Indentation creep of lead-free Sn-9Zn and Sn-8Zn-3Bi solder alloys

被引:74
作者
Mahmudi, R. [1 ]
Geranmayeh, A. R. [2 ]
Khanbareh, H. [1 ]
Jahangiri, N. [1 ]
机构
[1] Univ Tehran, Sch Met & Mat Engn, Tehran, Iran
[2] Islamic Azad Univ, Dept Mech Engn, S Tehran Branch, Tehran, Iran
基金
美国国家科学基金会;
关键词
Creep; Mechanical; PB-FREE SOLDER; COOLING RATE; MECHANICAL-PROPERTIES; INTERFACIAL REACTIONS; IMPRESSION CREEP; SN-AG; BEHAVIOR; CU; DEFORMATION; TIN;
D O I
10.1016/j.matdes.2008.05.058
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Creep behavior of Sn-9%Zn and Sn-8%Zn-3%Bi solders together with Sn-37% Pb, as the material for comparison, was studied by indentation tests at room-temperature (T> 0.6T(m)) in order to evaluate the correspondence of the creep results obtained by different methods of analysis, and to evaluate the effect of Bi on the creep response of the eutectic Sn-9%Zn alloy. Stress exponent values determined through these methods were in good agreement. The better creep resistance of the ternary alloy is attributed to solid solutioning effect and precipitation of Bi in the Sn matrix. Both tin-based alloys showed creep resistances higher than that of the Sn-37% Pb alloy. (C) 2008 Elsevier Ltd. All rights reserved,
引用
收藏
页码:574 / 580
页数:7
相关论文
共 50 条
[1]   Effect of isothermal aging on room temperature impression creep of lead free Sn-9Zn and Sn-8Zn-3Bi solders [J].
Mahmudi, R. ;
Geranmayeh, A. R. ;
Noori, H. ;
Khanbareh, H. ;
Jahangiri, N. .
MATERIALS SCIENCE AND TECHNOLOGY, 2010, 26 (08) :1001-1007
[2]   A comparison of impression, indentation and impression-relaxation creep of lead-free Sn-9Zn and Sn-8Zn-3Bi solders at room temperature [J].
Mahmudi, R. ;
Geranmayeh, A. R. ;
Noori, H. ;
Khanbareh, H. ;
Jahangiri, N. .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2009, 20 (04) :312-318
[3]   Effect of cooling rate on the room-temperature impression creep of lead-free Sn-9Zn and Sn-8Zn-3Bi solders [J].
Mahmudi, R. ;
Geranmayeh, A. R. ;
Noori, H. ;
Jahangiri, N. ;
Khanbareh, H. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 487 (1-2) :20-25
[4]   Effects of Ag on Properties of Sn-9Zn Lead-Free Solder [J].
Chen Wenxue ;
Xue Songbai ;
Wang Hui ;
Hu Yuhua .
RARE METAL MATERIALS AND ENGINEERING, 2010, 39 (10) :1702-1705
[5]   Effect of Sb additions on the creep behaviour of low temperature lead-free Sn-8Zn-3Bi solder alloy [J].
Ren, Guang ;
Collins, Maurice .
SOLDERING & SURFACE MOUNT TECHNOLOGY, 2021, 33 (03) :159-169
[6]   Silver effect on the intermetallic growth in the Sn-8Zn-3Bi lead-free solder [J].
Mayappan, Ramani ;
Jasli, Nor Aishah .
MATERIALS TODAY-PROCEEDINGS, 2018, 5 (09) :17553-17560
[7]   Microstructure Evolution and Shear Strength Study of Sn-9Zn and Sn-8Zn-3Bi on Cu Substrate [J].
Mayappan, Ramani ;
Ahmad, Zainal Arifin .
TRANSACTIONS ON ELECTRICAL AND ELECTRONIC MATERIALS, 2024, 25 (01) :48-58
[8]   Effects of current density on the formation and microstructure of Sn-9Zn, Sn-8Zn-3Bi and Sn-3Ag-0.5Cu solder joints [J].
Othman, R. ;
Binh, D. N. ;
Ismail, A. B. ;
Long, B. D. ;
Ariga, T. .
INTERMETALLICS, 2012, 22 :1-6
[9]   Effects of Sulfur on the Properties of Sn-9Zn as Lead-Free Solder [J].
Wei, Xiuqin ;
Li, Yinghui ;
Huang, Huizhen .
JOURNAL OF ELECTRONIC MATERIALS, 2017, 46 (02) :1067-1071
[10]   Corrosion Study of Sn-9Zn Lead-Free Solder in Alkaline Solution [J].
Nazeri, Muhammad Firdaus Mohd ;
Affendy, Muhammad Ghaddafy ;
Mohamad, Ahmad Azmin .
INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2012, 7 (05) :4182-4191