Fracture energy and softening behavior of high-strength concrete

被引:155
作者
Rao, GA [1 ]
Prasad, BKR [1 ]
机构
[1] Indian Inst Sci, Dept Civil Engn, Bangalore 560012, Karnataka, India
关键词
aggregate; concrete; compressive strength; fracture toughness; silica fume;
D O I
10.1016/S0008-8846(01)00667-6
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
An experimental investigation on the fracture properties of high-strength concrete (HSC) is reported. Three-point bend beam specimens of size 100 x 100 x 500 mm were used as per RILEM-FMC 50 recommendations. The influence of maximum size of coarse aggregate on fracture energy, fracture toughness, and characteristic length of concrete has been studied. The compressive strength of concrete ranged between 40 and 75 MPa. Relatively brittle fracture behavior was observed with the increase in compressive strength. The load-CMOD relationship is linear in the ascending portion and gradually drops off after the peak value in the descending portion. The length of the tail end portion of the softening curve increases as the size of coarse aggregate increases. The fracture energy increases as the maximum size of coarse aggregate and compressive strength of concrete increase. The characteristic length of concrete increases with the maximum size of coarse aggregate and decreases as the compressive strength increases, (C) 2002 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:247 / 252
页数:6
相关论文
共 24 条
[21]   Effects of silica fume and aggregate size on the brittleness of concrete [J].
Tasdemir, C ;
Tasdemir, MA ;
Lydon, FD ;
Barr, BIG .
CEMENT AND CONCRETE RESEARCH, 1996, 26 (01) :63-68
[22]  
Walsh P.F., 1979, INDIAN CONCR J, V46, P469
[23]  
XIE J, 1995, ACI MATER J, V92, P135
[24]   FRACTURE PROPERTIES OF HIGH-STRENGTH CONCRETE WITH VARYING SILICA FUME CONTENT AND AGGREGATES [J].
ZHOU, FP ;
BARR, BIG ;
LYDON, FD .
CEMENT AND CONCRETE RESEARCH, 1995, 25 (03) :543-552