Surface Chemistry, Reactivity, and Pore Structure of Porous Silicon Oxidized by Various Methods

被引:75
作者
Riikonen, Joakim [1 ]
Salomaki, Mikko [3 ]
van Wonderen, Jessica [5 ]
Kemell, Marianna [6 ]
Xu, Wujun [1 ]
Korhonen, Ossi [2 ]
Ritala, Mikko [6 ]
MacMillan, Fraser [5 ]
Salonen, Jarno [4 ]
Lehto, Vesa-Pekka [1 ]
机构
[1] Univ Eastern Finland, Dept Appl Phys, FI-70211 Kuopio, Finland
[2] Univ Eastern Finland, Sch Pharm, FI-70211 Kuopio, Finland
[3] Univ Turku, Dept Chem, FI-20014 Turku, Finland
[4] Univ Turku, Dept Phys & Astron, FI-20014 Turku, Finland
[5] Univ E Anglia, Sch Chem, Henry Welcome Unit Biol EPR, Norwich NR4 7TJ, Norfolk, England
[6] Univ Helsinki, Lab Inorgan Chem, FI-00014 Helsinki, Finland
基金
芬兰科学院;
关键词
MESOPOROUS SILICON; THERMAL-OXIDATION; PHOTOLUMINESCENCE; HYDROGEN; LAYERS; SI; MICROSTRUCTURE; MODEL; STATE; WATER;
D O I
10.1021/la301642w
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Oxidation is the most commonly used method of passivating porous silicon (PSi) surfaces against unwanted reactions with guest molecules and temporal changes during storage or use. In the present study, several oxidation methods were compared in order to find optimal methods able to generate inert surfaces free of reactive hydrides but would cause minimal changes in the pore structure of PSi. The studied methods included thermal oxidations, liquid-phase oxidations, annealings, and their combinations. The surface-oxidized samples were studied by Fourier transform infrared spectroscopy, isothermal titration microcalorimetry, nitrogen sorption, ellipsometry, X-ray diffraction, electron paramagnetic resonance spectroscopy, and scanning electron microscopy imaging. Treatment at high temperature was found to have two advantages. First, it enables the generation of surfaces free of hydrides, which is not possible at low temperatures in a liquid or a gas phase. Second, it allows the silicon framework to partially accommodate a volume expansion because of oxidation, whereas at low temperature the volume expansion significantly consumes the free pore volume. The most promising methods were further optimized to minimize the negative effects on the pore structure. Simple thermal oxidation at 700 degrees C was found to be an effective oxidation method although it causes a large decrease in the pore volume. A novel combination of thermal oxidation, annealing, and liquid-phase oxidation was also effective and caused a smaller decrease in the pore volume with no significant change in the pore diameter but was more complicated to perform. Both methods produced surfaces that were not found to react with a model drug cinnarizine in isothermal titration microcalorimetry experiments. The study enables a reasonable choice of oxidation method for PSi applications.
引用
收藏
页码:10573 / 10583
页数:11
相关论文
共 44 条
[1]   CHARACTERIZATION OF POROUS SILICON LAYERS BY GRAZING-INCIDENCE X-RAY-FLUORESCENCE AND DIFFRACTION [J].
BENSAID, A ;
PATRAT, G ;
BRUNEL, M ;
DEBERGEVIN, F ;
HERINO, R .
SOLID STATE COMMUNICATIONS, 1991, 79 (11) :923-928
[2]   X-ray diffuse scattering of p-type porous silicon [J].
Buttard, D ;
Bellet, D ;
Dolino, G ;
Baumbach, T .
JOURNAL OF APPLIED PHYSICS, 2002, 91 (05) :2742-2752
[3]   ELECTRON-PARAMAGNETIC-RESONANCE STUDY OF THE MICROSCOPIC STRUCTURE OF THE SI(001)-SIO2 INTERFACE [J].
CANTIN, JL ;
SCHOISSWOHL, M ;
VONBARDELEBEN, HJ ;
ZOUBIR, NH ;
VERGNAT, M .
PHYSICAL REVIEW B, 1995, 52 (16) :11599-11602
[4]   Silicon surfaces as electron acceptors: Dative bonding of amines with Si(001) and Si(111) surfaces [J].
Cao, XP ;
Hamers, RJ .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2001, 123 (44) :10988-10996
[5]  
Chin V, 2001, ADV MATER, V13, P1877, DOI 10.1002/1521-4095(200112)13:24<1877::AID-ADMA1877>3.0.CO
[6]  
2-4
[7]   A detailed model of local structure and silanol hydrogen banding of silica gel surfaces [J].
Chuang, IS ;
Maciel, GE .
JOURNAL OF PHYSICAL CHEMISTRY B, 1997, 101 (16) :3052-3064
[8]  
Debarge L., 1998, Materials Science in Semiconductor Processing, V1, P281, DOI 10.1016/S1369-8001(98)00039-0
[9]  
Desai K. R., 2008, SURFACE CHEM, P28
[10]   Investigation of different oxidation processes for porous silicon studied by spectroscopic ellipsometry [J].
Frotscher, U ;
Rossow, U ;
Ebert, M ;
Pietryga, C ;
Richter, W ;
Berger, MG ;
ArensFischer, R ;
Munder, H .
THIN SOLID FILMS, 1996, 276 (1-2) :36-39