Metal Release and Speciation Changes during Wet Aging of Coal Fly Ashes

被引:41
作者
Catalano, Jeffrey G. [1 ]
Huhmann, Brittany L. [1 ]
Luo, Yun [1 ,2 ]
Mitnick, Elizabeth H. [1 ]
Slavney, Adam [1 ]
Giammar, Daniel E. [2 ]
机构
[1] Washington Univ, Dept Earth & Planetary Sci, St Louis, MO 63130 USA
[2] Washington Univ, Dept Energy Environm & Chem Engn, St Louis, MO 63130 USA
基金
加拿大自然科学与工程研究理事会;
关键词
FINE-STRUCTURE SPECTROSCOPY; FUEL COMBUSTION RESIDUES; OXIDE-WATER INTERFACE; BY-PRODUCTS; THERMODYNAMIC MODEL; CHROMATE REDUCTION; AQUEOUS-SOLUTIONS; FEED COALS; PHOTOCATALYTIC OXIDATION; COMPETITIVE ADSORPTION;
D O I
10.1021/es302807b
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Introduction of coal fly ash into aquatic systems poses a potential environmental hazard because of its heavy metal content. Here we investigate the relationship between solid phase transformations, fluid composition, and metal release and speciation during prolonged wet aging of a class C and class F coal fly ash. The class C ash causes rapid alkalinization of water that is neutralized over time by CO2 uptake from air and calcite precipitation. The resulting aqueous metal concentrations are below regulatory limits with the exception of Cr; solubility constraints suggest this is released as chromate. Limited As release is accompanied by no change in solid-phase speciation, but up to 35% of the Zn in the ash dissolves and reprecipitates in secondary phases. Similar processes inhibit Ba and Cu release. In contrast, the class F ash causes rapid acidification of water and initially releases substantial quantities of As, Se, Cr, Cu, Zn, and Ba. Arsenic concentrations decline during aging because of adsorption to the iron oxide-rich ash; this is aided by As(III) oxidation. Precipitation processes lower Ba and Cr concentrations during aging. Se, Cu, and Zn concentrations remain elevated during wet aging and solid-phase Zn speciation is not affected by ash-water reactions. Total metal contents were poor predictors of metal release, which is predominantly controlled by metal speciation and the effects of ash-water reactions on fluid pH. While contact with atmospheric gases has little effect on class F ash, carbonation of class C ash inhibits metal release and neutralizes the alkalinity produced by the ash.
引用
收藏
页码:11804 / 11812
页数:9
相关论文
共 81 条
[1]  
American Coal Ash Association, 2010, COAL COMB PROD CCP P
[2]  
[Anonymous], 2010, Fed Regist, V75, P35128
[3]  
[Anonymous], 2009, NAT ATM DEP PROGR NR
[4]  
ASTM International, 2012, J ASTM INT
[5]   Carbonation of lignite fly ash at ambient T and P in a semi-dry reaction system for CO2 sequestration [J].
Bauer, Markus ;
Gassen, Niklas ;
Stanjek, Helge ;
Peiffer, Stefan .
APPLIED GEOCHEMISTRY, 2011, 26 (08) :1502-1512
[6]  
Bethke C.M., 2009, GEOCHEMISTS WORKBENC
[7]   Photoinduced Oxidation of Arsenite to Arsenate on Ferrihydrite [J].
Bhandari, Narayan ;
Reeder, Richard J. ;
Strongin, Daniel R. .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2011, 45 (07) :2783-2789
[8]   Arsenic - a review. Part II: Oxidation of arsenic and its removal in water treatment [J].
Bissen, M ;
Frimmel, FH .
ACTA HYDROCHIMICA ET HYDROBIOLOGICA, 2003, 31 (02) :97-107
[9]   TiO2-catalyzed photooxidation of arsenite to arsenate in aqueous samples [J].
Bissen, M ;
Vieillard-Baron, MM ;
Schindelin, AJ ;
Frimmel, FH .
CHEMOSPHERE, 2001, 44 (04) :751-757
[10]   Arsenic immobilization by calcium arsenate formation [J].
Bothe, JV ;
Brown, PW .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 1999, 33 (21) :3806-3811