TIG-cladding of Al-Cu and Al-Cu-Sn alloys on pure Al substrate

被引:3
|
作者
Alirezaei, Mohammad-Amin [1 ]
Raiszadeh, Ramin [1 ]
Khayati, Gholamreza [1 ]
机构
[1] Shahid Bahonar Univ Kerman, Sch Engn, Dept Met & Mat Sci, Jomhoori Eslami Blvd, Kerman, Iran
来源
关键词
TIG; Cladding; L-CuP6; L-CuSn6; Al; 2; Cu; RESIDUAL-STRESS; DUCTILE IRON; MICROSTRUCTURE; ALUMINUM; WIRE; STEEL; WEAR;
D O I
10.1016/j.mtcomm.2022.104624
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A tungsten inert gas (TIG) welding process was utilized successfully to produce a dense and hard cladding layer on a commercial purity Al substrate using two commercial filler wires (L-CuP6 and L-CuSn6). Effect of the type of filler wire, welding frequency, and the type of electrical current (AC or DCEN) on the microstructure, hardness, and the residual stress of the cladding layer were studied using scanning electron microscopy, X-ray diffraction, and a hardness test. The results showed that the L-CuP6 wire produced a homogeneous layer containing Al2Cu-Al eutectic in an alpha-Al matrix. The microstructure of the cladding layer formed with the L-CuSn6 wire also contained Al2Cu (theta) primary intermetallic and beta-Sn grains. The hardness of the cladding layer was found to depend on the fraction of Al2Cu intermetallic formed in the microstructure. Increasing the frequency or using a DCEN instead of AC caused the fraction of Al2Cu formed to decrease. These effects were attributed to the decrease in the volume of the weld pool and the inability of the DCEN to remove the oxide film from the Al substrate, respectively.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Cu concentration dependence of the mechanical behaviour of Al-Cu alloys
    Lokker, JP
    van Winden, RSA
    Janssen, GCAM
    Radelaar, S
    ADVANCED INTERCONNECTS AND CONTACTS, 1999, 564 : 477 - 482
  • [42] Subsurface deformation of worn Al-Cu and Al-Mg alloys
    Ghazali, M. J.
    Rainforth, W. M.
    Abdullah, S.
    Ihsan, A. K. A.
    Hassan, M.
    ADVANCES IN FRACTURE AND MATERIALS BEHAVIOR, PTS 1 AND 2, 2008, 33-37 : 483 - +
  • [43] Thermodynamic properties of liquid Al-Si and Al-Cu alloys
    D. S. Kanibolotsky
    O. A. Bieloborodova
    N. V. Kotova
    V. V. Lisnyak
    Journal of Thermal Analysis and Calorimetry, 2002, 70 : 975 - 983
  • [44] Milling parameters of Al-Cu and Al-Si cast alloys
    M. Hamed
    Y. Zedan
    A. M. Samuel
    H. W. Doty
    F. H. Samuel
    The International Journal of Advanced Manufacturing Technology, 2019, 104 : 3731 - 3743
  • [45] ELECTRICAL RESISTIVITIES OF LIQUID AL-MG AND AL-CU ALLOYS
    KHAJIL, TMA
    TOMAK, M
    NUOVO CIMENTO DELLA SOCIETA ITALIANA DI FISICA D-CONDENSED MATTER ATOMIC MOLECULAR AND CHEMICAL PHYSICS FLUIDS PLASMAS BIOPHYSICS, 1989, 11 (05): : 739 - 744
  • [46] Transformation defects on θ′ precipitates in Al-Cu alloys
    Purdy, GR
    Hirth, JP
    PHILOSOPHICAL MAGAZINE LETTERS, 2006, 86 (03) : 147 - 154
  • [47] MICROSTRUCTURE, CORROSION AND WEAR BEHAVIOUR OF UFG-POWDER-METALLURGICAL Al-Cu ALLOYS, Al-Cu/Al2O3(p) AND Al-Cu/SiC(p) COMPOSITES
    Nickel, D.
    Alisch, G.
    Podlesak, H.
    Hockauf, M.
    Fritsche, G.
    Lampke, T.
    REVIEWS ON ADVANCED MATERIALS SCIENCE, 2010, 25 (03) : 261 - 269
  • [48] Milling parameters of Al-Cu and Al-Si cast alloys
    Hamed, M.
    Zedan, Y.
    Samuel, A. M.
    Doty, H. W.
    Samuel, F. H.
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 104 (9-12): : 3731 - 3743
  • [49] THE STRUCTURE OF GPI ZONES IN AL-CU ALLOYS
    GEROLD, V
    BUBECK, E
    SCRIPTA METALLURGICA, 1982, 16 (09): : 1101 - 1105
  • [50] Texture of Al-Cu alloys deformed by ECAP
    Kusnierz, J
    Mathon, MH
    Baudin, T
    Jasienski, Z
    Penelle, R
    ICOTOM 14: TEXTURES OF MATERIALS, PTS 1AND 2, 2005, 495-497 : 851 - 856