Plane stress fracture toughness of cryorolled 6082 Al alloy

被引:17
作者
Kumar, N. [1 ]
Owolabi, G. M. [1 ]
Jayaganthan, R. [2 ]
Ajide, O. O. [1 ,3 ]
机构
[1] Howard Univ, Dept Mech Engn, Washington, WA 20059 USA
[2] Indian Instttuie Technol Madra, Dept Engn Design, Chennai 600036, Tamil Nadu, India
[3] Univ Ibadan, Dept Mech Engn, Ibadan, Nigeria
关键词
Cryorolling; Room temperature rolling; Ultrafine grains; Critical plane stress fracture toughness; SEVERE PLASTIC-DEFORMATION; MECHANICAL-PROPERTIES; MICROSTRUCTURAL EVOLUTION; CORROSION BEHAVIOR; GRAIN-BOUNDARIES; AGING TREATMENT; ALUMINUM-ALLOY; FATIGUE; TEMPERATURE; ANISOTROPY;
D O I
10.1016/j.tafmec.2018.02.011
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this paper, the plane stress fracture toughness of 6082 Al alloy produced by cryorolling is reported for the first time. The rolling was performed to achieve a 75% reduction in the sample thickness at two different temperatures, namely, liquid nitrogen temperature (-196 degrees C), and room temperature (25 degrees C). The plane stress fracture toughness was evaluated for cryorolled (CR), room temperature rolled (RTR), cryorolled and annealed (CR + AN), and room temperature and annealed (RTR + AN) samples using ASTM E1820.13 standard and compact tension specimens. Two methods, i.e., the Load point displacement (LPD)-load and the J-Integral resistance (J-R) curves, were used to calculate the plane stress fracture toughness. The results showed that the fracture toughness calculated using the J-R curve is more accurate since it accounts for all the constraints for evaluating the critical plane stress fracture toughness of the alloy for all the processing routes. The values of the critical plane stress fracture toughness (J(IC)) obtained via the J-R curve were 49 kJ/m(2) for CR, 31 kJ/m(2) for RTR, 69 kJ/m(2) for CR + AN and 39 kJ/m(2) for RTR + AN samples. Microstructural features obtained through scanning electron microscopy (SEM) and electron backscattered diffraction (EBSD) were also correlated with the fracture toughness. It is found from the SEM results that Mg-Si phases evolved at the crack tip/path during crack propagation in all the investigated samples. The EBSD results showed that CR + AN sample exhibits high kernel average missorentation and crack branches due to the evolution of small sized Mg-Si (Si-rich) precipitates during the fatigue testing. The presence of mixed grains (coarse and fine), fractographic features such as shallow ridges, transgranular facets, fiat circular and elongated dimples, small sized Si-rich precipitates and high kernel average missorentation support the high plane stress fracture toughness observed for the CR + AN sample.
引用
收藏
页码:28 / 41
页数:14
相关论文
共 57 条
[1]  
Annual Book of ASTM Standards, 1986, ANN BOOK ASTM STAND, V03, P772
[2]   Fractographical analysis of fatigue failed Cu-2.55Ni-0.55Si alloy [J].
Atapek, S. H. ;
Pantelakis, S. G. ;
Polat, S. ;
Chamos, A. N. ;
Aktas, G. .
THEORETICAL AND APPLIED FRACTURE MECHANICS, 2016, 83 :60-66
[3]  
Babu KK, 2017, MATER TODAY-PROC, V4, P285, DOI 10.1016/j.matpr.2017.01.023
[4]  
Begley J, 1972, J INTEGRAL FRACTURE, P1, DOI [10.1520/STP38816S, DOI 10.1520/STP38816S]
[5]   PREDICTING SLIP BEHAVIOR IN ALLOYS CONTAINING SHEARABLE AND STRONG PARTICLES [J].
BLANKENSHIP, CP ;
HORNBOGEN, E ;
STARKE, EA .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1993, 169 (1-2) :33-41
[6]  
Carvalho A. L. M., 2016, P INT C MULT ENG COM, VII
[7]   The effect of initial aging treatment on the microstructure and mechanical properties of cryorolled 6016 Al alloy [J].
Chen, X. P. ;
Mei, L. ;
Chen, D. ;
Bao, Z. L. ;
Liu, Q. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 667 :311-316
[8]   Effect of equal channel angular pressing on fracture toughness of Al-7075 [J].
Darban, Hossein ;
Mohammadi, Bijan ;
Djavanroodi, Faramarz .
ENGINEERING FAILURE ANALYSIS, 2016, 65 :1-10
[9]   Improvement of mechanical properties and fracture toughness of low SFE Cu-Al alloy through microstructural modification by multiaxial cryoforging [J].
Dasharath, S. M. ;
Mula, Suhrit .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 690 :393-404
[10]   Microstructural evolution and mechanical properties of low SFE Cu-Al alloys processed by cryorolling followed by short-annealing [J].
Dasharath, S. M. ;
Mula, Suhrit .
MATERIALS & DESIGN, 2016, 99 :552-564