAMICS OF MATERIALS, 2007, 263 :111-+
[50]   Short-Term Oxidation in HT-SEM of the Pt-Containing TROPEA Single Crystal Ni-Based Superalloy from 680 to 1000 °C [J].
Mathieu, S. ;
Podor, R. ;
Emo, M. ;
Hunault, L. ;
Vilasi, M. ;
Cormier, J. ;
Pedraza, F. .
HIGH TEMPERATURE CORROSION OF MATERIALS, 2024, 101 (05) :1211-1223