On the hydrogen embrittlement behavior of nickel-based alloys: Alloys 718 and 725

被引:83
作者
Lu, Xu [1 ]
Ma, Yan [2 ,3 ]
Wang, Dong [1 ]
机构
[1] Norwegian Univ Sci & Technol, Dept Mech & Ind Engn, Richard Birkelands Vei 2B, NO-7491 Trondheim, Norway
[2] Rhein Westfal TH Aachen, Steel Inst IEHK, Intzestr 1, D-52072 Aachen, Germany
[3] Max Plank Inst Eisenforsch GmbH, Max Planck Str 1, D-40237 Dusseldorf, Germany
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 792卷
关键词
Hydrogen embrittlement; Nickel-based superalloys; Intergranular precipitates; Grain boundary; Hydrogen-induced cracking; VACANCY FORMATION ENERGIES; REDUCING GRAIN-BOUNDARY; SOLUTE SEGREGATION; TENSILE PROPERTIES; DISLOCATION LINE; CRACKING; DEFORMATION; INCONEL-718; MECHANISMS; DIFFUSION;
D O I
10.1016/j.msea.2020.139785
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Nickel-based superalloys have attracted immense attention in the oil and gas industry due to their outstanding combination of mechanical properties and corrosion resistance. In corrosive service environment, hydrogen embrittlement is a severe issue. In the present work, the susceptibility of two precipitation-hardened nickel-based alloys, i.e., Alloy 718 and Alloy 725, to hydrogen embrittlement was studied using slow strain-rate tensile test and advanced characterization techniques. The mechanical properties and fracture behavior of these two alloys were compared in both hydrogen-free and hydrogen-charged conditions. In the presence of hydrogen, Alloy 718 failed prevalently through a combination of transgranular and intergranular cracking behavior, while Alloy 725 failed primarily through intergranular failure with a considerably lower resistance to hydrogen embrittlement. This distinction was attributed to their different microstructures and different types of precipitates along grain boundaries. Specifically, in Alloy 725, the decoration of (Cr, Mo)-rich precipitates at grain boundaries distort the local structures and cause such boundaries to be vulnerable to hydrogen attack, thus promoting intergranular cracking.
引用
收藏
页数:11
相关论文
共 59 条
[51]   Effect of double aging treatment on structure in Inconel 718 alloy [J].
Wang, CZ ;
Li, RB .
JOURNAL OF MATERIALS SCIENCE, 2004, 39 (07) :2593-2595
[52]   Effect of hydrogen on nanomechanical properties in Fe-22Mn-0.6C TWIP steel revealed by in-situ electrochemical nanoindentation [J].
Wang, Dong ;
Lu, Xu ;
Deng, Yun ;
Guo, Xiaofei ;
Barnoush, Afrooz .
ACTA MATERIALIA, 2019, 166 :618-629
[53]   Quantitative analysis on hydrogen trapping of TiC particles in steel [J].
Wei, FG ;
Tsuzaki, K .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (02) :331-353
[54]   Shearing of γ" precipitates and formation of planar slip bands in Inconel 718 during cyclic deformation [J].
Xiao, L ;
Chen, DL ;
Chaturvedi, MC .
SCRIPTA MATERIALIA, 2005, 52 (07) :603-607
[55]   Investigation on hydrogen induced cracking behaviors of Ni-base alloy [J].
Yao, Yuan ;
Pang, Xiaolu ;
Gao, Kewei .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2011, 36 (09) :5729-5738
[56]  
Yoon D. N., 1990, Colloque de Physique, P721
[57]   Evidence that carbide precipitation produces hydrogen traps in Ni-17Cr-8Fe alloys [J].
Young, GA ;
Scully, JR .
SCRIPTA MATERIALIA, 1997, 36 (06) :713-719
[58]   On the role of precipitates in hydrogen trapping and hydrogen embrittlement of a nickel-based superalloy [J].
Zhang, Zhenbo ;
Moore, Katie L. ;
McMahon, Greg ;
Morana, Roberto ;
Preuss, Michael .
CORROSION SCIENCE, 2019, 146 :58-69
[59]   Hydrogen assisted crack initiation and propagation in a nickel-based superalloy [J].
Zhang, Zhenbo ;
Obasi, Gideon ;
Morana, Roberto ;
Preuss, Michael .
ACTA MATERIALIA, 2016, 113 :272-283