Shear bond strength between Ni-Cr alloy bonded to a ceramic substrate

被引:2
|
作者
do Nascimento, Cassio [1 ]
Miani, Paola Kirsten [1 ]
Bezzon, Osvaldo Luiz [1 ]
Goncalves, Mariane [1 ]
de Albuquerque Junior, Rubens Ferreira [1 ]
机构
[1] Univ Sao Paulo, Fac Odontol Ribeirao Preto, Dept Dent Mat & Prosthodont, BR-14040904 Ribeirao Preto, SP, Brazil
关键词
shear bond strength; Ni-Cr alloy; ceramic; thermocycling; RESIN; METAL; CASTABILITY; DURABILITY; RESISTANCE; SYSTEMS; POSTS;
D O I
10.1111/j.1741-2358.2011.00585.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Shear bond strength between Ni-Cr alloy bonded to a ceramic substrate Introduction: The aim of this study was to evaluate the shear bond strength between a Ni-Cr alloy and a ceramic system submitted or not to thermocycling. Materials and methods: Forty-eight cylinder blocks of Ni-Cr with 3.0 mm diameter by 4.0 mm hight and 48 disc-shaped specimens (7.0 mm in diameter by 2.0 mm thick) composed of ceramic were prepared. The Ni-Cr cylinder blocks were randomised in two groups of 24 specimens each. One group was submitted to air-particle abrasion (sandblasting) with 50 mu m Al2O3 (0.4-0.7 MPa) during 20 s, and the other group was submitted to mechanical retentions with carbide burrs. Each group was subdivided into other two groups (n = 12), submitted or not to thermocycling (500 cycles, 5-55 degrees C). The cylinder blocks were bonded to the disc-shaped ceramic specimens under 10 N of load. The shear bond strengths (MPa) were measured using a universal testing machine at a cross head speed of 0.5 mm/min and 200 kgf of load. The data were submitted to statistical analysis (ANOVA and Tukey's test). Results: The air-particle abrasion group exhibited significantly higher shear bond strength when compared to drilled group (p < 0.05). Conclusions: Thermocycling decreased significantly the bond strengths for all groups tested.
引用
收藏
页码:E909 / E913
页数:5
相关论文
共 50 条
  • [1] Shear bond strength of aesthetic materials bonded to Ni-Cr alloy
    Almilhatti, HJ
    Giampaolo, ET
    Vergani, CE
    Machado, AL
    Pavarina, AC
    JOURNAL OF DENTISTRY, 2003, 31 (03) : 205 - 211
  • [2] Shear bond strength between esthetic materials and Ni-Cr alloy.
    Almilhatti, HJ
    Giampaolo, ET
    Machado, AL
    Pavarina, AC
    Vergani, CE
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : B200 - B200
  • [3] Shear bond strength of a composite resin bonded to a porcelain and a Ni-Cr alloy surface.
    Bernardi, SE
    Silva, MAMR
    JOURNAL OF DENTAL RESEARCH, 2000, 79 (05) : 1149 - 1149
  • [4] ALLOY PRETREATMENT AND SHEAR-STRENGTH OF PORCELAIN BONDED TO NI-CR
    FERNANDEZ, A
    MORENO, M
    BARGHI, N
    REY, R
    JOURNAL OF DENTAL RESEARCH, 1987, 66 : 288 - 288
  • [5] Effect of soldering on the metal-ceramic bond strength of an Ni-Cr base alloy
    Nikellis, L
    Levi, A
    Zinellis, S
    JOURNAL OF PROSTHETIC DENTISTRY, 2005, 94 (05): : 435 - 439
  • [6] Shear bond strength of optibond and scotchbond MP to dentin, Ni-Cr alloy and porcelain
    Mendes, RF
    Bastos, MTAA
    Souza, MHS
    Ishiquiriama, A
    JOURNAL OF DENTAL RESEARCH, 1997, 76 : 2386 - 2386
  • [7] Opacification systems: bond strength with Ni-Cr alloy.
    Dekon, S
    Goiato, M
    JOURNAL OF DENTAL RESEARCH, 2000, 79 (05) : 1153 - 1153
  • [8] Shear bond strength of three veneering resins to a Ni-Cr alloy using two bonding procedures
    Seimenis, I.
    Sarafianou, A.
    Papadopoulou, H.
    Papadopoulos, Tr.
    JOURNAL OF ORAL REHABILITATION, 2006, 33 (08) : 600 - 608
  • [9] Electrodeposition of Ni-Cr alloy on aluminum substrate
    杨余芳
    龚竹青
    邓丽元
    罗北平
    马玉天
    阳征会
    Journal of Central South University of Technology(English Edition), 2006, (03) : 219 - 224
  • [10] Electrodeposition of Ni-Cr alloy on aluminum substrate
    Yang, Yu-fang
    Gong, Zhu-qing
    Deng, Li-yuan
    Luo, Bei-ping
    Ma, Yu-tian
    Yang, Zhen-hui
    JOURNAL OF CENTRAL SOUTH UNIVERSITY OF TECHNOLOGY, 2006, 13 (03): : 219 - 224