Quasi-static and dynamic fracture behavior of particulate polymer composites: A study of nano- vs. micro-size filler and loading-rate effects

被引:72
作者
Jajam, Kailash C. [1 ]
Tippur, Hareesh V. [1 ]
机构
[1] Auburn Univ, Dept Mech Engn, Auburn, AL 36849 USA
基金
美国国家科学基金会;
关键词
Polymer-matrix composites (PMCs); Particle-reinforcement; Fracture; Impact behaviour; Micro-; vs; nano-composites; CRACK VELOCITY RELATIONSHIP; IMAGE CORRELATION METHOD; STRESS INTENSITY FACTOR; HIGH-SPEED PHOTOGRAPHY; PARTICLE-SIZE; EPOXY-RESIN; MATRIX ADHESION; POLYESTER/TIO2; NANOCOMPOSITES; TOUGHENING MECHANISMS; VOLUME FRACTION;
D O I
10.1016/j.compositesb.2012.01.042
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The role of nano- vs. micro-filler particle size-scale on static and dynamic fracture behaviors of silicafilled epoxy is examined. Particulate composites of epoxy matrix are studied under quasi-static and stress-wave loading conditions. Mode-I crack initiation and crack growth behaviors are examined using 2D digital image correlation method and high-speed photography in symmetrically impacted specimens. The measured displacement fields are analyzed using 20 crack-tip fields for dynamically propagating cracks in brittle solids to extract stress intensity factor (K-1(d)) histories, and crack velocity histories (V). K-1(d)-V plots for each type of composite are also presented. The quasi-static fracture tests show fracture toughness enhancement in case of nanocomposites relative to micro-particle filled ones. On the other hand, the dynamic crack-initiation toughness is consistently higher for micro-particle filled composites relative to the nano-filler counterparts. These counterintuitive results are supported by crack velocity histories in nanocomposites being significantly higher than that observed in micro-filler cases. The characteristic K-1(d)-V profiles suggest higher terminal velocities and lower dynamic fracture toughness for nanocomposites. Also, the post-mortem analyses of fracture surfaces reveal greater surface ruggedness for nanocomposites under quasi-static conditions. However, the opposite is evident under dynamic loading conditions. The qualitative and quantitative fractographic measurements correlate well with the measured fracture parameters for both quasi-static and dynamic fracture tests. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3467 / 3481
页数:15
相关论文
共 52 条
[1]   Fracture toughness of nano- and micro-spherical silica-particle-filled epoxy composites [J].
Adachi, Tadaharu ;
Osaki, Mayuka ;
Araki, Wakako ;
Kwon, Soon-Chul .
ACTA MATERIALIA, 2008, 56 (09) :2101-2109
[2]  
[Anonymous], 1996, ANN BOOK ASTM STAND, P325
[3]   RELATIONSHIPS BETWEEN FRACTURE PARAMETERS AND FRACTURE SURFACE-ROUGHNESS OF BRITTLE POLYMERS [J].
ARAKAWA, K ;
TAKAHASHI, K .
INTERNATIONAL JOURNAL OF FRACTURE, 1991, 48 (02) :103-114
[4]   Insitu multiscale analysis of fracture mechanisms in nanocomposites [J].
Boesl, Benjamin P. ;
Bourne, Gerald R. ;
Sankar, Bhavani V. .
COMPOSITES PART B-ENGINEERING, 2011, 42 (05) :1157-1163
[5]  
Broberg KB, 1999, CRACK FRACTURE
[6]  
Dally JW, 1985, INT J FRACTURE, V27, P159
[7]   Stress intensity factor and crack velocity relationship for polyester/TiO2 nanocomposites [J].
Évora, VMF ;
Jain, N ;
Shukla, A .
EXPERIMENTAL MECHANICS, 2005, 45 (02) :153-159
[8]   Fabrication, characterization, and dynamic behavior of polyester/TiO2 nanocomposites [J].
Evora, VMF ;
Shukla, A .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 361 (1-2) :358-366
[9]   Effects of particle size, particle/matrix interface adhesion and particle loading on mechanical properties of particulate-polymer composites [J].
Fu, Shao-Yun ;
Feng, Xi-Qiao ;
Lauke, Bernd ;
Mai, Yiu-Wing .
COMPOSITES PART B-ENGINEERING, 2008, 39 (06) :933-961
[10]  
FULLMAN RL, 1953, T AM I MIN MET ENG, V197, P447