Microstructure and mechanical properties of dissimilar friction stir welded type 304 austenitic stainless steel to Q235 low carbon steel

被引:66
作者
Wang, Hongduo [1 ,3 ]
Wang, Kuaishe [1 ,2 ]
Wang, Wen [1 ,2 ]
Huang, Liying [1 ,2 ]
Peng, Pai [1 ,2 ]
Yu, Hailiang [4 ]
机构
[1] Xian Univ Architecture & Technol, Sch Met Engn, Xian 710055, Shaanxi, Peoples R China
[2] Natl & Local Joint Engn Res Ctr Funct Mat Proc, Xian 710055, Shaanxi, Peoples R China
[3] Xian Shiyou Univ, Sch Mat Sci & Engn, Xian 710065, Shaanxi, Peoples R China
[4] Cent South Univ, Coll Mech & Elect Engn, Changsha 410083, Hunan, Peoples R China
基金
中国国家自然科学基金;
关键词
Stainless steel; Low carbon steel; Friction stir welding; Recrystallization; Phase transformation; Mechanical properties; RESIDUAL-STRESS; ALUMINUM-ALLOYS; GRAIN-STRUCTURE; ELECTRON-BEAM; EVOLUTION; MAGNESIUM; JOINT; TEMPERATURE; DIFFUSION; TEXTURE;
D O I
10.1016/j.matchar.2019.109803
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, friction stir welding (FSW) was used to weld dissimilar metals (Type 304 stainless steel (SS304) and Q235 low carbon steel). The microstructure, interfacial characteristics, residual stress distribution and mechanical properties of the joint were investigated. The results show that FSW results in grain refinement in the stir zone (SZ) and thermal-mechanical affected zone (TMAZ) in SS304 side. Discontinuous dynamic re crystallization and twinning-induced dynamic recrystallization are the main grain refinement mechanisms. Dynamic recovery occurs in the heat-affected zone (HAZ). On the Q235 steel side, the acicular ferrite and pearlite are generated in the SZ, which is due to its peak temperature of up to Ac-3. Additionally, the amount of acicular ferrite decreases in the TMAZ. Continuous and discontinuous dynamic recrystallization is the main recrystallization mechanism in the two regions. The interfacial bonding mechanism of FSW joint consists of both mechanical and metallurgical bonding. In addition, the difference in expansion coefficient and microstructure between the two steels results in the formation of residual compressive stress in the SZ. Grain refinement and acicular ferrite are responsible for the microhardness distribution in the whole joint. The tensile strength of FSW joint is 493 MPa, which is more than that of Q235 steel by around 4%. However, the elongation is 17%, which shows a decrease of around 50%. Furthermore, the fracture surface shows ductile fracture with dimples.
引用
收藏
页数:12
相关论文
共 53 条
[1]   Strain-Induced Martensite Formation and Recrystallization Behavior in 304 Stainless Steel [J].
Al-Fadhalah, Khaled J. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (04) :1697-1709
[2]  
蔡建鹏, 2016, [焊接学报, Transactions of the China Welding Institution], V37, P71
[3]  
[Anonymous], SCR MAT
[4]  
[Anonymous], 2013, E8E8M ASTM INT
[5]  
[Anonymous], 2005, NPL MEASUREMENT GOOD
[6]   Friction stir lap welding of stainless steel and plain carbon steel to enhance corrosion properties [J].
Argade, G. R. ;
Shukla, S. ;
Liu, K. ;
Mishra, R. S. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2018, 259 :259-269
[7]   Investigation on AISI 304 austenitic stainless steel to AISI 4140 low alloy steel dissimilar joints by gas tungsten arc, electron beam and friction welding [J].
Arivazhagan, N. ;
Singh, Surendra ;
Prakash, Satya ;
Reddy, G. M. .
MATERIALS & DESIGN, 2011, 32 (05) :3036-3050
[8]   Microstructural Aspects of TIG and A-TIG Welding Process of Dissimilar Steel Grades and Correlation to Mechanical Behavior [J].
Badheka, Vishvesh J. ;
Basu, Ritwik ;
Omale, Joseph ;
Szpunar, Jerzy .
TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (09) :1765-1773
[9]   Multiscale Measurements of Residual Stress in a Low-Alloy Carbon Steel Weld Clad with IN625 Superalloy [J].
Benghalia, G. ;
Rahimi, S. ;
Wood, J. ;
Coules, H. ;
Paddea, S. .
MATERIALS PERFORMANCE AND CHARACTERIZATION, 2018, 7 (04) :606-629
[10]   Dissimilar Friction Stir Welding of Carbon Steel and Stainless Steel: Some Observation on Microstructural Evolution and Stress Corrosion Cracking Performance [J].
Bin Matlan, Mohd Joharif ;
Mohebbi, Hamed ;
Pedapati, Srinivasa Rao ;
Awang, Mokhtar B. ;
Ismail, Mokhtar Che ;
Kakooei, Saeid ;
Dan, Nsikan Etim .
TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2018, 71 (10) :2553-2564