Mechanistic study on flame retardance of polycarbonate with a small amount of potassium perfluorobutane sulfonate by TGA-FTIR/XPS

被引:60
作者
Huang, XB
Ouyang, XY
Ning, FL
Wang, JQ
机构
[1] Beijing Inst Technol, Sch Mat Sci & Engn, Natl Lab Flame Retardant Mat, Beijing 100081, Peoples R China
[2] Guangzhou KINGFA Sci & Technol Co Ltd, Guangzhou 510520, Peoples R China
关键词
flame retardant polycarbonate; potassium perfluorobutane sulfonate; FTIR-TGA; XPS;
D O I
10.1016/j.polymdegradstab.2005.02.028
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The work focuses on a mechanistic study of the title system with the aid of both TGA-FTIR (in the gas phase) and XPS (in the condensed phase). It is concluded that: (1) although the change in yield of char for PC/PPFBS is insignificant with respect to PC itself it appears that the majority of the crucial FR activity is in the condensed phase as indicated by the XPS data; (2) TGA-FTIR experiments support the view that the degradation of polycarbonate proceeds by the cleavage of the C-alpha-O and the C-beta-H bonds, leading to the formation of dienes, diols and carbon dioxide; (3) the reverse reaction of the intermediates, like phenols, may Occur via the basic catalyst, possibly K-alkyl oxide, a weaker base is generated in the process; (4) voluminous evolution of CO, accelerated by PPFBS may give flame retardance by way of intumescent action and its dilution into the gas phase. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:606 / 613
页数:8
相关论文
共 22 条
[1]  
BRADY DG, 1977, J FIRE RETARD CHEM, V4, P150
[2]   Additional XPS studies on the degradation of poly(methyl methacrylate) and polystyrene nanocomposites [J].
Du, JX ;
Wang, JQ ;
Su, SP ;
Wilkie, CA .
POLYMER DEGRADATION AND STABILITY, 2004, 83 (01) :29-34
[3]   An XPS investigation of thermal degradation and charring on poly(vinyl chloride)-clay nanocomposites [J].
Du, JX ;
Wang, DY ;
Wilkie, CA ;
Wang, JQ .
POLYMER DEGRADATION AND STABILITY, 2003, 79 (02) :319-324
[4]   An XPS investigation of thermal degradation and charring on PMMA clay nanocomposites [J].
Du, JX ;
Zhu, J ;
Wilkie, CA ;
Wang, JQ .
POLYMER DEGRADATION AND STABILITY, 2002, 77 (03) :377-381
[5]  
FENIMORE CP, 1972, PUBLICATION NATL BUR, V357, P159
[6]  
FRECHET JMJ, 1997, J PHOTOPOLYM SCI TEC, V19, P31
[7]   An XPS study of the radiation-induced effect on the thermal degradation and charring of butadiene and its copolymers [J].
Hao, JW ;
Wu, SL ;
Wilkie, CA ;
Wang, JQ .
POLYMER DEGRADATION AND STABILITY, 1999, 66 (01) :81-86
[8]   An XPS investigation of thermal degradation and charring of cross-linked polyisoprene and polychloroprene [J].
Hao, JW ;
Wilkie, CA ;
Wang, JQ .
POLYMER DEGRADATION AND STABILITY, 2001, 71 (02) :305-315
[9]   The pyrolysis of esters [J].
Hurd, CD ;
Blunck, FH .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1938, 60 :2419-2425
[10]  
QIAN Z, 1987, HDB PROPERTY APPL PL, P255