Microwave dielectric properties of the (1-x)La(Nb0.9V0.1)O4-xCaMoO4 (0.05 ≤ x ≤ 0.50) scheelite solid solution ceramics

被引:12
作者
Ma, Zhili [1 ]
Zhao, Jinxiong [2 ]
Zhou, Di [3 ,4 ]
机构
[1] State Grid Gansu Elect Power Co, Lanzhou 730030, Gansu, Peoples R China
[2] State Grid Gansu Elect Power Res Inst, Lanzhou 730070, Gansu, Peoples R China
[3] Xi An Jiao Tong Univ, Minist Educ, Key Lab, Elect Mat Res Lab, Xian 710049, Shaanxi, Peoples R China
[4] Xi An Jiao Tong Univ, Int Ctr Dielect Res, Sch Elect & Informat Engn, Xian 710049, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
Microwave dielectric; LaNbO4; Low temperature co-fired ceramic (LTCC); PROTON CONDUCTION; CRYSTAL-STRUCTURE; CA; SR; BA; TRANSITIONS; EVOLUTION; NIOBATES; OXIDES; PB;
D O I
10.1016/j.jallcom.2019.03.057
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The CaMoO4 was added into La(Nb0.9V0.1)O-4 ceramics by solid state reaction method to adjust the temperature coefficient of frequency (TCF) values. The series of (1-x)La(Nb0.9V0.1)O-4-xCaMoO(4) (0.05 <= x <= 0.5) ceramics were sintered at 1060-1180 degrees C and found to possess permittivity (epsilon(r)) = 10.38-17.73, Q x f = 31,820-76,570 GHz (Q = 1/dielectric loss, f = resonant frequency lying between 8.5 and 9 GHz), and TCF = -26.3 similar to +160.7 ppm/degrees C. The structures of ceramic samples changed from monoclinic fergusonite to tetragonal scheelite continuously at x = 0.20 along with the shift of TCF values from positive to negative. The best microwave dielectric properties with epsilon(r) = 15.71, Q x f = 76,310 GHz (at 8.825 GHz), and TCF = - 26.3 ppm/degrees C were obtained in 0.8La(Nb0.9V0.1)O4-0.2CaMoO(4) ceramics sintered at 1160 degrees C and these ceramics might be good candidates for microwave devices. (C) 2019 Elsevier B.V. All rights reserved..
引用
收藏
页码:345 / 350
页数:6
相关论文
共 50 条
[41]   Crystal structure and microwave dielectric properties of (1-x)ZnTa2O6-xTiO2 ceramics [J].
Park, Jeong-Hyun ;
Nahm, Sahn ;
Park, Jae-Gwan .
JOURNAL OF ALLOYS AND COMPOUNDS, 2012, 537 :221-226
[42]   Dielectric properties, microstructure and phase evolution of non-stoichiometric 0.9Mg2+xSiO4+x-0.1CaTiO3 microwave dielectric ceramics [J].
Liu, Yangfu ;
Tan, Youhong ;
Liu, Shunguo ;
Xie, Kainan ;
Lu, Guanyu ;
Luo, Shaojin ;
Tong, Jianxi ;
Tian, Zhongqing ;
Meng, Fancheng .
CERAMICS INTERNATIONAL, 2021, 47 (23) :33798-33804
[43]   Bond characteristics and microwave dielectric properties of temperature-stable (1-x)Mg2TiO4-xLi4/3Ti5/3O4 (0.15 ≤ x ≤ 0.9) spinel solid solutions [J].
Zhang, Bing ;
Gan, Lin ;
Jiang, Juan ;
Wang, Jinzhao ;
Zhang, Tianjin .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2024, 35 (04)
[44]   Structural Evolution and Microwave Dielectric Properties of Article xZn0.5Ti0.5NbO4-(1-x)Zn0.15Nb0.3Ti0.55O2 Ceramics [J].
Yang, Hongyu ;
Zhang, Shuren ;
Yang, Hongcheng ;
Zhang, Xing ;
Li, Enzhu .
INORGANIC CHEMISTRY, 2018, 57 (14) :8264-8275
[45]   Microwave and Infrared Dielectric Response of Temperature Stable (1-x)BaMoO4-xTiO2 Composite Ceramics [J].
Guo, Jing ;
Zhou, Di ;
Wang, Hong ;
Chen, Yuehua ;
Zeng, Yi ;
Xiang, Feng ;
Wu, Ying ;
Yao, Xi .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (01) :232-237
[46]   Structure and microwave dielectric properties of the Li2/3(1-x)Sn1/3(1-x)MgxO systems (x=0-4/7) [J].
Fang, Zixuan ;
Tang, Bin ;
Yuan, Ying ;
Zhang, Xing ;
Zhang, Shuren .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2018, 101 (01) :252-264
[47]   Studies on Stuctural and Electrical Properties of (1-X) Ba(Fe0.5Nb0.5)O3-xSrTiO3, with X=0, 0.05 Ceramics [J].
Singh, N. K. ;
Kumar, P. ;
Kumar, H. ;
Choudhary, R. N. P. .
XVI NATIONAL SEMINAR ON FERROELECTRICS AND DIELECTRICS (NSFD-XVI), 2011, 1372
[48]   Effects of phase transition on the structure and microwave dielectric properties of (1-x)CeO2-0.5xSm2O3 (x=0-0.9) ceramics [J].
Ma, Shu-Yang ;
Xia, Wang-Suo ;
Shi, Ming-An ;
Wang, Ying ;
Chen, Lei-Ming ;
Wu, Hai-Tao .
CERAMICS INTERNATIONAL, 2025, 51 (02) :1432-1438
[49]   Crystal Structure and Microwave Dielectric Behaviors of Ultra-Low-Temperature Fired x(Ag0.5Bi0.5)MoO4-(1-x)BiVO4 (0.0 ≤ x ≤ 1.0) Solid Solution with Scheelite Structure [J].
Zhou, Di ;
Pang, Li-Xia ;
Qi, Ze-Ming .
INORGANIC CHEMISTRY, 2014, 53 (17) :9222-9227
[50]   Refining the phase diagram of Pb1-xLax(Zr0.9Ti0.1)1-x/4O3 ceramics by structural, dielectric, and anelastic spectroscopy investigations [J].
Craciun, F. ;
Cordero, F. ;
Ciuchi, I. V. ;
Mitoseriu, L. ;
Galassi, C. .
JOURNAL OF APPLIED PHYSICS, 2015, 117 (18)