Friction and wear of binder-less niobium carbide

被引:36
作者
Woydt, Mathias [1 ]
Mohrbacher, Hardy [2 ]
机构
[1] BAM Fed Inst Mat Res & Testing, DE-12200 Berlin, Germany
[2] Niobelcon BVBA, BE-2970 Schilde, Belgium
关键词
Sliding friction; Sliding wear; Ceramic; Coating; NbC;
D O I
10.1016/j.wear.2013.07.013
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The tribological profile of alumina (99.7%) mated against binder-less niobium carbide (NbC) rotating disks were determined unidirectional sliding tests (0.1-7.5 m/s; 22 degrees C and 400 degrees C) as well as in oscillation tests (f=20 Hz, Delta x=0.2 mm, 2/50/98% rel. humidity, n=10(5)/10(6) cycles) under un-lubricated (dry) conditions. In addition, the microstructure and mechanical properties of NbC were determined as well. The reason for testing hot-pressed NbC was to avoid side effects generated by sintering additives and/or second phases. The tribological data obtained were benchmarked with different ceramics, cermets and thermally sprayed coatings. NbC exhibited low wear rates under dry sliding associated with high load carrying capacity. The tribological profile established revealed a strong position of NbC under tribological considerations and for closed tribo-systems against traditional references, such as WC, Cr3C2, (Ti,Mo) (C,N), etc. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:126 / 130
页数:5
相关论文
共 9 条
[1]   Dry sliding up to 7.5 m/s and 800 °C of thermally sprayed coatings of the TiO2-Cr2O3 system and (Ti,Mo)(C,N)-Ni(Co) [J].
Berger, L. -M. ;
Stahr, C. C. ;
Saaro, S. ;
Thiele, S. ;
Woydt, M. ;
Kelling, N. .
WEAR, 2009, 267 (5-8) :954-964
[2]  
Berger L.-M., 2008, THERMAL SPRAY B, P39
[3]   FRETTING WEAR OF CERAMICS [J].
KLAFFKE, D .
TRIBOLOGY INTERNATIONAL, 1989, 22 (02) :89-101
[5]  
Mohrbacher H., 2011, Materials Science Technology, P434
[6]  
Nylén T, 2001, NIOBIUM: SCIENCE & TECHNOLOGY, P1063
[7]   CERAMIC AND CERAMIC COMPOSITE-MATERIALS WITH IMPROVED FRICTION AND WEAR PROPERTIES [J].
SKOPP, A ;
WOYDT, M .
TRIBOLOGY TRANSACTIONS, 1995, 38 (02) :233-242
[8]   HIGH-TEMPERATURE TRIBOLOGY OF CERAMICS [J].
WOYDT, M ;
HABIG, KH .
TRIBOLOGY INTERNATIONAL, 1989, 22 (02) :75-88
[9]   Wear engineering oxides/anti-wear oxides [J].
Woydt, M ;
Skopp, A ;
Dorfel, I ;
Witke, K .
WEAR, 1998, 218 (01) :84-95