Effect of glaze thickness on the fracture toughness and hardness of alumina-reinforced porcelain

被引:30
作者
Baharav, H [1 ]
Laufer, BZ [1 ]
Pilo, R [1 ]
Cardash, HS [1 ]
机构
[1] Tel Aviv Univ, Maurice & Gabriela Goldschleger Sch Dent Med, Dept Oral Rehabil, IL-69978 Tel Aviv, Israel
关键词
D O I
10.1016/S0022-3913(99)70204-0
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Statement of problem. Although porcelain is the most esthetic restorative material available, it is subject to fracture during function. Glazing reduces the size of flaws in the surface of the porcelain and increases its resistance to crack propagation, but the optimum thickness of this glazed layer has not been determined. Purpose. This study compared the fracture toughness (K-c) and Vickers hardness number (VHN) of an alumina-reinforced porcelain at different thicknesses of glaze. Material and methods. Disks of feldspathic porcelain reinforced with 2% aluminum oxide were prepared and glazed for 0, 30, 60, 90, and 120 seconds. Fracture toughness and Vickers microhardness were determined with a microindentation technique. Thickness of the glazed layers was measured with a SEM. Results. Mean Vickers hardness number and fracture toughness values both decreased significantly with glazing times from 0 to 60 seconds, and increased significantly with glazing times from 60 to 120 seconds (P<.001, ANOVA). SEM examination revealed an increase in glazed layer thickness with increased glazing time. Conclusions. Minimal and maximum thicknesses of glaze layers on alumina-reinforced porcelain resulted in a surface that was harder and more resistant to fracture than moderate glaze thicknesses.
引用
收藏
页码:515 / 519
页数:5
相关论文
共 24 条
  • [1] INFLUENCE OF TEMPERING AND CONTRACTION MISMATCH ON CRACK DEVELOPMENT IN CERAMIC SURFACES
    ANUSAVICE, KJ
    DEHOFF, PH
    HOJJATIE, B
    GRAY, A
    [J]. JOURNAL OF DENTAL RESEARCH, 1989, 68 (07) : 1182 - 1187
  • [2] EFFECT OF FIRING TEMPERATURE AND WATER EXPOSURE ON CRACK-PROPAGATION IN UNGLAZED PORCELAIN
    ANUSAVICE, KJ
    LEE, RB
    [J]. JOURNAL OF DENTAL RESEARCH, 1989, 68 (06) : 1075 - 1081
  • [3] Effect of different cooling rates on fracture toughness and microhardness of a glazed alumina reinforced porcelain
    Baharav, H
    Laufer, BZ
    Mizrachi, A
    Cardash, HS
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1996, 76 (01) : 19 - 22
  • [4] AN EVALUATION OF PORCELAIN STRENGTH AND THE EFFECT OF SURFACE-TREATMENT
    BRACKETT, SE
    LEARY, JM
    TURNER, KA
    JORDAN, RD
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1989, 61 (04) : 446 - 451
  • [5] Castellani D, 1996, INT J PROSTHODONT, V9, P459
  • [6] CREYKE WEC, 1968, BRIT CERAM TRANS J, V67, P339
  • [7] THE 3-POINT BEAM TEST FOR THE EVALUATION OF DENTAL PORCELAIN
    EDWARDS, MR
    JACOBSEN, PH
    WILLIAMS, GJ
    [J]. JOURNAL OF DENTAL RESEARCH, 1983, 62 (10) : 1086 - 1088
  • [8] THE EFFECT OF GLAZE ON PORCELAIN STRENGTH
    FAIRHURST, CW
    LOCKWOOD, PE
    RINGLE, RD
    THOMPSON, WO
    [J]. DENTAL MATERIALS, 1992, 8 (03) : 203 - 207
  • [9] AMALGAM RESTORATIONS, PLAQUE REMOVAL AND PERIODONTAL HEALTH
    GORZO, I
    NEWMAN, HN
    STRAHAN, JD
    [J]. JOURNAL OF CLINICAL PERIODONTOLOGY, 1979, 6 (02) : 98 - 105
  • [10] A COMPARISON OF THE ABRASIVENESS OF 6 CERAMIC SURFACES AND GOLD
    JACOBI, R
    SHILLINGBURG, HT
    DUNCANSON, MG
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1991, 66 (03) : 303 - 309