Morphology and phase composition of corrosion products formed at the zinc-iron interface of a galvanized steel

被引:39
作者
Carbucicchio, M. [2 ]
Ciprian, R. [2 ]
Ospitali, F. [3 ]
Palombarini, G. [1 ]
机构
[1] Univ Bologna, Dept Met Sci Electrochem & Chem Tech, Bologna, Italy
[2] Univ Parma, Dept Phys, I-43100 Parma, Italy
[3] Univ Bologna, Dept Phys & Inorgan Chem, Bologna, Italy
关键词
Galvanized steel; Hot water corrosion; Iron oxyhydroxides;
D O I
10.1016/j.corsci.2008.06.007
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion products formed on the inner wall of pipes made of galvanized low carbon steel, exposed for similar to 2 years to water flowing in a large household heating system, were analysed using X-ray diffraction, Mossbauer and Raman spectroscopic techniques, as well as metallographic techniques. Products grew in the form of large-sized tubercles that gradually developed causing base metal losses up to perforation of the steel pipe. Considerable differences in the phase composition were found between the products formed in contact with the steel and those constituting the outer part of tubercles. The former were mainly made of FeCO3 (siderite), with small amounts of Zn-5(CO3)(2)(OH)(6) (hy&Ozincite), ZnCO3 (smithsonite), (Fe,Zn)CO3 mixed carbonate and CaCO3 (calcite), the latter mainly by Fe(III) oxyhydroxide goethite. Both parts of the tubercles also contained small amounts of other ferric oxyhydroxides, gamma-FeOOH (lepidocrocite) and beta-FeOOH (akaganeite), and very small amounts of hematite. The procedures used proved effective for an adequate identification of both the iron-containing and iron-free compounds in the corrosion products as well as for suggesting a corrosion mechanism. (c) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2605 / 2613
页数:9
相关论文
共 36 条
[1]   Characterisation of Spanish coal by means of Mossbauer spectroscopy [J].
Ahmed, MA ;
Vandenberghe, RE ;
De Grave, E ;
Eissa, NA ;
Ibarra, JV .
FUEL, 1999, 78 (04) :453-457
[2]   Relationship between (00.2) and (20.1) texture components and corrosion resistance of hot-dip galvanized zinc coatings [J].
Asgari, H. ;
Toroghinejad, M. R. ;
Golozar, M. A. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 198 (1-3) :54-59
[3]   Transmission Mossbauer analysis of nanophased oxides formed on high strength steels [J].
Balasubramanian, R ;
Cook, DC ;
Townsend, H .
HYPERFINE INTERACTIONS, 2002, 141 (1-4) :369-379
[4]   New analysis of the Mossbauer spectra of akaganeite [J].
Barrero, C. A. ;
Garcia, K. E. ;
Morales, A. L. ;
Kodjikian, S. ;
Greneche, J. M. .
JOURNAL OF PHYSICS-CONDENSED MATTER, 2006, 18 (29) :6827-6840
[5]   Catalogue of 45 reference Raman spectra of minerals concerning research in art history or archaeology, especially on corroded metals and coloured glass [J].
Bouchard, M ;
Smith, DC .
SPECTROCHIMICA ACTA PART A-MOLECULAR AND BIOMOLECULAR SPECTROSCOPY, 2003, 59 (10) :2247-2266
[6]   Synthesis and characterization of nanophasic goethite [J].
Cabral-Prieto, A ;
Reyes-Felipe, AA ;
Siles-Dotor, MG .
NANOSTRUCTURED MATERIALS, 1998, 10 (02) :311-326
[7]  
CHERKEZOVAJELEV.Z, 2002, NANOSCI NANOTECH, P99
[8]   Raman identification of corrosion products on automotive galvanized steel sheets [J].
Colomban, Ph. ;
Cherifi, S. ;
Despert, G. .
JOURNAL OF RAMAN SPECTROSCOPY, 2008, 39 (07) :881-886
[9]   Spectroscopic identification of protective and non-protective corrosion coatings on steel structures in marine environments [J].
Cook, DC .
CORROSION SCIENCE, 2005, 47 (10) :2550-2570
[10]   Effects of sediment iron mineral composition on microbially mediated changes in divalent metal speciation: Importance of ferrihydrite [J].
Cooper, DC ;
Neal, AL ;
Kukkadapu, RK ;
Brewe, D ;
Coby, A ;
Picardal, FW .
GEOCHIMICA ET COSMOCHIMICA ACTA, 2005, 69 (07) :1739-1754