Microstructure and Mechanical Properties of TiC-Reinforced 316L Stainless Steel Composites Fabricated Using Selective Laser Melting

被引:92
|
作者
Zhao, Zhanyong [1 ]
Li, Jing [1 ]
Bai, Peikang [1 ,2 ]
Qu, Hongqiao [1 ]
Liang, Minjie [1 ]
Liao, Haihong [1 ]
Wu, Liyun [1 ]
Huo, Pengchen [1 ]
Liu, Hu [3 ]
Zhang, Jiaoxia [4 ]
机构
[1] North Univ China, Sch Mat Sci & Engn, Taiyuan 030051, Shanxi, Peoples R China
[2] Shanxi Inst Technol, Dept Mech & Elect Engn, Yangquan 045000, Peoples R China
[3] Zhengzhou Univ, Engn Res Ctr Adv Polymer Proc Technol, Zhengzhou 450002, Henan, Peoples R China
[4] Jiangsu Univ Sci & Technol, Sch Mat Sci & Engn, Zhenjiang 212003, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
selective laser melting; TiC/316Lss composites; microstructure; mechanical property; corrosion resistance; HEAT-TREATMENT; WEAR PROPERTIES; CORROSION BEHAVIOR; PROCESS PARAMETERS; MATRIX COMPOSITES; NANOCOMPOSITES; EVOLUTION; ALLOY; AL; SOLIDIFICATION;
D O I
10.3390/met9020267
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
TiC/316L stainless steel (316Lss) metal matrix composite parts have been formed using selective laser melting (SLM). In this study, we have investigated the influence of the TiC mass fraction on the microstructure evolution, microhardness, friction properties, wear properties, and corrosion resistance of the TiC/316Lss composites. The results show that the microhardness increased by the addition of the TiC mass fraction. In terms of friction and wear properties, the corrosion resistance initially increased, and then decreased. Compared with the pure 316Lss (298.3 HV0.2), the microhardness of the TiC/316Lss composites, which were formed with 2 wt% TiC, was raised to 335.2 HV0.2, which was a 12.4% increase, while the average friction coefficient was 0.123. The reason for this is that the addition of TiC can effectively refine the cell size, and as the TiC content increases, the refinement effect is more obvious. During the melting process, TiC particles act as nucleation centres, hindering the growth of crystal cells, promoting the formation of the austenite phase, and forming fine equiaxed structures, which increases the strength. However, excessive TiC particles aggravate the spheroidisation during the process of SLM, leading to increased defects, as well as a decrease in density and corrosion resistance.
引用
收藏
页数:16
相关论文
共 50 条
  • [31] Microstructure and mechanical properties relationship of additively manufactured 316L stainless steel by selective laser melting
    Puichaud, Anne-Helene
    Flament, Camille
    Chniouel, Aziz
    Lomello, Fernando
    Rouesne, Elodie
    Giroux, Pierre-Francois
    Maskrot, Hicham
    Schuster, Frederic
    Bechade, Jean-Luc
    EPJ NUCLEAR SCIENCES & TECHNOLOGIES, 2019, 5
  • [32] Tungsten particle-reinforced 316L steel fabricated by laser melting deposition: Microstructure and mechanical properties
    Sun, Yiping
    Wang, Bin
    Ren, Yongpeng
    Li, Chunlei
    Lei, Jianbo
    Zhang, Songpeng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 929
  • [33] Anisotropy in the microstructure and mechanical property for the bulk and porous 316L stainless steel fabricated via selective laser melting
    Kong, Decheng
    Ni, Xiaoqing
    Dong, Chaofang
    Zhang, Liang
    Man, Cheng
    Cheng, Xuequn
    Li, Xiaogang
    MATERIALS LETTERS, 2019, 235 : 1 - 5
  • [34] 316L Stainless Steel with Gradient Porosity Fabricated by Selective Laser Melting
    Ruidi Li
    Jinhui Liu
    Yusheng Shi
    Mingzhang Du
    Zhan Xie
    Journal of Materials Engineering and Performance, 2010, 19 : 666 - 671
  • [35] 316L Stainless Steel with Gradient Porosity Fabricated by Selective Laser Melting
    Li, Ruidi
    Liu, Jinhui
    Shi, Yusheng
    Du, Mingzhang
    Xie, Zhan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2010, 19 (05) : 666 - 671
  • [36] Characterization of carbide particle-reinforced 316L stainless steel fabricated by selective laser melting
    Bhowmik, Ayan
    Zhai, Wengang
    Zhou, Wei
    Nai, Sharon Mui Ling
    MATERIALS CHARACTERIZATION, 2021, 179
  • [37] Microstructure and mechanical properties of 316L stainless steel manufactured by multi-laser selective laser melting (SLM)
    Zhao, Lin
    Zhang, Jianfeng
    Yang, Jinlei
    Hou, Juan
    Li, Jianjian
    Lin, Jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 913
  • [38] Effect of boron element on microstructure and mechanical properties of 316L stainless steel manufactured by selective laser melting
    Zheng, Qi
    Chen, Hong Sheng
    Zhou, Jun
    Wang, Wenxian
    Xi, San Xiao
    Yuan, Ye
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 : 3744 - 3755
  • [39] Cavitation erosion resistance of 316L stainless steel fabricated using selective laser melting
    Ding, Hongqin
    Tang, Qing
    Zhu, Yi
    Zhang, Chao
    Yang, Huayong
    FRICTION, 2021, 9 (06) : 1580 - 1598
  • [40] Cavitation erosion resistance of 316L stainless steel fabricated using selective laser melting
    Hongqin DING
    Qing TANG
    Yi ZHU
    Chao ZHANG
    Huayong YANG
    Friction, 2021, 9 (06) : 1580 - 1598