Experimental and Numerical Study of the Influence of Prefabricated Crack Width on the Fracture Toughness of NSCB Specimens

被引:26
|
作者
Zhang, Sheng [1 ,3 ]
Wang, Longfei [1 ,2 ]
Gao, Mingzhong [3 ]
机构
[1] Henan Polytech Univ, Collaborat Innovat Ctr Coal Work Safety, Sch Energy Sci & Engn, Jiaozuo 454001, Henan, Peoples R China
[2] Chongqing Univ, Sch Civil Engn, Chongqing 400045, Peoples R China
[3] Shenzhen Univ, Coll Civil & Transportat Engn, Inst Deep Earth Sci & Green Energy, Guangdong Prov Key Lab Deep Earth Sci & Geotherma, Shenzhen 518060, Peoples R China
基金
中国国家自然科学基金;
关键词
Prefabricated crack width; Fracture toughness; Notched semi-circular bend; Crack initiation position; MODE-I FRACTURE; PHASE-FIELD MODELS; LIMESTONE ROCK; SIZE; CHEVRON; GEOMETRY; PRESSURE; STRAIGHT; INITIATION; BEHAVIOR;
D O I
10.1007/s00603-020-02211-2
中图分类号
P5 [地质学];
学科分类号
0709 ; 081803 ;
摘要
The accuracy measurement of rock fracture toughness is one of the basic tasks of rock fracture mechanics. In order to study the influence of the width of the prefabricated crack on the fracture toughness of rock, the failure process of notched semi-circular bend (NSCB) specimens with four sizes and five different width of the prefabricated crack was studied by experimental and numerical methods. The influence of the width of the prefabricated crack on the peak load, crack initiation position, dimensionless stress intensity factor and fracture toughness is analyzed and discussed. The results show that the peak load and fracture toughness of NSCB increase with the increase of the width of the prefabricated crack, and the smaller the specimen size is, the larger the increase is. When the width of the prefabricated crack is less than 1.3 mm, the crack initiates at the dichotomy of the prefabricated crack tip; when the width of the prefabricated crack is greater than or equal to 1.3 mm, the crack initiates near the corner of the prefabricated crack tip. If NSCB specimen is adopted to determine the fracture toughness of limestone, it is recommended that the width of prefabricated crack should be less than 1.3 mm. The conclusions provide a reference for the fabrication of NSCB specimens and the accurate measurement of limestone fracture toughness.
引用
收藏
页码:5133 / 5154
页数:22
相关论文
共 50 条
  • [21] An experimental and numerical study of fracture coalescence in pre-cracked specimens under uniaxial compression
    Lee, Heekwang
    Jeon, Seokwon
    INTERNATIONAL JOURNAL OF SOLIDS AND STRUCTURES, 2011, 48 (06) : 979 - 999
  • [22] An Experimental and Numerical Study on the Influence of Filling Materials on Double-Crack Propagation
    Zhuang, Xiaoying
    Zhou, Shuwei
    ROCK MECHANICS AND ROCK ENGINEERING, 2020, 53 (12) : 5571 - 5591
  • [23] Experimental study on the influence of prefabricated fissure size on the directional propagation law of rock type-I crack
    Chen, Le-xin
    Guo, Wei-yao
    Zhang, Dong-xiao
    Zhao, Tong-bin
    INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2022, 160
  • [24] Theoretical and numerical prediction of crack path in the material with anisotropic fracture toughness
    Gao, Yue
    Liu, Zhanli
    Zeng, Qinglei
    Wang, Tao
    Zhuang, Zhuo
    Hwang, Keh-Chih
    ENGINEERING FRACTURE MECHANICS, 2017, 180 : 330 - 347
  • [25] Experimental investigation of fracture toughness of nanoclay reinforced polymer concrete composite: Effect of specimen size and crack angle
    Ghasemi-Ghalebahman, A.
    Aghdam, A. Abdi
    Pirmohammad, S.
    Niaki, M. Hassani
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2022, 117
  • [26] Study of mode I crack dynamic propagation behaviour and rock dynamic fracture toughness by using SCT specimens
    Dong, Y. Q.
    Zhu, Z. M.
    Zhou, L.
    Ying, P.
    Wang, M.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2018, 41 (08) : 1810 - 1822
  • [27] An experimental and theoretical assessment of semi-circular bend specimens with chevron and straight-through notches for mode I fracture toughness testing of rocks
    Wei, Ming-Dong
    Dai, Feng
    Xu, Nu-Wen
    Zhao, Tao
    Liu, Yi
    INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES, 2017, 99 : 28 - 38
  • [28] Preferable initial crack length for fracture toughness evaluation using subsized bend specimens
    Schindler, HJ
    SMALL SPECIMEN TEST TECHNIQUES: FOURTH VOLUME, 2002, 1418 : 67 - 79
  • [29] EFFECTS OF CRACK FRONT CURVATURE ON J AND CTOD DETERMINATION IN FRACTURE TOUGHNESS SPECIMENS BY FEA
    Hutchison, Emily K.
    Pisarski, Henryk G.
    PROCEEDINGS OF THE ASME 32ND INTERNATIONAL CONFERENCE ON OCEAN, OFFSHORE AND ARCTIC ENGINEERING - 2013, VOL 3, 2013,
  • [30] Bone toughness and crack propagation: an experimental study
    Libonati, Flavia
    Vergani, Laura
    XVII INTERNATIONAL COLLOQUIUM ON MECHANICAL FATIGUE OF METALS (ICMFM17), 2014, 74 : 464 - 467