Suppressing type IV failure via modification of heat affected zone microstructures using high boron content in 9Cr heat resistant steel welded joints

被引:63
作者
Kondo, M
Tabuchi, M
Tsukamoto, S
Yin, F
Abe, F
机构
[1] Natl Inst Mat Sci, Tsukuba, Ibaraki 3050047, Japan
[2] Mitsubishi Heavy Ind Co Ltd, Nagasaki Res & Dev Ctr, Nagasaki 8510392, Japan
关键词
heat resistant steel; welded joint; boron; type IV failure; creep; heat affected zone;
D O I
10.1179/174329306X89260
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Creep rupture strength at 923 K and microstructural evolution of welded joints have been investigated for high boron-low nitrogen-9Cr heat resistant steels developed at the National Institute for Materials Science ( Japan). Welded joints were prepared from plates containing 47 180 ppm boron using gas tungsten arc welding and Inconel type filler metal, and showed superior creep properties to those of welded joints of conventional high chromium steels such as P92 and P122. No type IV failure was observed in the boron steel welded joints. A large grained microstructure was observed in the heat affected zone heated to Ac-3 (Ac-3 HAZ) during welding, whereas the grains are refined at the same location in conventional steel welded joints. The simulated Ac-3 HAZ structures of the boron steels have a creep life almost equal to that of the base metal. Large grained HAZ microstructures and stabilisation of M23C6 precipitates are probable reasons for suppression of type IV failure and improved creep resistance of the boron steel welded joints.
引用
收藏
页码:216 / 223
页数:8
相关论文
共 17 条
[1]  
ABE F, 2002, P C MAT ADV POW ENG, V3, P1397
[2]  
Babu SS, 1998, WELD J, V77, p249S
[3]  
BAKKER WT, 2001, ADV MAT TECHNOLOGY F, P1
[4]  
Horiuchi T., 2002, ISIJ Int, V42, P67, DOI [10.2355/isijinternational.42.Suppl_S67, DOI 10.2355/ISIJINTERNATIONAL.42.SUPPL_S67]
[5]   AUSTENITE MEMORY EFFECT IN 1CR-1MO-0.75V(TI,B) STEEL [J].
KIMMINS, ST ;
GOOCH, DJ .
METAL SCIENCE, 1983, 17 (11) :519-532
[6]   Analysis of factors affecting type IV cracking in welded joints of high chromium ferritic heat resistant steels [J].
Li, D ;
Shinozaki, K ;
Kuroki, H ;
Harada, H ;
Ohishi, K .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2003, 8 (04) :296-302
[7]  
MAKI M, 1979, TETSU TO HAGANE, V65, P1598
[8]   History of power plants and progress in heat resistant steels [J].
Masuyama, F .
ISIJ INTERNATIONAL, 2001, 41 (06) :612-625
[9]  
Matsui M., 2003, Journal of the Society of Materials Science, Japan, V52, P119, DOI 10.2472/jsms.52.119
[10]   Degradation of creep strength in welded joint of 9%Cr steel [J].
Matsui, M ;
Tabuchi, M ;
Watanabe, T ;
Kubo, K ;
Kinugawa, J ;
Abe, F .
ISIJ INTERNATIONAL, 2001, 41 :S126-S130