Shear bond strength between Ni-Cr alloy bonded to a ceramic substrate

被引:2
|
作者
do Nascimento, Cassio [1 ]
Miani, Paola Kirsten [1 ]
Bezzon, Osvaldo Luiz [1 ]
Goncalves, Mariane [1 ]
de Albuquerque Junior, Rubens Ferreira [1 ]
机构
[1] Univ Sao Paulo, Fac Odontol Ribeirao Preto, Dept Dent Mat & Prosthodont, BR-14040904 Ribeirao Preto, SP, Brazil
关键词
shear bond strength; Ni-Cr alloy; ceramic; thermocycling; RESIN; METAL; CASTABILITY; DURABILITY; RESISTANCE; SYSTEMS; POSTS;
D O I
10.1111/j.1741-2358.2011.00585.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Shear bond strength between Ni-Cr alloy bonded to a ceramic substrate Introduction: The aim of this study was to evaluate the shear bond strength between a Ni-Cr alloy and a ceramic system submitted or not to thermocycling. Materials and methods: Forty-eight cylinder blocks of Ni-Cr with 3.0 mm diameter by 4.0 mm hight and 48 disc-shaped specimens (7.0 mm in diameter by 2.0 mm thick) composed of ceramic were prepared. The Ni-Cr cylinder blocks were randomised in two groups of 24 specimens each. One group was submitted to air-particle abrasion (sandblasting) with 50 mu m Al2O3 (0.4-0.7 MPa) during 20 s, and the other group was submitted to mechanical retentions with carbide burrs. Each group was subdivided into other two groups (n = 12), submitted or not to thermocycling (500 cycles, 5-55 degrees C). The cylinder blocks were bonded to the disc-shaped ceramic specimens under 10 N of load. The shear bond strengths (MPa) were measured using a universal testing machine at a cross head speed of 0.5 mm/min and 200 kgf of load. The data were submitted to statistical analysis (ANOVA and Tukey's test). Results: The air-particle abrasion group exhibited significantly higher shear bond strength when compared to drilled group (p < 0.05). Conclusions: Thermocycling decreased significantly the bond strengths for all groups tested.
引用
收藏
页码:E909 / E913
页数:5
相关论文
共 50 条
  • [31] NI ATOM STATE IN NI-CR ALLOY
    KALINOVICH, DF
    KOVENSKI.II
    SMOLIN, MD
    FIZIKA TVERDOGO TELA, 1972, 14 (12): : 3699 - 3700
  • [32] Retention between Ni-Cr alloy and adhesive cements.
    Franca, RDO
    Muench, A
    Cardoso, PEC
    JOURNAL OF DENTAL RESEARCH, 1997, 76 (05) : 985 - 985
  • [33] Fracture toughness of the interface between Ni-Cr/ceramic, alumina/ceramic and zirconia/ceramic systems
    Porto, C. P. S.
    Parente, M. P. L.
    Jorge, R. M. N.
    Pereira, L. C.
    Griza, S.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2016, 39 (07) : 817 - 829
  • [34] Microanalysis of interface between Ni-Cr alloy and diamond (or steel)
    Wu, ZB
    Xu, HJ
    Xiao, B
    ADVANCES IN ABRASIVE PROCESSES, 2001, 202-2 : 143 - 146
  • [35] Microanalysis of interface between Ni-Cr alloy and diamond (or steel)
    Wu, Z.B.
    Xu, H.J.
    Xiao, B.
    Key Engineering Materials, 2001, 202-203 : 143 - 146
  • [36] Density of Liquid Ni-Cr Alloy
    F.XiaoJoining and Welding Research Institute
    JournalofMaterialsScience&Technology, 2003, (01) : 16 - 18
  • [37] Density of liquid Ni-Cr alloy
    Xiao, F.
    2003, Chinese Society of Metals (19):
  • [38] Density of liquid Ni-Cr alloy
    Xiao, F
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2003, 19 (01) : 16 - 18
  • [39] Study on Ni-Cr alloy electrodepositing technology on Fe substrate and coating performance
    Xu, Lijian
    Du, JIngjing
    He, Quanguo
    Tang, Jianxin
    He, Nongyue
    Li, Song
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2007, 233 : 29 - 29
  • [40] Ni-Sn intermetalics on the interface between porcelain and Ni-Cr alloy
    Ishibashi, K
    Nezu, T
    Ishibashi, H
    Terada, Y
    JOURNAL OF DENTAL RESEARCH, 2000, 79 : 272 - 272