Effect of a novel charring-foaming agent on flame retardancy and thermal degradation of intumescent flame retardant polypropylene

被引:302
|
作者
Li, B [1 ]
Xu, MJ [1 ]
机构
[1] NE Forestry Univ, Coll Sci, Dept Chem, Harbin 150040, Peoples R China
关键词
triazine polymer; flame retardancy; thermal degradation; polypropylene; intumescent flame retardant;
D O I
10.1016/j.polymdegradstab.2005.07.020
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A new triazine polymer was synthesized by using cyanuric chloride, ethanolamine and ethylenediamine as raw materials. It is used both as a charring agent and as a foaming agent in intumescent flame retardants, designated as charring-foaming agent (CFA). Effect of CFA on flame retardancy, thermal degradation and mechanical properties of intumescent flame retardant polypropylene (PP) system (IFR-PP system) has been investigated. The results demonstrated that the intumescent flame retardant (IFR) consisting of CFA, APP and Zeolite 4A is very effective ill flame retardancy of PP. It was found that when the weight ratio of CFA to APP is 1:2, that is, the components of the IFR are 64 wt% APP, 32 wt% CFA and 4 wt% Zeolite 4A, the IFR presents the most effective flame retardancy in PP systems. LOI value of IFR-PP reaches 37.0, when the IFR loading is 25 wt% in PP. It was also found that when the IFR loading is only 18 wt% in PP, the flame retardancy of IFR-PP can still pass V-0 rating, and its LOI value reaches 30.2. TGA data obtained in pure nitrogen demonstrated that CFA has a good ability of char formation itself, and CFA shows a high initial temperature of the thermal degradation. The char residue of CFA can reach 35.7 wt% at 700 degrees C. APP could effectively promote the char formation of the APP-CFA system. The char residue reaches 39.7 wt% at 700 degrees C, while it is 19.5% based on calculation. The IFR can change the thermal degradation behaviour of PP, enhance T-max of the decomposition peak of PP, and promote PP to form char, based upon the results of the calculation and the experiment. This is attributed to the fact that endothermic reactions took place in IFR charring process and the char layer formed by IFR prevented heat from transferring into inside of IFR-PP system. TGA results further explained the effective flame retardancy of the IFR containing CFA. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1380 / 1386
页数:7
相关论文
共 50 条
  • [1] Synthesis, thermal degradation, and flame retardancy of a novel charring agent aliphaticuaromatic polyamide for intumescent flame retardant polypropylene
    Yi, Jiangsong
    Liu, Yi
    Pan, Dongdong
    Cai, Xufu
    JOURNAL OF APPLIED POLYMER SCIENCE, 2013, 127 (02) : 1061 - 1068
  • [2] Flame retardancy and thermal degradation of intumescent flame retardant EVA composite with efficient charring agent
    Feng, Caimin
    Liang, Minyi
    Chen, Wenjing
    Huang, Jianguang
    Liu, Hongbo
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2015, 113 : 266 - 273
  • [3] Effect of Polyborosiloxane on the Flame Retardancy and Thermal Degradation of Intumescent Flame Retardant Polypropylene
    Lai, Xuejun
    Zeng, Xingrong
    Li, Hongqiang
    Zhang, Haili
    JOURNAL OF MACROMOLECULAR SCIENCE PART B-PHYSICS, 2014, 53 (04): : 721 - 734
  • [4] Synthesis and Application of Novel Triazine-Based Charring-Foaming Agents in Intumescent Flame Retardant Polypropylene
    Ligong Chen
    Yanyan Yuan
    Bowei Wang
    Na Liu
    Yuzhi Xing
    Yang Li
    Transactions of Tianjin University, 2017, 23 (03) : 221 - 229
  • [5] Synthesis and Application of Novel Triazine-Based Charring-Foaming Agents in Intumescent Flame Retardant Polypropylene
    Ligong Chen
    Yanyan Yuan
    Bowei Wang
    Na Liu
    Yuzhi Xing
    Yang Li
    Transactions of Tianjin University , 2017, (03) : 221 - 229
  • [6] Synthesis and Application of Novel Triazine-Based Charring-Foaming Agents in Intumescent Flame Retardant Polypropylene
    Chen L.
    Yuan Y.
    Wang B.
    Liu N.
    Xing Y.
    Li Y.
    Transactions of Tianjin University, 2017, 23 (3) : 221 - 229
  • [7] Flame retardancy and thermal degradation of intumescent flame retardant polypropylene material
    Chen, Xilei
    Jiao, Chuanmei
    POLYMERS FOR ADVANCED TECHNOLOGIES, 2011, 22 (06) : 817 - 821
  • [8] Flame retardancy and thermal degradation of intumescent flame retardant polypropylene with MP/TPMP
    Xing, Weiyi
    Song, Lei
    Lu, Hongdian
    Hu, Yuan
    Zhou, Shun
    POLYMERS FOR ADVANCED TECHNOLOGIES, 2009, 20 (08) : 696 - 702
  • [9] Effect of a Novel Phosphorus-Containing Compound on the Flame Retardancy and Thermal Degradation of Intumescent Flame Retardant Polypropylene
    Zhang, Shengqiang
    Li, Bin
    Lin, Mo
    Li, Qifei
    Gao, Suliang
    Yi, Wei
    JOURNAL OF APPLIED POLYMER SCIENCE, 2011, 122 (05) : 3430 - 3439
  • [10] A novel intumescent flame retardant with nanocellulose as charring agent and its flame retardancy in polyurethane foam
    Luo, Fubin
    Wu, Kun
    Li, Dengfeng
    Zheng, Jian
    Guo, Huilong
    Zhao, Qiang
    Lu, Mangeng
    POLYMER COMPOSITES, 2017, 38 (12) : 2762 - 2770