Investigation of intergranular penetration behavior in CrMnFeCoNi HEA/304 SS dissimilar brazing joints

被引:25
|
作者
Wang, Ge [1 ]
Sheng, Guangmin [1 ]
Yu, Qili [1 ]
Yuan, Xinjian [1 ]
Sun, Jianchun [2 ]
Jiao, Yingjun [1 ]
Zhang, Yuntao [1 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, 174 Shazheng St, Chongqing 400044, Peoples R China
[2] Chongqing Univ Sci & Technol, Coll Mat Sci & Engn, 20 Daxuechengdong Rd, Chongqing 401331, Peoples R China
关键词
Brazing; Diffusion; Dissimilar joint; High-entropy alloy; Intergranular penetration; Stainless steel; HIGH-ENTROPY ALLOY; MECHANICAL-PROPERTIES; STAINLESS-STEEL; MICROSTRUCTURE; EVOLUTION; DIFFUSION; WELDABILITY; STABILITY; STRENGTH; TITANIUM;
D O I
10.1016/j.intermet.2020.106940
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
As-rolled and annealed CrMnFeCoNi high-entropy alloys (HEAs) were selected to braze 304 SS by using Ag50Cu as the filler metal (FM) in a vacuum furnace. Intergranular penetration was detected in each joint. To explore the evolvement mechanism of microstructure and performance, three different series of dissimilar joints were prepared and the microstructure and mechanical properties of the dissimilar joints were observed and tested. The penetration of liquid FM into the grain boundaries (GBs) of HEA was attributed to the imbalance between GB energy and solid-liquid interface energy. Intergranular penetration accelerated interdiffusion between FM and HEA, and diffusion induced further penetration. The mechanism of interdiffusion was studied, and the effects of brazing temperature, Ag50Cu content and Mn concentration in HEA on atomic immigration during brazing were discussed. Intergranular penetration inhibited grain growth in the penetration zone (PZ) of HEA. The physical difference between HEA and penetration phase generated residual stress. A layer of sigma (Cr, Fe) phase formed at the 304 SS/FM interfaces, and increased the embrittlement of the dissimilar joints brazed at high temperatures. However, the tensile strength of the joints is improved by the immigration of a huge amount of Mn (a solution-strengthened element of Ag-Cu alloy) into FM and the increasing contact area induced by penetration. The tensile strength of 304 SS and the as-rolled HEA reached 434.7 MPa, which is higher than that of the joint brazed using BNi2. The annealed HEA processed low GB density and low driving force for grain growth, decreasing the difference in grain sizes in PZ, reducing penetration and ensuring interdiffusion between HEA and FM. The tensile strength of the joint of annealed HEA reached 487.1 MPa, indicating that controlling parameters of brazing and changing conditions of HEA are effective to reduce penetration.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Creep behavior and damage evolution of T92/Super304H dissimilar weld joints
    Zhai, Xiao-wei
    Du, Jin-feng
    Li, Lin-ping
    Zhou, Chao
    Zhang, Zheng
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2019, 26 (07) : 751 - 760
  • [32] Investigation on Processing Maps of Diffusion Bonding Process Parameters for Ti-6Al-4 V/AISI304 Dissimilar Joints
    Arun Negemiya, A.
    Shankar, A. N.
    Guruprasad, B.
    Prakash, B.
    Dineshkumar, S.
    Batu, Areda
    Rajakumar, S.
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2021, 2021
  • [33] The effect of friction stir welding on the microstructure and mechanical properties of the dissimilar SS304 and Al7075-T6 alloy joints
    Kumar, Ranjan
    Manjaiah, M.
    Davidson, M. J.
    WELDING INTERNATIONAL, 2023, 37 (11) : 643 - 654
  • [34] Microstructure evolution and fracture behavior of rotating laser welded-brazed 6061 aluminum alloys/304 SS dissimilar joint
    Xie, Jia
    Cai, Chuang
    Zhang, Bingbing
    Yu, Jie
    Liu, Yonghong
    Chen, Hui
    MATERIALS CHARACTERIZATION, 2023, 195
  • [35] Investigation on mechanical properties and corrosion behavior of dissimilar joints of 5083 and 6005A alloy welded by friction stir welding
    Chang, Yongpeng
    Han, Bin
    Shi, Yunjia
    Wang, Xiangnan
    Liu, Nian
    Guo, Jiaqi
    Dou, Shengchuan
    Zhang, Guopeng
    Li, Mengjia
    Cai, Bin
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2024, 75 (04): : 489 - 504
  • [36] Creep and High-Temperature Tensile Deformation Behavior of the TIG Welded P92/304L Dissimilar Steel Weld Joints
    Dak, Gaurav
    Guguloth, Krishna
    Sirohi, Sachin
    Adin, Mehmet Sukru
    Pandey, Chandan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024,
  • [37] An investigation into the effects of fabric reinforcements in the bonding surface on failure response and transverse impact behavior of adhesively bonded dissimilar joints
    Ozdemir, Okan
    Oztoprak, Nahit
    COMPOSITES PART B-ENGINEERING, 2017, 126 : 72 - 80
  • [38] Studies on localized electrochemical activity of 304L SS-Zr-4 dissimilar joints using alternating current scanning electrochemical microscopy
    Pal, Ankita
    Thinaharan, C.
    Krishna, Nanda Gopala
    Shankar, A. Ravi
    Philip, John
    APPLIED SURFACE SCIENCE, 2022, 578
  • [39] Investigation of Deformation Behavior of SS304 and Pure Copper Subjected to Electrically Assisted Forming Process
    Jiang, Tianhao
    Peng, Linfa
    Yi, Peiyun
    Lai, Xinmin
    JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2017, 139 (01):
  • [40] Investigation on AISI 304 austenitic stainless steel to AISI 4140 low alloy steel dissimilar joints by gas tungsten arc, electron beam and friction welding
    Arivazhagan, N.
    Singh, Surendra
    Prakash, Satya
    Reddy, G. M.
    MATERIALS & DESIGN, 2011, 32 (05): : 3036 - 3050