Microstructure, texture and mechanical properties of Mg-3.0Zn-0.2Ca alloys fabricated by extrusion at various temperatures

被引:129
作者
Li, Cheng-jie [1 ]
Sun, Hong-fei [1 ]
Li, Xue-wen [2 ]
Zhang, Jun-ling [1 ]
Fang, Wen-bin [1 ,2 ]
Tan, Ze-yi [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Harbin Univ Sci & Technol, Sch Mat Sci & Engn, Harbin 150080, Peoples R China
关键词
Magnesium alloy; Extrusion; Tensile properties; Strengthening mechanisms; Ductility; ZN-CA ALLOYS; MAGNESIUM ALLOYS; DEFORMATION MECHANISMS; POWDER-METALLURGY; HIGH-STRENGTH; ZK60; ALLOYS; MG; BEHAVIOR; PRECIPITATION; ANISOTROPY;
D O I
10.1016/j.jallcom.2015.08.215
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The Mg-3.0Zn-0.2Ca (wt.%) alloy has been extruded at temperature range of 25-300 degrees C and the resulting microstructure, texture and mechanical properties are systematically investigated. The results show that the grain size monotonically increases with the increasing of the extrusion temperature and the texture intensity increases firstly and decreases subsequently. In addition, a large number of nano-scale precipitates are formed in alloys extruded above 250 degrees C. The weakest basal texture developed in the cold extrusion alloy is related to the deformation twinning, while, the combining effects of activation of multiple deformation mechanisms and dynamic precipitates contribute to developing the weaker basal texture in alloys extruded above 250 degrees C. A sharp basal texture enhances the yield strength of alloy extruded at 150 degrees C greatly at the cost of work hardening rate. The highest elongation is achieved in the alloy extruded at 300 degrees C. The enhanced formability is considered to be associated with the dependence of the weaker basal texture and dynamic precipitates on the strain hardening behavior. Among the multiple strengthening mechanisms, the fine grain strengthening and the solid solution strengthening play a dominant role in the increment of strength for the as-extruded alloys. (C) 2015 Elsevier B.V. All rights reserved.
引用
收藏
页码:122 / 131
页数:10
相关论文
共 36 条
[1]   SOLID SOLUTION STRENGTHENING OF MAGNESIUM SINGLE CRYSTALS .I. ALLOYING BEHAVIOUR IN BASAL SLIP [J].
AKHTAR, A ;
TEGHTSOONIAN, E .
ACTA METALLURGICA, 1969, 17 (11) :1339-+
[2]  
Ashby M.F., 1982, DEFORMATION MECH MAP
[3]   Application of rapid solidification powder metallurgy to the fabrication of high-strength, high-ductility Mg-Al-Zn-Ca-La alloy through hot extrusion [J].
Ayman, Elsayed ;
Junko, Umeda ;
Katsuyoshi, Kondoh .
ACTA MATERIALIA, 2011, 59 (01) :273-282
[4]   Micro-macro modelling of the effects of the grain size distribution on the plastic flow stress of heterogeneous materials [J].
Berbenni, S. ;
Favier, V. ;
Berveiller, M. .
COMPUTATIONAL MATERIALS SCIENCE, 2007, 39 (01) :96-105
[5]   Current wrought magnesium alloys: Strengths and weaknesses [J].
Bettles, CJ ;
Gibson, MA .
JOM, 2005, 57 (05) :46-49
[6]   Twinning behavior and deformation mechanisms of extruded AZ31 Mg alloy [J].
Chino, Yasumasa ;
Kimura, Katsuya ;
Mabuchi, Mamoru .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 486 (1-2) :481-488
[7]   Solid solution strengthening behaviors in binary Mg-Y single phase alloys [J].
Gao, L. ;
Chen, R. S. ;
Han, E. H. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 472 (1-2) :234-240
[8]   Precipitation-hardened Mg-Ca-Zn alloys with superior creep resistance [J].
Gao, X ;
Zhu, SM ;
Muddle, BC ;
Nie, JF .
SCRIPTA MATERIALIA, 2005, 53 (12) :1321-1326
[9]   Effect of extrusion temperature on superplasticity of PM-WE54 [J].
Garces, G. ;
Maeso, M. ;
Perez, P. ;
Adeva, P. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 462 (1-2) :127-131
[10]   MULTICOMPONENT INTRINSIC SOLID-SOLUTION SOFTENING AND HARDENING [J].
GYPEN, LA ;
DERUYTTERE, A .
JOURNAL OF THE LESS-COMMON METALS, 1977, 56 (01) :91-101