Indentation creep of lead-free Sn-9Zn and Sn-8Zn-3Bi solder alloys

被引:74
作者
Mahmudi, R. [1 ]
Geranmayeh, A. R. [2 ]
Khanbareh, H. [1 ]
Jahangiri, N. [1 ]
机构
[1] Univ Tehran, Sch Met & Mat Engn, Tehran, Iran
[2] Islamic Azad Univ, Dept Mech Engn, S Tehran Branch, Tehran, Iran
基金
美国国家科学基金会;
关键词
Creep; Mechanical; PB-FREE SOLDER; COOLING RATE; MECHANICAL-PROPERTIES; INTERFACIAL REACTIONS; IMPRESSION CREEP; SN-AG; BEHAVIOR; CU; DEFORMATION; TIN;
D O I
10.1016/j.matdes.2008.05.058
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Creep behavior of Sn-9%Zn and Sn-8%Zn-3%Bi solders together with Sn-37% Pb, as the material for comparison, was studied by indentation tests at room-temperature (T> 0.6T(m)) in order to evaluate the correspondence of the creep results obtained by different methods of analysis, and to evaluate the effect of Bi on the creep response of the eutectic Sn-9%Zn alloy. Stress exponent values determined through these methods were in good agreement. The better creep resistance of the ternary alloy is attributed to solid solutioning effect and precipitation of Bi in the Sn matrix. Both tin-based alloys showed creep resistances higher than that of the Sn-37% Pb alloy. (C) 2008 Elsevier Ltd. All rights reserved,
引用
收藏
页码:574 / 580
页数:7
相关论文
共 50 条
[21]   Effect of rare earth element additions on the impression creep of Sn-9Zn solder alloy [J].
Mahmudi, R. ;
Geranmayeh, A. R. ;
Zahiri, B. ;
Marvasti, M. H. .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2010, 21 (01) :58-64
[22]   Temperature and Flux Effect on Contact Angles and Intermetallic between Sn-8Zn-3Bi Lead-free Solder and Cu Substrate [J].
Mayappan, Ramani ;
Ahmad, Zainal Arifin .
SAINS MALAYSIANA, 2009, 38 (03) :395-400
[23]   Effects of small addition of Ag and/or Cu on the microstructure and properties of Sn-9Zn lead-free solders [J].
El-Daly, A. A. ;
Hammad, A. E. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (20) :5212-5219
[24]   Effect of silver and indium addition on mechanical properties and indentation creep behavior of rapidly solidified Bi-Sn based lead-free solder alloys [J].
Shalaby, Rizk Mostafa .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 560 :86-95
[25]   Creep-fatigue life of Sn-8Zn-3Bi solder under multiaxial loading [J].
Yamamoto, Takaei ;
Itoh, Takamoto ;
Sakane, Masao ;
Tsukada, Yutaka .
INTERNATIONAL JOURNAL OF FATIGUE, 2012, 43 :235-241
[26]   The effects of antimony additions on microstructures, thermal and mechanical properties of Sn-8Zn-3Bi alloys [J].
Ren, Guang ;
Collins, Maurice N. .
MATERIALS & DESIGN, 2017, 119 :133-140
[27]   Crystallographic, microstructure, electrical, and hardness characterization of advanced Sn-9Zn-0.5ZrO2 and Sn-9Zn-xNi lead-free solder alloys [J].
Mohamed, H. S. ;
Mostafa, M. M. ;
Mahmoud, N. M. .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2025, 36 (13)
[28]   Development of a lead-free solder: Sn-4.0Bi-3.7Ag-0.9Zn [J].
Wang, Xun ;
Liu, Yongchang ;
Yu, Liming ;
Dong, Zhizhong ;
Gao, Zhiming .
SOLDERING & SURFACE MOUNT TECHNOLOGY, 2011, 23 (01) :15-21
[29]   The effects of Cu and Al on dry sliding wear properties of eutectic Sn-9Zn lead-free solder alloy [J].
Ozyurek, D. ;
Yavuzer, B. ;
Tuncay, T. .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2016, 30 (15) :1662-1670
[30]   Microstructure and tensile properties of Sn-9Zn-xAg lead-free solder alloys [J].
Song, JM ;
Lan, GF ;
Lui, TS ;
Chen, LH .
SCRIPTA MATERIALIA, 2003, 48 (08) :1047-1051